article·1990-01-01Open access

Hot-Pressing of Ti(C, N)-Cr3C2-Al2O3 Mixed Powder

Tadahiko Watanabe, Kazuhisa Shobu, Yukio Kai

Abstract

Cutting tools of Ti(C, N)-Cr3C2 ceramics have better wear resistance than those of TiC-TiN cermets and WC-Co alloy tools for carbon steel. Sintered bodies of this system have the fracture toughness K1C of 2.5MPa⋅m1/2. Higher fracture toughness is necessary for wider application. Therefore, addition of Al2O3 to Ti(C, N)-Cr3C2 system is tried. The main results are as follows:(1) Ti(C, N)-5wt% Cr3C2-Al2O3 sintered bodies containing 30-50wt% Al2O3 have the porosity of 0.1vol%, K1C of 4.2MPa⋅m1/2, transverse rupture strength of about 700MPa, and Vickers hardness of 1850Hv.(2) These sintered bodies consist of (Ti, Cr) (C, N, O) and Al2O3.(3) It is thought that high K1C is due to high toughness of Al2O3 grains and grain boundaries between (Ti, Cr) (C, N, O) and Al2O3.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Powder Metallurgy Techniques and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References