article·1996-01-01Open access

Dense PZT/PbTiO3 Ceramic Composite Prepared by O2 HIPing

Hisao Banno, Noriyasu Sugimoto, Takashi Hayashi

Abstract

In order to obtain a diphasic ceramic composite consisting of Pb(Zr, Ti)O3 (PZT) and PbTiO3, the following experiment was carried out. Raw materials were (1) Bi2O3- and Pb(W1/2Ni1/2)O3-modified PZT powder with a composition near the morphotropic phase boundary and average particle size of 0.6μm, pure PbTiO3 powders with average particle size of (2) 5μm and (3) 20μm. These powders were mixed at PZT/PbTiO3 mass ratios of 75/25, 50/50 and 25/75, pressed into disks and then fired at around 1000°C for 0.5h (short-time soak) or 12h (long-time soak). The short-time-soaked compact with PZT/PbTiO3 (20μm) mass ratio of 32.5/67.5 was hot-isostatically pressed (HIPed) at 1000°C and 200MPa in O2(5%)/Ar gas atmosphere for 1h without encapsulation. PZT/PbTiO3 diphasic ceramic composites were obtained at PZT/PbTiO3 mass ratios of 50/50 and 25/75 for (a) short-time soak (0.5h) with 5μm and 20μm PbTiO3 powders and (b) long-time soak (12h) with 20μm PbTiO3 powder, although their relative densities were 50-70%. The HIPed compact was a PZT/PbTiO3 diphasic ceramic composite with 95% relative density. The composition of the reacted PZT in the ceremic composite was shifted to the tetragonal (Ti-rich) side from that of starting PZT powder and compositional fluctuation was observed, while that of PbTiO3 was not detected by X-ray analysis.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electrophoretic Deposition in Materials Science

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.