article·1993-01-01Open access

Slip Casting of Silicon Nitride and Mechanical Properties of Sintered Body (Part 3)

Kazuyuki Ohshima, Kiichi Oda, Saburo Sano, Yasuo Shibasaki

Abstract

Slip casting of silicon nitride powder produced by imide decomposition (median particle size=0.55μm in diameter) was studied to fabricate Si3N4 engineering ceramic parts with a complicated shape. The zeta potential of α-Si3N4 showing the isoelectric point of pH=7.0 was +32mV at pH=2 and -47mV at pH=11. Preparation conditions of well-dispersed slurries were investigated for the mixed powders of 92wt% α-Si3N4, 4wt% α-Al2O3, and 4wt% Y2O3, using an organic polymer deflocculant (polyacrylic ammonium). High-density green bodies (density=1.76-1.82g/cm3) were prepared from the slurries containing solids of 67 to 70wt% by vacuum-filtration with a porous polymer resin mold. High-density Si3N4 ceramics were obtained by gas pressure sintering at 1775°C for 4h at about 0.9MPa of N2 pressure. The samples showed an average flexural strength of 814MPa and a Weibull modulus of 10.4 at room temperature.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Additive Manufacturing and 3D Printing Technologies · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.