article·2005-01-01Open access

Immobilization of Harmful Metallic Elements in HZr2(PO4)3

Hiroko Nakata, Katsuhiko Itoh, S. Nakayama

Abstract

Several harmful metal ions (M=Mn(II), Cu(II), Zn(II), Cd(II) and Pb(II)) were completely immobilized in the crystalline zirconium phosphate, HZr2(PO4)3, by thermal-treating the mixture of M(NO3)2 and HZr2(PO4)3 under the molar ratios of M(NO3)2/HZr2(PO4)3=0.1-0.5 at 700°C for 5 h. The XRD analyses suggested that all the M(II) immobilized products have the same structure as that of the NASICON-type HZr2(PO4)3. Such immobilized products were subjected to the leaching test of M(II) ion in 1 mol•dm-3 HCl at 160°C for 24 h. For the M(II) immobilized products with the ratio of M(NO3)2/HZr2(PO4)3=0.5, the leaching rate was decreased with the increase in ionic radius of M(II).
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Nuclear materials and radiation effects · Chemical Synthesis and Characterization · Inorganic Chemistry and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.