Fabrication of (K0.5Bi0.5)Bi4Ti4O15 ceramics and their electrical properties

Genta NISHIO, Hajime NAGATA, Tadashi TAKENAKA

Journal of the Ceramic Society of Japan· Volume 122· Issue 1426

Abstract

(K0.5(1+x)Bi0.5)Bi4Ti4O15 [KBT-10000x, 10000x = (−200)–7] were prepared by the conventional ceramic fabrication process using the KHCO3 powder as the starting material. KBT-0 ceramic indicated high density ratio of higher than 95% and high resistivity of approximately 1012 Ω·cm. A remanent polarization Pr, and coercive field Ec, are 10.4 µC/cm2 and 70.8 kV/cm, respectively. Additionally, a high relative density ratio and resistivity exceeding 97% and approximately 1014 Ω·cm were obtained in K-poor KBT-(−100) ceramics derived from KHCO3. This ceramic also indicated good ferroelectric and piezoelectric properties such as Pr of 12.6 µC/cm2, piezoelectric constant d33 of 16.0 pC/N and the mechanical quality factor Qm of 2366, respectively.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Multiferroics and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Faculty of Science and Technology, Tokyo University of Science

References (21)

Show source-provided references
1. 1) C. F. Buhrer, J. Chem. Phys., 36, 798–803 (1962).10.1063/1.1732613 ↗
2. 2) Y. Saito, H. Takao, T. Tani, T. Nonoyama, K. Takatori, T. Homma, T. Nagaya and M. Nakamura, Nature, 432, 84 (2004).10.1038/nature03028 ↗
3. 3) K. Kakimoto, I. Masuda and H. Ohsato, Jpn. J. Appl. Phys., 42, 6102 (2003).10.1143/JJAP.42.6102 ↗
4. 4) T. Takenaka, K. Maruyama and K. Sakata, Jpn. J. Appl. Phys., 30, 2236 (1991).10.1143/JJAP.30.2236 ↗
5. 5) Y. Hiruma, T. Watanabe, H. Nagata and T. Takenaka, Jpn. J. Appl. Phys., 47, 7659 (2008).10.1143/JJAP.47.7659 ↗
6. 6) M. Kimura, T. Minamikawa, A. Ando and Y. Sakabe, Jpn. J. Appl. Phys., 36, 6051 (1997).10.1143/JJAP.36.6051 ↗
7. 7) Y. Nakai, T. Eguchi, H. Nakakubo and S. Fukuoka, 102nd Annual Meet. Amer. Ceram. Soc., A2-026-00 (5/2/2000).
8. 8) G. A. Smolenskii, V. A. Isupov and A. I. Agranovskays, Sov. Phys. Solid State, 3, 651 (1961).
9. 9) E. C. Subbarao, J. Am. Ceram. Soc., 45, 166 (1962).10.1111/j.1151-2916.1962.tb11113.x ↗
10. 10) L. E. Cross and R. C. Pohanka, Mater. Res. Bull., 6, 939 (1971).10.1016/0025-5408(71)90072-9 ↗
11. 11) T. Takenaka and K. Sakata, Jpn. J. Appl. Phys., 19, 31 (1980).10.1143/JJAP.19.31 ↗
12. 12) S. Kawada, H. Ogawa, M. Kimura, K. Shiratsuyu and H. Niimi, Jpn. J. Appl. Phys., 45, 7455 (2006).10.1143/JJAP.45.7455 ↗
13. 13) H. Ogawa, S. Kawada, M. Kimura, K. Shiratsuyu and Y. Sakabe, IEEE Trans. Ultrason. Ferroelectr. Freq. Control, 54, 2500 (2007).10.1109/TUFFC.2007.567 ↗
14. 14) S. Kawada, H. Ogawa, M. Kimura, K. Shiratsuyu and Y. Higuchi, Jpn. J. Appl. Phys., 46, 7079 (2007).10.1143/JJAP.46.7079 ↗
15. 15) H. Ogawa, S. Kawada, M. Kimura, Y. Higuchi and H. Takagi, Jpn. J. Appl. Phys., 48, 09KD05 (2009).10.1143/JJAP.48.09KD05 ↗
16. 16) Doctor thesis: T. Takenaka (1984) p. 131.
17. 17) S. Ikegami and I. Ueda, Jpn. J. Appl. Phys., 13, 1572 (1974).10.1143/JJAP.13.1572 ↗
18. 18) C.-M. Wang and J.-F. Wang, J. Am. Ceram. Soc., 91, 918 (2008).10.1111/j.1551-2916.2007.02211.x ↗
19. 19) Y. Noguchi, M. Suzuki, Y. Kitanaka, S. Teranishi and M. Miyayama, Appl. Phys. Lett., 93, 032904 (2008).10.1063/1.2956397 ↗
20. 20) H. Nagata, S. Sato, Y. Hiruma and T. Takenaka, Appl. Phys. Express, 5, 011502 (2012).10.1143/APEX.5.011502 ↗
21. 21) K. Tabuchi, H. Nagata and T. Takenaka, J. Ceram. Soc. Japan, 121, 623 (2013).10.2109/jcersj2.121.623 ↗