Mechanical Properties of Hot-Pressed Si3N4-SiC Composites
Source abstract
Abstract
The composite with Si3N4 matrix, doped with 2wt% Al2O3 and 5wt% Y2O3, and 50wt% SiC powder having mean particle size of 0.3, 0.7 and 1.0μm were fabricated by hot-pressing at 1850°C under a pressure of 300kg/cm2 for 1 hour, and their mechanical properties were investigated. The composite with 0.3μm SiC showed a bending strength of 93kgf/mm2, which is slightly lower than that of monolithic Si3N4, 100kgf/mm2. The strength of the composite decreased with increasing mean particle size of SiC, suggesting that large size particle becomes defects in the sintered body. Fracture toughness of the composite, about 7MNm-3/2, doesn't depend on the particle size, and is almost same as that of monolithic Si3N4.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.