Abstract
Porous mullite ceramics were prepared by leaching glassy matrixes with a mixed acid from the sintered samples with compositions Al2O3/SiO2=1/3.3, 1/2, 1/1 and 3/2 in molar ratio. The shape of the mullite crystals were granular for the samples from submicron powder mixtures of Al2O3 and SiO2 sintered at 1400°-1600°C. Addition of CaO, MgO, BaO, TiO2, or Fe2O3 (5wt%) to the Al2O3-SiO2 system with composition Al2O3/SiO2=1/3.3 promoted the formation of elongated or needle-like mullite crystals. Effects of these oxides on the formation of mullite grains with high aspect ratio were discussed on the basis of the ternary phase diagrams. Average pore sizes of the leached porous mullite ceramics were in the range of 0.4-3μm, and became larger in the order of CaO>MgO>Fe2O3>none>BaO>TiO2 in additives. The pore size measured by mercury-penetration method agreed with that observed by SEM.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Recycling and utilization of industrial and municipal waste in materials production · Pigment Synthesis and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.