journal article·2014Open access

Floating zone growth of cerium tetra-boride crystals

Shigeki OTANI, Hiroyo SEGAWA, Naoki OHASHI

Journal of the Ceramic Society of Japan· Volume 122· Issue 1423

Abstract

Single crystals of cerium tetra-boride, CeB4, were prepared in 0.4 MPa of argon ambient gas by the RF-heated floating zone method. The feed rod was prepared according to the following reaction formula: CeB6 + 1/2 (CeO2 + 2C) → 3/2 CeB4 + CO↑. The growth rate was 0.3 cm/h. The obtained crystal rods were 4 cm long and 1.2 cm in diameter. The lattice constants were a = 0.72052 nm and c = 0.40898 nm of a tetragonal lattice. The micro Vickers hardness, Hv, values on the (100), (110), and (001) planes were 1403, 1440, and 1099, respectively.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Advanced Materials Characterization Techniques · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Environment and Energy Materials Division, National Institute for Materials Science

Materials Research Center for Element Strategy, Tokyo Institute of Technology

References (11)

Show source-provided references
1. 1) T. B. Massalski, (Ed.) Binary Alloy Phase Diagram, 2nd edition, ASM, OH (1990).
2. 2) Z. Fisk, A. S. Cooper, P. H. Schmidt and R. N. Castellano, Mater. Res. Bull., 7, 285–288 (1972).10.1016/0025-5408(72)90205-X ↗
3. 3) K. H. J. Buschow and J. H. N. Creyghton, J. Chem. Phys., 57, 3910–3914 (1972).10.1063/1.1678862 ↗
4. 4) S. Otani and Y. Ishizawa, Prog. Cryst. Growth Charact., 23, 153–177 (1991).10.1016/0960-8974(92)90022-I ↗
5. 5) H. Segawa, T. Igarashi, T. Sakamoto, K. Mizuno, T. Konishi and S. Inoue, Int. J. Appl. Glass Sci., 4, 378–387 (2010).10.1111/j.2041-1294.2010.00034.x ↗
6. 6) S. Otani, M. M. Korsukova, T. Mitsuhashi and N. Kieda, J. Cryst. Growth, 217, 378–382 (2000).10.1016/S0022-0248(00)00513-3 ↗
7. 7) G. D. Sturgeon and H. A. Eick, J. Phys. Chem., 69, 3705–3708 (1965).10.1021/j100895a007 ↗
8. 8) J. A. Deacon and S. E. R. Hiscocks, J. Mater. Sci., 6, 309–312 (1971).10.1007/PL00020372 ↗
9. 9) A. Zalkin and D. H. Templeton, J. Chem. Phys., 18, 391 (1950).10.1063/1.1747637 ↗
10. 10) A. S. Bolgar, V. B. Muratov, A. V. Blinder, A. I. Kryklya and A. P. Suodis, J. Alloys Compd., 201, 127–128 (1993).10.1016/0925-8388(93)90872-K ↗
11. 11) V. Babizhetskyy, A. Simon and K. Hiebl, Z. Naturforsch., 62b, 896–900 (2007).10.1515/znb-2007-0704 ↗