journal article·2007Open access

Detoxification of Sprayed Amosite

Hayami TAKEDA, Shinobu HASHIMOTO, Atsushi Okuda, Sawao HONDA, Hideo AWAJI, Koichiro FUKUDA

Journal of the Ceramic Society of Japan· Volume 115· Issue 1345

Abstract

According to XRD analysis, when sprayed amosite was heated at over 900°C for 3 h, amosite crystal was not detected in the sample. In contrast, a part of the needlelike amosite grains were not detected in the sprayed amosite using a phase-contrast microscope analysis after heating at 500°C for 3 h. Then the color of the needlelike amosite grains changed to red, because Fe2O3 (hematite) was precipitated at the surface of the amosite grains. The grindability of the needlelike amosite grains was improved with an increase of the heating temperature. When the sprayed amosite was heated at 1100°C for 3 h, a fine powder with under aspect ratio of 3 was obtained after grinding.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Radioactive element chemistry and processing · Nuclear materials and radiation effects · Iron oxide chemistry and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Environmental and Materials Engineering, Nagoya Institute of Technology

Fuji Seiku Kogyosho Corporation. Ltd.

References (6)

Show source-provided references
1. 10.2109/jcersj.114.71610.2109/jcersj.114.716 ↗
2. 10.2109/jcersj.114.115010.2109/jcersj.114.1150 ↗
3. 10.2109/jcersj.113.31210.2109/jcersj.113.312 ↗
4. 10.2109/jcersj.113.80410.2109/jcersj.113.804 ↗
5. 10.2109/jcersj.115.29010.2109/jcersj.115.290 ↗
6. R. W. Winson · Asbestos · 1975 · 384