article·1994-01-01Open access

Preparation of Chromium Boride Crystals Obtained from High-Temperature Metal Solutions

Shigeru Okada, Kunio Kudou, Kiyokata Iizumi, Katsuya Kudaka

Abstract

Chromium boride crystals were obtained by the high-temperature metal (copper, lead or tin) solutions using chromium metal and boron powders as starting materials in an argon atmosphere. CrB and CrB2 crystals were obtained as a single phase, however, Cr3B4 and Cr2B3 were obtained invariably as a phase mixture for various atomic ratios of the starting material in molten metal solutions. The largest CrB and CrB2 crystals were obtained from Cu solution. CrB crystals were obtained in the form of pillar shape extending to a-axis or c-axis and thin plates with well-developed {010} faces, and CrB2 crystals were obtained in the form of nearly spherical polyhedron. The largest crystals prepared had the maximum dimensions of about 0.12mm×0.13mm×3.30mm for CrB and 30μm for CrB2. The results of unit cell dimension and chemical analysis of CrB and CrB2 crystals are also present.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallurgical and Alloy Processes · Advanced materials and composites · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.