article·1994-01-01Open access

Internal Friction of 16.3Na2O⋅33.7MgO⋅50.0SiO2 Glass

Kazutaka Takizawa, Toshihiko Sakai, Masaki EMURA, Mikihiro SANO, Naoto Watanabe

Abstract

The internal friction of 16.3Na2O⋅33.7MgO⋅50.0SiO2 glass was measured with an inverted torsion pendulum in the frequency range 0.35-0.95Hz, and the tracer diffusion coefficients of oxygen and magnesium were measured at temperatures below the glass transition point by use of stable isotopes 18O and 26Mg, respectively. The temperature dependence of the relaxation time of a high-temperature peak was represented by τH.P.(s)=(2.04±0.05)×10-15×exp[{183.8±5.7 (kJ/mol)}/RT] The temperature dependence of the tracer diffusion coefficients for oxygen and magnesium was represented by the following equations: DOxy(m2⋅s-1)=(1.22±0.06)×10-10×exp[{-150.2±5.1(kJ/mol)}/RT] DMg(m2⋅s-1)=(4.29-1.15+1.57)×10-6×exp[{-195.3±19.9(kJ/mol)}/RT] The activation energy for the high-temperature peak (183.8kJ/mol) was smaller than that for magnesium diffusion (195.3kJ/mol) by about 7% but greater than that for oxygen diffusion (150.2kJ/mol). Comparison of the results of the present study with those obtained by Hino et al. led to the conclusion that the high-temperature peak was caused by the movement of magnesium ion under stress.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Glass properties and applications · Advanced ceramic materials synthesis · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.