Synthesis and Thermal Behavior of Zirconium Oxynitride
Source abstract
Abstract
Zirconium oxynitrides (ZrON) were prepared by heating ZrO2 or ZrN powders in NH3 at 1100°C. Single phased β-ZrON and γ-ZrON were obtained by controlling the heating time. Tetragonal ZrO2 formed under some cases changed to monoclinic ZrO2 by mortar milling. Phase stability of β-ZrON against heating in the stream of N2-H2 gas mixture (3:1) was examined. β-ZrON was oxidized to form m-ZrO2 by heating below 1100°C for a long time. When β-ZrON was heated at 1000°C or higher temperature in a short time, β′-ZrON and a small amounts of m-ZrO2 and ZrN were formed. β′-ZrON and ZrN decreased and m-ZrO2 increased with heating time between 1000° and 1100°C. Three phases, i.e., β′-ZrON, m-ZrO2 and ZrN, coexisted above 1200°C, and the ratio of each phase was almost constant.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advancements in Solid Oxide Fuel Cells · Inorganic Chemistry and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.