Fabrication of Si3N4 and Si3N4/SiC Composites by Pressureless Sintering Using Nitrate as Sintering Additives
Source abstract
Abstract
The effect of nitrates as sintering additives on the densification of Si3N4 based ceramics by pressureless sintering was compared with that of oxide additives. The surface of Si3N4 particles milled with a methanol solution of Al and Y nitrates, was coated with a layer containing Al, Y and O. Homogeneous distribution of sintering additives increased the sinterability of Si3N4. Monolithic Si3N4 with nitrate additives could be sintered to 94% T. D. at 1500°C. Furthermore, after pressureless sintering at 1750°C for 2h in N2, the bulk density of a Si3N4/20mass% SiC composite reached 95% T. D. with nitrate additives. The enhancement of densification in the case of nitrate additives was attributed to the enhancement of primary particle rearrangement due to the homogeneous distribution of liquid phase, a consequence of the homogeneous distribution of sintering additives, during sintering.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.