Dielectric property of (001) one-axis oriented CaBi4Ti4O15-based thin films and their temperature dependence
Source abstract
Abstract
We proposed a thin-film capacitor with a stable temperature coefficient of capacitance (TCC) based on bismuth layer-structured dielectrics, CaBi4Ti4O15. Two types of doping were conducted to lower the dielectric loss in a higher temperature range above 300°C, i.e., Mn ion to compensate for lattice defects in crystalline grains and Bi12SiO20 to form a grain boundary phase were attempted in order to improve the insulating property of the oriented CaBi4Ti4O15 films. (00l) one-axis oriented Mn-doped or Bi12SiO20-doped CaBi4Ti4O15 films (with Mn or Bi12SiO20 content up to 3.0 or 1.75%) were fabricated successfully on (111)Pt/TiO2/(100)Si substrates buffered by (001)Ca2Nb3O10 nanosheets. These films exhibited a relatively lower loss factor in the temperature range from R.T. up to 400°C. In particular, the behavior of TCC on the Bi12SiO20-doped CaBi4Ti4O15 film was significantly stable, with a change in capacitance, ΔC/CR.T., within ±10% even at 400°C.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Multiferroics and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials and Life Sciences, Sophia University
Department of Innovative and Engineered Materials, Tokyo Institute of Technology
Institute for Material Research, Tohoku University
References (30)
Show source-provided references
1. 1) H.-S. Chin, K.-Y. Cheong and A. B. Ismail, Metall. Mater. Trans., B, Process Metall. Mater. Proc. Sci., 41B, 824–832 (2010).10.1007/s11663-010-9365-5 ↗
2. 2) C. Buttay, D. Planson, B. Allard, D. Bergogne, P. Bevilacqua, C. Joubert, M. Lazar, C. Martin, H. Morel, D. Tournier and C. Raynaud, Mater. Sci. Eng., B, 176, 283–288 (2011).10.1016/j.mseb.2010.10.003 ↗
3. 3) R. S. Pengelly, S. M. Wood, J. W. Milligan, S. T. Sheppard and W. L. Pribble, IEEE Trans. Microw. Theory Tech., 60, 1746–1783 (2012).10.1109/TMTT.2012.2187535 ↗
4. 4) P. Padmini, T. R. Taylor, M. J. Lefevre, A. S. Nagra, R. A. York and J. S. Speck, Appl. Phys. Lett., 75, 3186–3188 (1999).10.1063/1.125272 ↗
5. 5) C. B. Parker, J. P. Maria and A. I. Kingon, Appl. Phys. Lett., 81, 340–342 (2002).10.1063/1.1490148 ↗
6. 6) K. Takahashi, M. Suzuki, T. Kojima, T. Watanabe, Y. Sakashita, K. Kato, O. Sakata, K. Sumitani and H. Funakubo, Appl. Phys. Lett., 89, 082901 (2006).10.1063/1.2336626 ↗
7. 7) K. Takahashi, M. Suzuki, T. Oikawa, T. Kojima, T. Watanabe and H. Funakubo, Chem. Vap. Depos., 12, 136–142 (2006).10.1002/cvde.200506373 ↗
8. 8) J. Kimura, I. Takuwa, M. Matsushima, S. Yasui, T. Yamada and H. Funakubo, J. Appl. Phys. Lett., 114, 027002 (2013).
9. 9) Y. Park, M. Miyayama and T. Kudo, J. Ceram. Soc. Japan, 107, 413–418 (1999).10.2109/jcersj.107.413 ↗
10. 10) H. Irie and M. Miyayama, Appl. Phys. Lett., 79, 251–253 (2001).10.1063/1.1384480 ↗
11. 11) H. Irie, M. Miyayama and T. Kudo, J. Appl. Phys., 90, 4089–4094 (2001).10.1063/1.1389476 ↗
12. 12) Y. Mizutani, H. Uchida, H. Funakubo and S. Koda, Jpn. J. Appl. Phys., 48, 09KA10 (2009).10.1143/JJAP.48.09KA10 ↗
13. 13) Y. Mizutani, T. Kiguchi, T. J. Konno, H. Funakubo and H. Uchida, Jpn. J. Appl. Phys., 49, 09MA02 (2010).10.1143/JJAP.49.09MA02 ↗
14. 14) Y. Kondoh, K. Sasajima, M. Hayashi, J. Kimura, I. Takuwa, Y. Ehara, H. Funakubo and H. Uchida, Jpn. J. Appl. Phys., 50, 09NA04 (2011).10.1143/JJAP.50.09NA04 ↗
15. 15) J.-Y. Kim, C.-R. Song and H.-I. Yoo, J. Electroceram., 1, 27–39 (1997).10.1023/A:1009994230779 ↗
16. 16) C. Voisard, D. Damijanovic and N. Setter, J. Eur. Ceram. Soc., 19, 1251–1254 (1999).10.1016/S0955-2219(98)00414-2 ↗
17. 17) S. K. Singh and H. Ishiwara, Solid State Commun., 140, 430–434 (2006).10.1016/j.ssc.2006.09.022 ↗
18. 18) Y. Noguchi, K. Yamamoto, Y. Kitanaka and M. Miyayama, J. Eur. Ceram. Soc., 27, 4081–4084 (2007).10.1016/j.jeurceramsoc.2007.02.104 ↗
19. 19) Y. Nomura, Y. Hiruma, H. Nagata and T. Takenaka, Jpn. J. Appl. Phys., 49, 09MD02 (2010).10.1143/JJAP.49.09MD02 ↗
20. 20) R. Wasser and M. Klee, Integr. Ferroelectr., 2, 1–4 (1992).
21. 21) W. Huebner, S. C. Zhang, B. Gilmore, M. L. Krogh, B. C. Schultz, R. C. Pate, L. F. Rinehart and J. M. Lundstrom, Dig. Tech. Paper: IEEE Pul. Pow. Conf., 2, 1242–1245 (1999).
22. 22) M. Touzin, D. Goeuriot, C. Guerret-Piécourt, D. Juvé and H.-J. Fitting, J. Eur. Ceram. Soc., 30, 805–817 (2010).10.1016/j.jeurceramsoc.2009.09.025 ↗
23. 23) S. Ogawa, Y. Kondoh, J. Kimura, H. Funakubo and H. Uchida, Jpn. J. Appl. Phys., 51, 09LA16 (2012).10.1143/JJAP.51.09LA16 ↗
24. 24) H. Uchida, K. Sakurai, I. Okada, H. Matsuda, T. Iijima, T. Kojima, T. Watanabe and H. Funakubo, Jpn. J. Appl. Phys., 42, 5990–5993 (2003).10.1143/JJAP.42.5990 ↗
25. 25) Y. Ebina, T. Sasaki and M. Watanabe, Solid State Ionics, 151, 177–182 (2002).10.1016/S0167-2738(02)00707-5 ↗
26. 26) F. F. Xu, Y. Ebina, Y. Bando and T. Sasaki, J. Phys. Chem. B, 107, 9638–9645 (2003).10.1021/jp030136u ↗
27. 27) K. Kikuta, K. Noda, S. Okumura, T. Yamaguchi and S. Hirano, J. Sol-Gel Sci. Technol., 42, 381–387 (2007).10.1007/s10971-006-0200-z ↗
28. 28) T. Shibata, K. Fukuda, Y. Ebina, T. Kogure and T. Sasaki, Adv. Mater., 20, 231–235 (2008).10.1002/adma.200701381 ↗
29. 29) S. Agarwal, G. L. Sharma and R. Manchanda, Solid State Commun., 119, 681–686 (2001).10.1016/S0038-1098(01)00284-8 ↗
30. 30) J. D. Baniecki, J. S. Cross, M. Tsukada and J. Watanabe, Appl. Phys. Lett., 81, 3837–3839 (2002).10.1063/1.1519359 ↗