The mechanism of curing of polycarbosilane (PCS) fiber has been investigated. Polycarbosilane has been melt-spun to fibers in the diameter range of 21-113μm. The rate of curing of PCS fiber was measured with a thermo-balance in Ar-O2 gas mixtures with 5-100kPa O2 at temperatures from 413K to 463K. The rate of curing increased with increasing curing temperature and pO2, and with decreasing fiber diameter. The fiber melted to agglomerate in a mass, depending on the curing temperature, pO2 in Ar-O2 gas mixtures and the size of fibers. A cured layer, through which oxygen molecules can advance and reach the reaction interface, was formed around the fiber. The reaction interface receded towards the center of the fiber as the curing progressed. In the early stage of curing, the kinetics followed the contracting-disc formula: 1-(1-X)1/2=κt. The apparent activation energy was 87.7kJ/mol. The rate constant κ was proportional to pO2 and was inversely proportional to the diameter of the fiber. It is considered that the curing of PCS fiber is controlled by the interfacial reaction. In the late stage of the reaction, curing is controlled by the diffusion of oxygen through the reaction layer.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fiber-reinforced polymer composites · Silicone and Siloxane Chemistry · Tribology and Wear Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.