article·2001-01-01Open access

Forming Conditions of Iron-Disilicide by Slip Casting.

Kiyoshi Nogi, Takuji Kita, Xiang-Qun Yan

Abstract

Optimal slip conditions for molding of iron-disilicide were determined. The chemical compositions of the starting material were Fe0.91Mn0.09Si2 and Fe0.98Co0.02Si2. The mean particle diameters of both kinds of powder were approximately 6μm. The slip were prepared by adding distilled water to the powder, then, the hydrogen exponent (=pH) of the slips was controlled by adding 3% aqua ammonia. Ammonium alginate was used as a deflocculant as well as a binder. When the pH was greater than 7 for the Fe0.98Co0.02Si2 slip and greater than 8.5 for the Fe0.91Mn0.09Si2 slip, the apparent viscosity was low enough to enable casting. The pHs of the Fe0.98Co0.02Si2 slip and the Fe0.91Mn0.09Si2 slip were determined to be 7 and 8.5, respectively, because a higher pH slip corroded the plaster faster. Although the apparent viscosity increased with the powder concentration, castability was satisfied and the density of the sintered specimen did not depend on the powder concentration under the slip and sintering conditions of this study. Accordingly, the powder concentration was determined to be 77%, because the apparent viscosity of the slip was the lowest at this concentration. The shrinkage of the specimen before and after sintering was 17.1±0.3% and was independent of both the powder concentration and starting material. The ammonium alginate provided stability to the slip and improved the strength of the green body.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Intermetallics and Advanced Alloy Properties · Metallic Glasses and Amorphous Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.