Synthesis and Pyrolysis of Thermosetting Copolymer of Polysilastyrene and Perhydropolysilazane

O. Funayama, H. Morozumi, M. Okoda, Takeshi Isoda

Abstract

Copolymer of polysilastyrene and perhydropolysilazane was obtained by the reaction of polysilastyrene with zirconium n-butoxide and perhydropolysilazane. Zirconium n-butoxide and perhydropolysilazane were essential to render the thermosetting property. The thermosetting copolymers were converted into silicon carbide-based ceramics by pyrolysis at 1000°C in a stream of N2 with about 80 mass% ceramic yield. The main phase of the pyrolysis product at 1500°C in N2 was small crystallite β-SiC. Free carbon, based on rule-of-mixtures composition in the final ceramics could be reduced by varying the ratio of polysilastyrene/perhydropolysilazane. The copolymer was dry spun and pyrolyzed to produce a ceramic fiber. Pyrolysis in N2 at 1500°C yielded a silicon carbide-based fiber. Tensile strength of 1.0 GPa and elastic modulus of 190 GPa were obtained for the fiber from 10 to 12μ in diameter. Crystallization to α-Si3N4, β-Si3N4, β-SiC, and ZrN proceeded on annealing in N2 at 1700°C for 1 h.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Silicone and Siloxane Chemistry · Synthesis and properties of polymers

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.