Microstructural observation of β-gallium oxide nanostructures after ammonolysis
Source abstract
Abstract
The reaction mechanism of β-gallium oxide (β-Ga2O3) to gallium nitride (GaN) under flowing ammonia was examined by observing the change in morphology according to the conversion of nanostructured β-Ga2O3 to GaN by ammonolysis. The morphology of the β-Ga2O3 nanostructures after ammonolysis was dependent on the experimental conditions (i.e. oxygen-rich and -deficient gas flow) for their growth. The surface of the β-Ga2O3 nanostructures grown in the oxygen-rich gas flow was striated after ammonolysis. On the other hand, the morphology of the β-Ga2O3 nanostructures grown in the oxygen-deficient gas flow was changed remarkably and diversely with maintaining their contour. These microstructural observations can be explained by the reaction mechanism, in which the ammonolysis of β-Ga2O3 to GaN consists of two successive reactions, the reduction of β-Ga2O3 to gaseous Ga2O and the nitridation of Ga2O(g) to GaN. The relative rates of the two reactions affect the morphology of the nitridated β-Ga2O3 nanostructures.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Ga2O3 and related materials · Advanced Photocatalysis Techniques · GaN-based semiconductor devices and materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Chemical Engineering, College of Engineering, Yeungnam University
References (21)
Show source-provided references
1. 1) J. Brendt, D. Samuelis, T. E. Weirich and M. Martin, Phys. Chem. Chem. Phys., 11, 3127–3137 (2009).10.1039/b901819k ↗
2. 2) W.-S. Jung and S.-A. Chae, Mater. Chem. Phys., 123, 610–613 (2010).10.1016/j.matchemphys.2010.05.023 ↗
3. 3) T. Suehiro, J. Tatami, T. Meguro, S. Matsuo and K. Komeya, Mater. Lett., 57, 910–913 (2002).10.1016/S0167-577X(02)00894-7 ↗
4. 4) T. Yamakawa, J. Tatami, T. Wakihara, K. Komeya, T. Meguro, K. J. D. MacKenzie, S. Takagi and M. Yokuchi, J. Am. Ceram. Soc., 89, 171–175 (2006).10.1111/j.1551-2916.2005.00693.x ↗
5. 5) W.-S. Jung, C. S. Ra and B.-K. Min, Bull. Korean Chem. Soc., 26, 1354–1358 (2005).10.5012/bkcs.2005.26.9.1354 ↗
6. 6) W.-S. Jung, Mater. Lett., 57, 110–114 (2002).10.1016/S0167-577X(02)00713-9 ↗
7. 7) C. M. Balkas and R. F. Davis, J. Am. Ceram. Soc., 79, 2309–2312 (1996).10.1111/j.1151-2916.1996.tb08977.x ↗
8. 8) H. Kiyono, T. Sakai, M. Takahashi and S. Shimada, J. Cryst. Growth, 312, 2823–2827 (2010).10.1016/j.jcrysgro.2010.06.021 ↗
9. 9) W.-S. Jung, Mater. Lett., 60, 2954–2957 (2006).10.1016/j.matlet.2006.02.022 ↗
10. 10) J. Q. Ning, S. J. Xu, P. W. Wang, Y. P. Song, D. P. Yu, Y. Y. Shan, S. T. Lee and H. Yang, Mater. Charact., 73, 153–157 (2012).10.1016/j.matchar.2012.08.013 ↗
11. 11) W.-S. Jung, J. Ceram. Soc. Japan, 121, 460–463 (2013).10.2109/jcersj2.121.460 ↗
12. 12) Q. N. Abdullah, F. K. Yam, Z. Hassan and M. Bououdina, Superlattices Microstruct., 54, 215–224 (2013).10.1016/j.spmi.2012.11.017 ↗
13. 13) S. Kumar and R. Singh, Phys. Status Solidi RRL, 7, 781–792 (2013).10.1002/pssr.201307253 ↗
14. 14) W.-S. Jung, H. J. Joo and B.-K. Min, Physica E, 36, 226–230 (2007).10.1016/j.physe.2006.12.001 ↗
15. 15) W.-S. Jung, Bull. Korean Chem. Soc., 27, 1963–1964 (2006).10.5012/bkcs.2006.27.12.1963 ↗
16. 16) R. Jalilian, M. M. Yazdanpanah, B. K. Pradhan and G. U. Sumanasekera, Chem. Phys. Lett., 426, 393–397 (2006).10.1016/j.cplett.2006.05.089 ↗
17. 17) H. W. Kim and S. H. Shim, Thin Solid Films, 515, 5158–5162 (2007).10.1016/j.tsf.2006.10.043 ↗
18. 18) L. Cao, M. K. Li, Z. Yang, Q. Wei and W. Zhang, Appl. Phys. A: Mater. Sci. Process., 91, 415–419 (2008).
19. 19) L. Binet and D. Gourier, J. Phys. Chem. Solids, 59, 1241–1249 (1998).10.1016/S0022-3697(98)00047-X ↗
20. 20) S. E. Collins, M. A. Baltanás and A. L. Bonivardi, Langmuir, 21, 962–970 (2005).10.1021/la0481389 ↗
21. 21) M. Imade, H. Kishimoto, F. Kawamura, M. Yoshimura, Y. Kitaoka, T. Sasaki and Y. Mori, J. Cryst. Growth, 312, 676–679 (2010).10.1016/j.jcrysgro.2009.12.028 ↗