Influence of Al2O3 Addition on the Sintering Behavior of NiO-CoO Solid Solution
Source abstract
Abstract
Sintering behavior of (Ni, Co) O was investigated measuring linear shrinkage as a function of Al2O3 addition. Morphological study was also attempted for the samples sintered at 1280°C for 10h. The added Al2O3 reacted with the (Ni, Co) O matrix to form (Ni, Co) Al2O4 spinel from 800 to 1200°C. The addition of Al2O3 inhibited the growth of (Ni, Co) O particles, and then decreased the linear shrinkage from 800 to 1100°C. Above 1150°C, in contrast to the constant linear shrinkage of (Ni, Co) O, (Ni, Co) O with Al2O3 showed steep linear shrinkage behavior. Furthermore, at 1400°C, the linear shrinkage for (Ni, Co) O without Al2O3 and with Al2O3 was 14 and 18%, respectively. The microstructure of the quenched samples showed that number of (Ni, Co) Al2O4 spinel precipitates decreased above 1150°C. The average grain size of the samples sintered at 1280°C for 10h decreased from 11 to 4μm with increasing Al2O3 additive from 0.5 to 8mass%; the addition of Al2O3 inhibited the grain growth of matrix in the final stage of sintering.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Advanced materials and composites · Powder Metallurgy Techniques and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.