Evaluation of Fracture Toughness of (0001) Twist Boundary Using Alumina Bicrystal
Source abstract
Abstract
Alumina bicrystals with (0001) twist boundary were fabricated by joining two alumina single crystals at 1900°C in Ar flow in a tungsten furnace. Single edge V-notched plate tension method was applied to evaluate the fracture toughness of the twist boundaries of the bicrystals. The fracture toughness of glass and single crystal alumina was also measured to make sure the validity of this method. The measured fracture toughness of (0001) twist boundaries were 3.6MPa√m at 0° twist angle, 2.8MPa√m at 10°, 2.1MPa at 28°, 1.8MPa√m at 38° and 2.7MPa√m at 60°, respectively. The dependence of twist angle of fracture toughness of grain boundary of alumina was discussed with changes in surface energy, boundary enemy and plastic dissipative energy.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · High-Velocity Impact and Material Behavior · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.