Comminution of Asbestos by a Mechanical Grinding and its Sinterability

Shinobu Hashimoto, Akira YAMAGUCHI

Abstract

When asbestos (chrysotile: Mg3Si2O5(OH)4) was heated at 600°C for 3 h, dehydration reaction of it had been almost finished, changing to an amorphous phase in crystallography. Then the remaining fiber became brittle, because the structure of fiber could be easily ground till <1 μm diameter in grain size using a mortar. When the compact body made by pressing the ground asbestos fiber at 80 MPa was heated at 1300°C for 1 h, the relative density of the compact reached 90%. Then the crystal phase of the compact was mainly forsterite (Mg2SiO4), but a small amount of chrinoenstatite (MgSiO3) was also detected.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Occupational and environmental lung diseases · Mineral Processing and Grinding · Advanced machining processes and optimization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.