Microstructural control of MgO–Al2O3–SiO2 glass-ceramics using titanium oxides with varying particle sizes and crystallinities as nucleation agents
Source abstract
Abstract
Microstructural control of MgO–Al2O3–SiO2 (MAS) glass-ceramic (GC) with precipitated enstatite (MgSiO3) in the 0.68–12 µm range from a parent glass having one composition was achieved by using titanium oxides with varying particle sizes and crystallinities as nucleation agents. Specifically, compared with the MAS-GC prepared using TiO2 with 50–200 nm and relative high crystallinity (TiO2-L-H), the MAS-GC prepared by mixing TiO2-L-H with TiO2 having single nanometer size and relative low crystallinity displayed an increase in the average crystal particle size from 6.0 to 12 µm with the preservation of volume fraction. In addition, compared with the MAS-GC prepared using TiO2-L-H, the MAS-GC prepared by TiO2 having single nanometer size and relative high crystallinity exhibited a decrease in the average size of crystal particle from 6.0 to 0. 68 µm with a decrease in the volume fraction from 76 to 67 %. Therefore, these results indicated that the particle size and crystallinity of the raw glass materials are key parameters for controlling the microstructure of GCs.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Recycling and utilization of industrial and municipal waste in materials production · Advanced ceramic materials synthesis · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Material Science and Technology, Faculty of Advanced Engineering, Tokyo University of Science
References (28)
Show source-provided references
1. 1) D. Stookey, US Patent 2 920 971 (Patented Jan. 12, 1960; Appl. June 4, 1956).
2. 2) A. V. Deceanne, L. R. Rodrigues, C. J. Wilkinson, J. C. Mauro and E. D. Zanotto, J. Non-Cryst. Solids, 591, 121714 (2022).10.1016/j.jnoncrysol.2022.121714 ↗
3. 3) J. Deubener, M. Allix, M. J. Davis, A. Duran, T. Höche, T. Honma, T. Komatsu, S. Krüger, I. Mitra, S. Müller, S. Nakane, M. J. Pascual, J. W. P. Schmelzeri, E. D. Zanotto and S. Zhou, J. Non-Cryst. Solids, 501, 3–10 (2018).10.1016/j.jnoncrysol.2018.01.033 ↗
4. 4) W. Höland and G. H. Beall, in “Glass-Ceramic Technology”, 3rd ed., Ed. by W. Höland and G. H. Beall, Wiley-America Ceramic Society, Hoboken, New Jersey (2019) pp. 67–357.10.1002/9781119423737 ↗
5. 5) M. Allix and L. Cormier, Crystallization and glassceramics, in “Springer Handbook of Glass”, 1st ed., Ed. by J. D. Musgraves, J. Hu and L. Calvez, Springer Nature, Switzerland (2019) pp. 113–168.10.1007/978-3-319-93728-1_4 ↗
6. 6) T. Homma, K. Maeda, S. Nakane and K. Shinozaki, J. Ceram. Soc. Jpn., 130, 545–551 (2022).10.2109/jcersj2.22037 ↗
7. 7) K. Maeda, M. Hirose and T. Kobayashi, J. Ceram. Soc. Jpn., 123, 949–954 (2015).10.2109/jcersj2.123.949 ↗
8. 8) G. H. Beall, J. Non-Cryst. Solids, 129, 163–173 (1991).10.1016/0022-3093(91)90092-K ↗
9. 9) Q. Fu, G. H. Beall and C. M. Smith, MRS Bull., 42, 220–225 (2017).10.1557/mrs.2017.31 ↗
10. 10) F. C. Serbena, I. Mathias, C. E. Foerster and E. D. Zanotto, Acta Mater., 86, 216–228 (2015).10.1016/j.actamat.2014.12.007 ↗
11. 11) K. Maeda, K. Akatsuka, G. Okuma and A. Yasumori, Crystals, 206, 393 (2021).10.3390/cryst11040393 ↗
12. 12) G. H. Beall, Annu. Rev. Mater. Sci., 22, 91–119 (1992).10.1146/annurev.ms.22.080192.000515 ↗
13. 13) L. Cormier, O. Dargaud, N. Menguy, G. S. Henderson, M. Guignard, N. Trcera and B. Watts, Cryst. Growth Des., 11, 311–319 (2011).10.1021/cg101318p ↗
14. 14) X. Zhou and M. Yamane, J. Ceram. Soc. Jpn., 96, 152–158 (1988).10.2109/jcersj.96.152 ↗
15. 15) K. Maeda, Y. Sera and A. Yasumori, J. Non-Cryst. Solids, 434, 13–22 (2016).10.1016/j.jnoncrysol.2015.12.001 ↗
16. 16) K. Maeda and A. Yasumori, J. Non-Cryst. Solids, 427, 152–159 (2015).10.1016/j.jnoncrysol.2015.07.040 ↗
17. 17) K. Katsumata, Y. Ohno, K. Tomita, T. Taniguchi, N. Matsushita and K. Okada, ACS Appl. Mater. Inter., 4, 4846–4852 (2012).10.1021/am301183t ↗
18. 18) Z. Strnad, in “Glass-Ceramic Materials”, Ed. by Z. Strnad, Elsevier, Amsterdam (1986) pp. 97–101.
19. 19) M. Chavoutier, D. Caurant, O. Majérus, R. Boulestiex, P. Loiseau, C. Jousseaume, E. Brunet and E. Lecomte, J. Non-Cryst. Solids, 384, 15–24 (2014).10.1016/j.jnoncrysol.2013.03.034 ↗
20. 20) O. Dargaud, G. Calas, L. Cormier, L. Galoisy, C. Jousseaume, G. Querel and M. Newville, J. Am. Ceram. Soc., 93, 342–344 (2010).10.1111/j.1551-2916.2009.03409.x ↗
21. 21) H. Hattori, Y. Ide and T. Sano, J. Mater. Chem. A, 2, 16381–16388 (2014).10.1039/C4TA02975E ↗
22. 22) K. Saito, M. Kozeni, M. Sohmiya, K. Komaguchi, M. Ogawa, Y. Sugahara and Y. Ide, Phys. Chem. Chem. Phys., 18, 30920–30925 (2016).10.1039/C6CP05635K ↗
23. 23) D. He, H. Ma and H. Zhong, J. Eur. Ceram. Soc., 41, 342–350 (2021).10.1016/j.jeurceramsoc.2021.09.034 ↗
24. 24) T. Benitez, A. Veber, K. P. Furlan, L. B. Rebouças, D. de Ligny, D. Hotza, A. P. N. de Oliveira and N. Travitzky, Int. J. Appl. Glass Sci., 11, 155–169 (2020).10.1111/ijag.13874 ↗
25. 25) N. Kumada, J. Ceram. Soc. Jpn., 121, 135–141 (2013).10.2109/jcersj2.121.135 ↗
26. 26) Y. Sugahara, J. Ceram. Soc. Jpn., 122, 523–529 (2014).10.2109/jcersj2.122.523 ↗
27. 27) S. Machida, N. Murayama, K. Maeda, K. Katsumata and A. Yasumori, J. Ceram. Soc. Jpn., 130, 850–856 (2022).10.2109/jcersj2.22088 ↗
28. 28) S. Machida, K. Maeda, K. Katsumata and A. Yasumori, Int. J. Appl. Glass Sci., 14, 88–96 (2023).10.1111/ijag.16609 ↗