Reactivity of High-Purity ZrSiO4 Sintered Bodies for Alkaline Glass Melts
Source abstract
Abstract
An experiment was conducted with reactivity of ZrSiO4 sintered bodies fabricated from synthesized high-purity ZrSiO4 powders for alkaline glass (2Na2O⋅SiO2) melts and change of their microstructure at 900°-1400°C. As evaluation of corrosion, comparison of the change of the weight loss and the corrosion depth of the ZrSiO4 sintered bodies with high-purity was made with zirconsand sintered bodies and ZrSiO4 sintered bodies with which treatment was performed by means of HIP. The corrosion reaction of three kinds of sintered bodies was liable to be governed by the melterosion mechanism, and it was known that the corrosion rate was dependent upon both purity and density of the ZrSiO4 sintered bodies. From the result of the comparison of TZP bodies with mullite sintered bodies, it was explained that the TZP bodies were corroded very hard. With respect to the mullite sintered bodies, 2Na2O⋅SiO2 melts severely dissolved them. It was ascertained that it was very important to heighten the density of the ZrSiO4 sintered bodies and to lower the reactivity with 2Na2O⋅SiO2 melts in order to heighten the stability in the 2Na2O⋅SiO2 melts. It was ascertained that it was likewise very important to heighten the stability of the ZrSiO4 at high temperatures by augmenting the purity of the ZrSiO4.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Glass properties and applications · Advanced ceramic materials synthesis · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.