Preparation and Oxidation Resistance of Carbon/Ceramic Composites Prepared from Phenolic Resin, B(OH)3 and Si(OC2H5)4
Source abstract
Abstract
To improve the oxidation resistance of carbon, B(OH)3 and Si(OC2H5)4 were dispersed in phenolic resin, and then carbonized at 1300°C, 1600°C and 1900°C. The oxidation resistance was investigated by TG-DTA. The results showed that the carbon/ceramic composites with 9mass% of SiO2:B(OH)3=0:1 had optimum oxidation resistance when heated at 1600°C. On the other hand, the sample with SiO2:B(OH)3=2:1 had optimum oxidation resistance when heated at 1900°C. Samples containing B(OH)3 were also heated to 1900°C and graphitic carbon was obtained.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Silicone and Siloxane Chemistry · Fiber-reinforced polymer composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.