Change of Electrical Properties of Co-Doped and Cr-Doped FeSi2 Thin Films during Amorphous-to-Crystalline Transformation
Source abstract
Abstract
The annealing temperature dependences of the XRD pattern, Seebeck coefficient and electrical resistivity for Cr-doped and Co-doped FeSi2 thin films were studied. The films were deposited by rf-sputtering method. Below 380°C, the films were amorphous and their Seebeck coefficient and electrical resistivity were relatively low. The crystallization of FeSi2 occurred at 400° to 460°C. The Seebeck coefficient (in absolute value) and electrical resistivity steeply increased with increasing amount of FeSi2 crystals in the amorphous matrix. Above 460°C, the electrical resistivity of the films gradually decreased with rising annealing temperature. The results of activation energy measurement explained the observed decrease of the electrical resistivity in Cr-doped thin films as due to both the increase of the carrier density and to the decrease of the activation energy.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and interfaces · Metallic Glasses and Amorphous Alloys · Copper Interconnects and Reliability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.