Microstructure Development during Sintering in Polycrystalline MgO⋅1.5Al2O3 Spinel

E. Proverbio, Masaki Yasuoka, Kiyoshi Hirao, Shuzo Kanzaki

Abstract

Fine Al-rich spinel MgO⋅1.5Al2O3 powder was synthesized by hydrolysis of mixed alkoxides. High sinterability of powder allowed to obtain relative density higher than 95% at temperature as low as 1300°C by pressureless sintering in air. Samples sintered at temperature of 1100°-1500°C had quite heterogeneous microstructure owing to precipitation of large corundum particles (<1400°C) and discontinuous grain growth of spinel matrix (>1400°C). However, homogeneous microstructure with fine grains could be obtained by a two step sintering process in which spinel grain growth at high temperature was inhibited by corundum particles momentarily retained above solvus temperature. Precipitation behavior during sintering was compared with that during annealing, and the precipitation mechanism was discussed.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.