Fabrication of Porous Alumina Ceramics from a Technique for Making a Cake
Source abstract
Abstract
We fabricated porous alumina ceramics from a technique for making a cake. Polyvinyl alcohol (PVA), methyl cellulose (MC), and granulated sugar (SUGAR) were used as additives to give the alumina slurry the foaming property and the foam stability. The alumina slurry with PVA, MC, and SUGAR became creamy by mixing for 2.5 min by an electric mixer at 940 rpm. The creamy alumina slurry was able to be extruded by a forcing bag and smoothed by a blade. The creamy alumina slurry dried at 45°C, and then was sintered at 1600°C to a density of about 20%. The pore sizes in the sintered porous alumina ceramics were 0.2 mm or less. The flexural strength of sintered porous alumina ceramics with 78% porosity was 12 MPa.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Bauxite Residue and Utilization · Anodic Oxide Films and Nanostructures · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.