Heat Resistance of Si3N4 Joined with Ni-Cr Alloy Interlayer
Source abstract
Abstract
Joining strength of Si3N4 with a 80wt%Ni-20wt%Cr alloy interlayer was evaluated by a four point bending test at elevated temperatures in air. After holding at 1273K for 3.6ks, the average joining strength was 220MPa, which was almost the same as room temperature strength. Furthermore, after annealing for 75ks at 973K in air, the strength of the joints at room temperature did not decrease.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.