Martensitic Transformation Effect on the Dislocation Emission from a Semi-infinite Crack Tip in Nanocomposites
Source abstract
Abstract
A theoretical model is established to investigate the effect of martensitic transformation particle on the dislocation emission from a crack tip in ceramic-matrix nanocomposites. Using the model of dislocation-based strain nucleus and the Green’s function method, the expressions of complex potentials and stress fields are derived in closed form. The critical stress intensity factors for the first-lattice dislocation emission and the maximum number of emitted dislocations are well calculated. The effects of important parameters such as the size of transformation particle, the dislocation emission angle and the distance from the crack tip to the transformation particle on dislocation emission are discussed in detail. The results reveal that the transformation particle shows a significant shielding effect on the dislocation emission from the crack tip, and the shielding effect enhances with an increase in the size of transformation particle. On the other hand, the results also imply that the emission of edge dislocations is closely related with the dislocation emission angle, and there exists a probable angle $${\vert }{\theta }{\vert }\approx 74\circ $$ making the dislocation emission easiest. Besides, the remarkable crack blunting induced by the dislocation emission is quite difficult for small grain size but easy for the growth of crack.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Ferroelectric and Piezoelectric Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Chevalier J, Gremillard L. Ceramics for medical applications: a picture for the next 20 years. J Eur Ceram Soc. 2009;29(7):1245–55.10.1016/j.jeurceramsoc.2008.08.025 ↗
2. Kirsten A, Begand S, Oberbach T, Telle R, Fischer H. Subcritical crack growth behavior of dispersion oxide ceramics. J Biomed Mater Res Part B Appl Biomater. 2010;95B(1):202–6.10.1002/jbm.b.31703 ↗
3. Sun X, Han W, Liu Q, Hu P, Hong C. ZrB $$_2$$ 2 -ceramic toughened by refractory metal Nb prepared by hot-pressing. Mater Des. 2010;31(9):4427–31.10.1016/j.matdes.2010.04.020 ↗
4. Zhu YF, Shi L, Liang J, Hui D, Lau KT. Synthesis of zirconia nanoparticles on carbon nanotubes and their potential for enhancing the fracture toughness of alumina ceramics. Compos Part B Eng. 2008;39(7–8):1136–41.10.1016/j.compositesb.2008.03.006 ↗
5. Li M, Schaffer H, Soboyejo WO. Transformation toughening of NiAl composites reinforced with yttria partially stabilized zirconia particles. J Mater Sci. 2000;35(6):1339–45.10.1023/A:1004769705123 ↗
6. Liu Y, Zhou J, Shen T. Effect of nano-metal particles on the fracture toughness of metal–ceramic composite. Mater Des. 2013;45(6):67–71.10.1016/j.matdes.2012.08.065 ↗
7. Kuntz JD, Zhan GD, Mukherjee AK. Nanocrystalline-matrix ceramic composites for improved fracture toughness. Mrs Bull. 2004;29(1):22–7.10.1557/mrs2004.12 ↗
8. Rao PG, Iwasa M, Tanaka T, Kondoh I, Inoue T. Preparation and mechanical properties of Al $$_2$$ 2 O $$_3$$ 3 —15 wt% ZrO $$_2$$ 2 composites. Scr Mater. 2003;48(4):437–41.10.1016/S1359-6462(02)00440-2 ↗
9. Szutkowska M, Boniecki M. Subcritical crack growth in zirconia-toughened alumina (ZTA) ceramics. J Mater Process Technol. 2006;175(1):416–20.10.1016/j.jmatprotec.2005.04.030 ↗
10. Yang G, Li JC, Wang GC, Min SL, Chen TC, Yashima M. Investigation on strengthening and toughening mechanisms of Ce-TZP/Al $$_2$$ 2 O $$_3$$ 3 nanocomposites. Metall Mater Trans A. 2006;37(6):1969–75.10.1007/s11661-006-0139-2 ↗
11. Basu B, Vleugels J, Biest OVD. ZrO $$_2$$ 2 –Al $$_2$$ 2 O $$_3$$ 3 composites with tailored toughness. J Alloys Compd. 2004;372(1–2):278–84.10.1016/j.jallcom.2003.09.157 ↗
12. Ma W, Wen L, Guan R, Sun X, Li X. Sintering densification, microstructure and transformation behavior of Al $$_2$$ 2 O $$_3$$ 3 /ZrO $$_2$$ 2 (Y $$_2$$ 2 O $$_3$$ 3 ) composites. Mater Sci Eng A. 2008;477(1):100–6.10.1016/j.msea.2007.06.058 ↗
13. Xin W, Tian J, Yu X, Yan S, Liu Z, Yin Y. Effect of microstructure on the fracture behavior of micro-nano ZTA composite. Mater Chem Phys. 2008;112(1):213–7.10.1016/j.matchemphys.2008.05.041 ↗
14. Hannink RHJ, Kelly PM, Muddle BC. Transformation toughening in zirconia-containing ceramics. J Am Ceram Soc. 2000;83(3):461–87.10.1111/j.1151-2916.2000.tb01221.x ↗
15. Hu J, Zhang Q, Liu Y, Wu G. Phase transformation behaviors of TiNi fibers embedded in an aluminum matrix. J Alloys Compd. 2014;589(5):491–7.10.1016/j.jallcom.2013.12.048 ↗
16. Liang YM, Zhao JH. Effect of zirconia particle size distribution on the toughness of zirconia-containing ceramics. J Mater Sci. 1999;34(9):2175–81.10.1023/A:1004588516105 ↗
17. Wang S, Li Y, Zhang X. Influence of the microstructure evolution of ZrO $$_2$$ 2 fiber on the fracture toughness of ZrB $$_2$$ 2 –SiC nanocomposite ceramics. Mater Des. 2013;49(49):808–13.10.1016/j.matdes.2013.01.039 ↗
18. Evans AG, Burlingame N, Drory M, Kriven WM. Martensitic transformations in zirconia–particle size effects and toughening. Acta Metall. 1981;29(2):447–56.10.1016/0001-6160(81)90170-X ↗
19. Mcmeeking RM, Evans AG. Mechanics of transformation-toughening in brittle materials. J Am Ceram Soc. 1982;65(5):242–6.10.1111/j.1151-2916.1982.tb10426.x ↗
20. Cai H, Faber KT. Effective dilatational transformation toughening in brittle materials. Scr Metall Mater. 1993;28(9):1161–6.10.1016/0956-716X(93)90027-P ↗
21. Li Q, Lv J, Hou J, Zuo H. Crack-tip shielding by the dilatant transformation of particles/fibers embedded in composite materials. Theor Appl Fract Mech. 2015;80:242–52.10.1016/j.tafmec.2015.06.005 ↗
22. He T, Xiao W, Zhang Y, Zhu H. Effect of cooperative grain boundary sliding and migration on dislocation emission from a branched crack tip in deformed nanocrystalline solids. Int J Fract. 2017;206(1):1–10.10.1007/s10704-017-0193-3 ↗
23. He T, Feng M. Influence of nanoscale deformation twins near a slant edge crack tip on crack blunting in nanocrystalline metals. Eng Fract Mech. 2017;184:286–95.10.1016/j.engfracmech.2017.08.007 ↗
24. Zhan GD, Kuntz J, Wan J, Garay J, Mukherjee AK. A novel processing route to develop a dense nanocrystalline alumina matrix ( $$<100 \text{ nm }$$ < 100 nm ) nanocomposite material. J Am Ceram Soc. 2003;86(1):200–2002.10.1111/j.1151-2916.2003.tb03306.x ↗
25. Kurland HD, Grabow J, Müller FA. Preparation of ceramic nanospheres by CO laser vaporization (LAVA). J Eur Ceram Soc. 2011;31(14):2559–68.10.1016/j.jeurceramsoc.2011.01.010 ↗
26. Bartolomé JF, Smirnov A, Kurland HD, Grabow J, Müller FA. New ZrO $$_2$$ 2 /Al $$_2$$ 2 O $$_3$$ 3 nanocomposites fabricated from hybrid nanoparticles prepared by CO $$_2$$ 2 laser co-vaporisation. Sci Rep. 2016;6:20589.10.1038/srep20589 ↗
27. Deville S, Chevalier J, Dauvergne C, Fantozzi G, Bartolomé JF, Moya JS, Torrecillas R. Microstructural investigation of the aging behavior of (3Y-TZP)-Al $$_2$$ 2 O $$_3$$ 3 composites. J Am Ceram Soc. 2005;88(5):1273–80.10.1111/j.1551-2916.2005.00221.x ↗
28. Muskhelishvili NI. Some basic problems of the mathematical theory of elasticity. Math Gaz. 1953;48(365):351.
29. Suo Z. Singularities interacting with interfaces and cracks. Int J Solids Struct. 1989;25(10):1133–42.10.1016/0020-7683(89)90072-3 ↗
30. Ma L. Fundamental formulation for transformation toughening. Int J Solids Struct. 2010;47(22–23):3214–20.10.1016/j.ijsolstr.2010.08.002 ↗
31. Hirth JP, Lothe J, Mura T. Theory of dislocations. 2nd ed. Hoboken: Wiley; 1983.
32. Zhang T-Y, Li J. Image forces and shielding effects of an edge dislocation near a finite length crack. Acta Metall Mater. 1991;39(11):2739–44.10.1016/0956-7151(91)90091-E ↗
33. Rice J, Thomson Robb. Ductile versus brittle behaviour of crystals. Philos Mag. 1974;29(1):73–97.10.1080/14786437408213555 ↗
34. Callister WD, Rethwisch DG. Materials science and engineering. Hoboken: Wiley; 2011.
35. Zhang HT, Ming Z. Microcracks related to dilational transformation in ceramics. J Mater Sci Lett. 1996;15(23):2055–7.10.1007/BF00278620 ↗
36. Huang M, Li Z. Dislocation emission criterion from a blunt crack tip. J Mech Phys Solids. 2004;52(9):1991–2003.10.1016/j.jmps.2004.03.003 ↗