Fabrication and Characterization of CVD-Deposited TiC-SiC Composites
Source abstract
Abstract
Composites with several compositions in TiC-SiC system were fabricated by chemical vapor deposition and several properties were measured. The CVD conditions used were, TiCl4-SiCl4-CH4-H2 system, deposition temperature of 1350°C and total gas pressure of 60Torr. The TiC-SiC composites with various compositions were fabricated by stepwise change in the Ti/(Ti+Si) ratio in the feed gas on the basis of thermodynamic calculation for the system. The obtained composites were fully dense with columnar structure perpendicular to the substrate plane and had (220) orientation on parallel there to. Thermal expansion coefficients of the TiC-SiC composites parallel to substrate ranged from 4.5 to 7.4×10-6K-1 and Young's Modulus perpendicular to the substrate ranged from 220 to 467GPa depending on the composition. These measured values agreed with that calculated from some rules of mixture in composite.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.