Sinterability of Magnesium Oxide Powder with Magnesium Phosphate Addition Prepared by Coprecipitation Technique (Part 3)
Source abstract
Abstract
Changes in relative density and grain size of magnesium oxide (MgO) compact containing magnisium phosphate equivalent to 0.5mol% P2O5 were investigated between 1200°C and 1700°C; the bending strength, thermal expansion and water resistivity were examined for sintered compacts. The relative densities of MgO compacts with phosphate additions attained 96-99% as the sintering times at 1300°C and at 1400°C were prolonged from 5 to 30h. The bending strength and the thermal expansion coefficient of MgO compact with phosphate addition sintered at 1400°C for 30h were 185MPa (estimated value of nonporous compact: 300MPa) and 13.3×10-6°C-1 (30°-1000°C), respectively; the water-resistivity test (3h-immersion at 90°C) showed that the weight increase due to the hydration of MgO to Mg(OH)2 amounted only to 0.03%. The bending strength and water-resistivity of MgO compact was enhanced by the addition of phosphate.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Magnesium Oxide Properties and Applications · Advanced ceramic materials synthesis · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.