journal article·2019-02-01Open access

Crystalline structure in SiC fibers driven by pyrolysis temperature and time

Cheng LI, Ruobing XIE, Mouhua WANG, Baoxing SUN, Guanhong LEI, Qing HUANG, Jianjian LI, Yongqi ZHU, Renduo LIU, Qi LEI

Abstract

In this work, we study the impact of pyrolysis temperature and time on the crystalline structure of lab made silicon carbide (SiC) fibers and their mechanical properties. The polycrystalline structure and the characteristic length scales of β-SiC in fibers were characterized with X-ray diffraction, transmission electron microscope and synchrotron small angle X-ray scattering. The sizes of crystallites, particles and interparticle distance all increase as pyrolysis temperature or time increases while the crystallinity nearly remains constant, indicating SiC crystals in the fiber grow by absorbing the surrounding small crystals. The crystal growth follows the Ostwald ripening when pyrolysis temperature reaches 1500°C. At this temperature, longer pyrolysis time seems to reduce the tensile strength, but still keep increasing the modulus. The stiffness is possibly associated with the growth of particle size, interparticle distance and the size of voids in fibers.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicon Carbide Semiconductor Technologies · Advanced ceramic materials synthesis · Carbon Nanotubes in Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Shanghai Institute of Applied Physics, Chinese Academy of Sciences (CAS)

References (21)

Show source-provided references
1. 1) J. J. Sha, T. Nozawa, J. S. Park, Y. Katoh and A. Kohyama, J. Mater. Sci., 329, 592–596 (2004).
2. 2) J. J. Sha, J. S. Park, T. Hinoki and A. Kohyama, Mech. Mater., 39, 175–182 (2007).
3. 3) R. Q. Yao, Y. Y. Wang and Z. D. Feng, Fatigue. Fract. Mater. Engng. Struct., 31, 777–787 (2008).
4. 4) J. J. Sha, T. Hinoki and A. Kohyama, Mater. Charact., 60, 796–802 (2009).
5. 5) J. J. Sha, J. S. Park, T. Hinoki and A. Kohyama, Mater. Charact., 57, 6–11 (2006).
6. 6) T. P. Harbell and W. A. Sanders, “The American Society of Mechanical Engineers”, New York (1992) pp. 19–41.
7. 7) S. Yajima, J. Hayashi and M. Omori, Chem. Lett., 9, 931–934 (1975).
8. 8) F. Octavio, K. B. Rajendra, N. Daisy, K. Walter and M. Gunter, Adv. Eng. Mater., 16, 621–636 (2014).
9. 9) D. H. Ding, W. C. Zhou, X. Zhou, F. Luo and D. M. Zhu, Trans. Nonferrous Met. Soc. China., 22, 2726–2729 (2012).
10. 10) Y. X. Yu, X. Y. Tang and X. D. Li, Compos. Sci. Technol., 68, 1697–1703 (2008).
11. 11) G. E. Youngblood, C. Lewinsohn, R. H. Jones and A. Kohyama, J. Mater. Sci., 289, 1–9 (2001).
12. 12) J. J. Sha, T. Nozawa, J. S. Park, Y. Katoh and A. Kohyama, J. Nucl. Mater., 329, 592–596 (2004).
13. 13) A. R. Bunsell and A. Piant, J. Mater. Sci., 41, 823–839 (2006).
14. 14) R. Xie, J. Ilavsky, H. F. Huang, X. L. Zhou, C. Yang, Y. Z. Wang and H. J. Xu, J. Appl. Crystallogr., 49, 2155–2160 (2016).
15. 15) B. X. Sun, R. B. Xie, C. Yu, C. Li and H. J. Xu, J. Semicond., 38, 103002 (2017).10.1088/1674-4926/38/10/103002 ↗
16. 16) GB/T 3362-2005, Test methods for tensile properties of carbon fiber multifilament (2005).
17. 17) J. Langford and A. Wilson, J. Appl. Crystallogr., 11, 102–103 (1978).
18. 18) K. Suzuya, M. Furusaka and N. Watanabe, J. Mater. Res., 11, 1169–1178 (1996).
19. 19) A. Hammersley, EuropeanSynchrotron Radiation Facility (ESRF) 1987–1997.
20. 20) I. M. Lifshitz and V. V. Slyozov, J. Phys. Chem. Solids Pergamon Press., 19, 35–50 (1961).
21. 21) V. C. Wagner, Z. Elektrochem., 65, 581–591 (1961).