journal article·2014Open access

Effects of N2/Ar gas ratio on phase formation and tribology of Ti–Si–N composite coatings prepared by hybrid PVD

Chan-Young PARK, Sung-Min LEE, Seong-Won KIM, Hyung-Tae KIM, Byung Koog JANG, Yoon-Suk OH

Journal of the Ceramic Society of Japan· Volume 122· Issue 1428

Abstract

Ti–Si–N hard coatings have been fabricated at different N2/Ar gas ratio (N2:Ar = 1:1, 1:2, or 1:3) sputtering conditions by the hybrid Physical Vapor Deposition (PVD) method, which consists of sputtering and arc ion plating (AIP). The pure silicon and titanium targets were selected for reactive sputtering and the AIP process, respectively. Field Emission Scanning Electron Microscopy (FESEM) and Energy Dispersive X-ray Spectroscopy (EDS) analysis has shown that the Ti/Si ratio increased as the Ar gas flow rate increased. Moreover, it found that the main growth plane of Ti–Si–N film was changed from (111) plane to (220) plane with increasing Ar gas flow from the results of X-ray diffraction (XRD) analysis. The wear rate of composite films was found to be lower than that of monolithic TiN with different friction coefficients at the initial running-in stage.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Engineering Ceramic Team, Korea Institute of Ceramic Engineering and Technology

High Temperature Materials Unit, National Institute for Materials Science

References (24)

Show source-provided references
1. 1) H. A. Jehn, Surf. Coat. Tech., 131, 433–440 (2000).10.1016/S0257-8972(00)00783-0 ↗
2. 2) D. V. Shtansky, P. V. Kiryukhantsev-Korneev, I. A. Bashkova, A. N. Sheveiko and E. A. Levashov, J. Refractory Met., 28, 32–39 (2010).10.1016/j.ijrmhm.2009.07.014 ↗
3. 3) L. Shizhi, Z. Cheng, X. Xiang, S. Yulong, Y. Hongshun, X. Yan and H. Wu, Surf. Coat. Tech., 43–44, 1007–1014 (1990).10.1016/0257-8972(90)90039-F ↗
4. 4) Z. T. Yang, B. Yang, L. P. Guo and D. J. Fu, Appl. Surf. Sci., 255, 4720–4724 (2009).10.1016/j.apsusc.2008.06.126 ↗
5. 5) S. Hayashi, T. Hirai, K. Hiraga and M. Hirabayashi, J. Mater. Sci., 17, 3336–3340 (1982).10.1007/BF01203503 ↗
6. 6) L. Shizhi, S. Yulong and P. Hongrui, Plasma Chem. Plasma Process., 12, 287–297 (1992).10.1007/BF01447027 ↗
7. 7) S. Veprek, S. Reiprich and L. Shizhi, Appl. Phys. Lett., 66, 2640–2642 (1995).10.1063/1.113110 ↗
8. 8) M. Diserens, J. Patscheider and F. Levy, Surf. Coat. Tech., 108–109, 241–246 (1998).10.1016/S0257-8972(98)00560-X ↗
9. 9) F. Vaz, L. M. Rebouta, S. Ramos, M. F. da Silva and J. C. Soares, Surf. Coat. Tech., 108–109, 236–240 (1998).10.1016/S0257-8972(98)00620-3 ↗
10. 10) F. J. Haug, L. Bonderer, P. Schwaller, J. Patscheider, M. Tobler and A. Karimi, Compos. Sci. Technol., 65, 799–803 (2005).10.1016/j.compscitech.2004.10.013 ↗
11. 11) S. H. Kim, J. W. Jang, S. S. Kang and K. H. Kim, J. Mater. Proc. Tech., 130–131, 283–288 (2002).10.1016/S0924-0136(02)00759-8 ↗
12. 12) R. F. Zhang and S. Veprek, Thin Solid Films, 516, 2264–2275 (2008).10.1016/j.tsf.2007.07.134 ↗
13. 13) M. P. Seah and T. S. Nunney, J. Phys. D: Appl. Phys., 43, 253001 (2010).
14. 14) J. L. He, C. K. Chen and M. H. Hon, Mater. Chem. Phys., 44, 9–16 (1996).10.1016/0254-0584(95)01655-E ↗
15. 15) F. Paumier, R. J. Gaboriaud and A. R. Kaul, Cryst. Eng., 5, 169–175 (2002).10.1016/S1463-0184(02)00026-6 ↗
16. 16) P. B. W. Burmester, G. Huber, M. Kurfiss and M. Schilling, Appl. Phys., A Mater. Sci. Process., 80, 627–630 (2005).10.1007/s00339-003-2250-1 ↗
17. 17) M. Jublot, F. Paumier, F. Pailloux, B. Lacroix, E. Leau, P. Guerin, M. Marteau, M. Jaouen, R. J. Gaboriaud and D. Imhoff, Thin Solid Films, 515, 6385–6390 (2007).10.1016/j.tsf.2006.11.177 ↗
18. 18) J. Iwasawa, R. Nishimizu, M. Tokita, M. Kiyohara and K. Uematsu, J. Am. Ceram. Soc., 90, 2327–2332 (2007).10.1111/j.1551-2916.2007.01738.x ↗
19. 19) L. Le Brizoual, A. Granier, F. Clenet, P. Briaud, G. Lemperiere and G. Turban, Surf. Coat. Tech., 116–119, 922–926 (1999).10.1016/S0257-8972(99)00133-4 ↗
20. 20) W. D. Sproul, D. J. Christie and D. C. Carter, Thin Solid Films, 491, 1–17 (2005).10.1016/j.tsf.2005.05.022 ↗
21. 21) D. M. Mattox, Handbook of Physical Vapor Deposition (PVD) Processing, Film Formation, Adhesion, Surface Preparation and Contamination Control, Ed. by the Society of Vacuum Coaters, Albuquerque, New Mexico (1998) pp. 142–145, 343–372.
22. 22) M. Kumar, S. Mishra and R. Mitra, Surf. Coat. Tech., 228, 100–114 (2013).10.1016/j.surfcoat.2013.04.014 ↗
23. 23) C. W. Zou, H. J. Wang, M. Li, Y. F. Yu, C. S. Liu, L. P. Guo and D. J. Fu, Vacuum, 84, 817–822 (2010).10.1016/j.vacuum.2009.10.050 ↗
24. 24) J. Prochazka, P. Karvankova, G. J. Martina, V. Heijman and S. Veprek, Mater. Sci. Eng., A, 384, 102–116 (2004).10.1016/j.msea.2004.05.046 ↗