journal article·2010Open access

Synthesis and properties of BiScO3-PbTiO3 powders and thin films using metal-organic precursor solutions

Hiroshi YAMAZAKI, Tetsuo SHIMURA, Wataru SAKAMOTO, Toshinobu YOGO

Journal of the Ceramic Society of Japan· Volume 118· Issue 1380

Abstract

The BiScO3–PbTiO3 binary system is known to have a morphotropic phase boundary (MPB) and a higher Curie temperature than Pb(Zr,Ti)O3 and to exhibit excellent dielectric and ferroelectric properties. Perovskite BiScO3–PbTiO3 powders and thin films were synthesized via a chemical process using metal-organic precursor solutions. Homogeneous and stable precursor solutions, perovskite BiScO3–PbTiO3 single-phase powders and thin films on Pt/TiOx/SiO2/Si substrates were successfully prepared by optimizing the processing conditions. The 0.35BiScO3–0.65PbTiO3 composition was close to the MPB and had a Curie temperature of around 470°C. The electrical properties of BiScO3–PbTiO3 thin films showed a maximum at this composition. The dielectric permittivity of the 0.35BiScO3–0.65PbTiO3 thin film at the MPB was approximately 1700, with a dielectric loss tangent of less than 5% at room temperature. Furthermore, BiScO3–PbTiO3 thin films showed a typical ferroelectric polarization (P)–electric field (E) hysteresis loop. The remnant polarization (Pr) and coercive field (Ec) of the 0.35BiScO3–0.65PbTiO3 film were approximately 23 µC/cm2 and 70 kV/cm, respectively.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Multiferroics and related materials · Microwave Dielectric Ceramics Synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Division of Nanomaterials Science, EcoTopia Science Institute, Nagoya University

References (24)

Show source-provided references
1. 10.1063/1.172174110.1063/1.1721741 ↗
2. 10.1111/j.1151-2916.1958.tb12903.x10.1111/j.1151-2916.1958.tb12903.x ↗
3. 10.1109/58.65563910.1109/58.655639 ↗
4. 10.1143/JJAP.40.599910.1143/JJAP.40.5999 ↗
5. 10.1143/jjap.41.209910.1143/jjap.41.2099 ↗
6. 10.1063/1.159572610.1063/1.1595726 ↗
7. 10.1016/S0167-577X(02)01143-610.1016/S0167-577X(02)01143-6 ↗
8. 10.1063/1.177781010.1063/1.1777810 ↗
9. 10.1143/JJAP.45.731510.1143/JJAP.45.7315 ↗
10. 10.1063/1.302652710.1063/1.3026527 ↗
11. 10.1063/1.165654210.1063/1.1656542 ↗
12. E. C. Subbarao · J. Am. Ceram. Soc. · 1960 · 43 · 43910.1111/j.1151-2916.1960.tb13694.x ↗
13. 10.1063/1.150735210.1063/1.1507352 ↗
14. 10.1557/jmr.2004.19.2.56810.1557/jmr.2004.19.2.568 ↗
15. H. Wen, X. Wang, X. Deng, T. Sun an · J. Appl. Phys. · 2007 · 101 · 01610310.1063/1.2404788 ↗
16. H. Wen, X. Wang, X. Deng, T. Sun an · Appl. Phys. Lett. · 2007 · 90 · 20290210.1063/1.2739326 ↗
17. 10.1143/JJAP.46.L31110.1143/JJAP.46.L311 ↗
18. 10.1143/JJAP.46.697110.1143/JJAP.46.6971 ↗
19. 10.1143/JJAP.48.09KA0810.1143/JJAP.48.09KA08 ↗
20. 10.1016/j.tsf.2009.12.10210.1016/j.tsf.2009.12.102 ↗
21. 10.1143/JJAP.42.522210.1143/JJAP.42.5222 ↗
22. 10.2109/jcersj2.117.93910.2109/jcersj2.117.939 ↗
23. CHENG J-R · J. Am. Ceram. Soc. · 2003 · 86 · 211110.1111/j.1151-2916.2003.tb03617.x ↗
24. 10.1063/1.157954310.1063/1.1579543 ↗