Strength and Microstructure of Silicon Nitride Fabricated by Post-Sintering Process Using Low-Purity Silicon Powder as Raw Materials

Hideki Kita, Hideki Hyuga, Takene Hirai, Tateoki IIZUKA, Kazuo Ohsumi

Abstract

Influence of sintering temperature on the strength and micro-structure were investigated on silicon nitride specimens fabricated by pressureless post-sintering process using low-purity silicon powder as raw materials. Densification of reaction-bonded silicon nitride with sintering aid did not proceed further upon setting the post-sintering temperature at 1600 or 1650°C due to the volatilization of species and poor sinterbility. Sintering at 1850°C provided almost fully densified silicon nitride having an average strength of 521 MPa, the grains of this materials were relatively fine but did not develop into a rod-like shape.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.