journal article·2015Open access

Preparation of mullite-zirconia composites from waste foundry sand and alumina

Ruofei XIANG, Yuanbing LI, Shujing LI, Yawei LI, Shaobai SANG

Journal of the Ceramic Society of Japan· Volume 123· Issue 1441

Abstract

Waste foundry sand (WFS) collected from lost foam casting (LFC) is adopted to prepare low cost mullite-zirconia composites with the addition of alumina by reaction sintering. The mixture samples of WFS and alumina as well as samples containing only WFS are sintered from 1200 to 1600°C. Thermal shock behaviors are evaluated by cool water quenching test with temperature differentials (ΔT) between 200–1000°C and 1–4 repeated cycles for ΔT = 1000°C. The degree of damage with thermal shock severity is measured through dynamic elastic modulus E using the impulse excitation method. The result shows that mullite-zirconia composites can be successfully manufactured at 1500 and 1600°C, but the thermal shock (TS) resistance for composites sintered at 1600°C is not satisfied. The critical temperature gradient (ΔTc) is below 200°C, and after three TS cycles with ΔT = 1000°C, the E/E0 reduced to a nearly constant.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Materials Engineering and Processing · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

The State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology

References (17)

Show source-provided references
1. 1) R. Siddique and G. Singh, Resour. Conserv. Recycl., 55, 885–892 (2011).10.1016/j.resconrec.2011.05.001 ↗
2. 2) A. Deng and P. J. Tikalsky, Waste Manage., 28, 2161–2170 (2008).10.1016/j.wasman.2007.09.018 ↗
3. 3) G. Singh and R. Siddique, Constr. Build. Mater., 26, 416–422 (2012).10.1016/j.conbuildmat.2011.06.041 ↗
4. 4) N. Pathak and R. Siddique, Constr. Build. Mater., 34, 512–521 (2012).10.1016/j.conbuildmat.2012.02.026 ↗
5. 5) N. Quijorna, A. Coz, A. Andres and C. Cheeseman, Resour. Conserv. Recycl., 65, 1–10 (2012).10.1016/j.resconrec.2012.05.004 ↗
6. 6) E. Furlani, G. Tonello, E. Aneggi and S. Maschio, Ceram. Int., 38, 2619–2625 (2012).10.1016/j.ceramint.2011.11.065 ↗
7. 7) S. Ananthakumar, M. Jayasankar and K. G. K. Warrier, Acta Mater., 54, 2965–2973 (2006).10.1016/j.actamat.2006.02.032 ↗
8. 8) H. Schneider, J. Schreuer and B. Hildmann, J. Eur. Ceram. Soc., 28, 329–344 (2008).10.1016/j.jeurceramsoc.2007.03.017 ↗
9. 9) S. K. Zhao, Y. Huang, C. A. Wang, X. X. Huang and J. K. Guo, Ceram. Int., 29, 49–53 (2003).10.1016/S0272-8842(02)00088-3 ↗
10. 10) Y. Dong, X. Feng, X. Feng, Y. Ding, X. Liu and G. Meng, J. Alloy. Compd., 460, 599–606 (2008).10.1016/j.jallcom.2007.06.023 ↗
11. 11) C. Y. Chen, G. S. Lan and W. H. Tuan, J. Eur. Ceram. Soc., 20, 2519–2525 (2000).10.1016/S0955-2219(00)00125-4 ↗
12. 12) A. Kaiser, M. Lobert and R. Telle, J. Eur. Ceram. Soc., 28, 2199–2211 (2008).10.1016/j.jeurceramsoc.2007.12.040 ↗
13. 13) S. Zhao, Y. Huang, C. Wang, X. Huang and J. Guo, Mater. Lett., 57, 1716–1722 (2003).10.1016/S0167-577X(02)01057-1 ↗
14. 14) H. J. Kleebe, F. Siegelin, T. Straubinger and G. Ziegler, J. Eur. Ceram. Soc., 21, 2521–2533 (2001).10.1016/S0955-2219(01)00275-8 ↗
15. 15) R. C. Stiffler and D. P. H. Haselma, J. Am. Ceram. Soc., 66, C52–C53 (1983).
16. 16) N. M. Rendtorff, L. B. Garrido and E. F. Aglietti, Ceram. Int., 34, 2017–2024 (2008).10.1016/j.ceramint.2007.07.035 ↗
17. 17) N. M. Rendtorff, L. B. Garrido and E. F. Aglietti, Mater. Sci. Eng., A, 498, 208–215 (2008).10.1016/j.msea.2008.08.036 ↗