journal article·2020-12Open access

Defect structure process maps for laser powder bed fusion additive manufacturing

Jerard V. Gordon, Sneha P. Narra, Ross W. Cunningham, He Liu, Hangman Chen, Robert M. Suter, Jack L. Beuth, Anthony D. Rollett

Abstract

Accurate detection, characterization, and prediction of defects has great potential for immediate impact in the production of fully-dense and defect free metal additive manufacturing (AM) builds. Accordingly, this paper presents Defect Structure Process Maps (DSPMs) as a means of quantifying the role of porosity as an exemplary defect structure in powder bed printed materials. Synchrotron-based micro-computed tomography (μSXCT) was used to demonstrate that metal AM defects follow predictable trends within processing parameter space for laser powder bed fusion (LPBF) materials. Ti-6Al-4 V test blocks were fabricated on an EOS M290 utilizing variations in laser power, scan velocity, and hatch spacing. In general, characteristic under-melting or lack-of-fusion defects were discovered in the low laser power, high scan velocity region of process space via μSXCT. These defects were associated with insufficient overlap between adjacent melt tracks and can be avoided through the application of a lack-of-fusion criterion using melt pool geometric modeling. Large-scale keyhole defects were also successfully mitigated for estimated melt pool morphologies associated with shallow keyhole front wall angles. Process variable selections resulting in deep keyholes, i.e., high laser power and low scan velocity, exhibit a substantial increase of spherical porosity as compared to the nominal (manufacturer recommended) processing parameters for Ti-6Al-4 V. Defects within fully-dense process space were also discovered, and are associated with gas porosity transfer to the AM test blocks during the laser-powder interaction. Overall, this work points to the fact that large-scale defects in LPBF materials can be successfully predicted and thus mitigated/minimized via appropriate selection of processing parameters.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Porosity measurements and analysis for metal additive manufacturing process control10.6028/jres.119.019 ↗
2. XCT analysis of the influence of melt strategies on defect population in Ti-6Al-4V components manufactured by Selective Electron beam Melting10.1016/j.matchar.2015.02.008 ↗
3. Analyzing the effects of powder and post-processing on porosity and properties of electron beam melted Ti-6Al-4V10.1080/21663831.2017.1340911 ↗
4. Analysis of defect generation in Ti-6Al-4V parts made using powder bed fusion additive manufacturing processes
5. Review of in-situ process monitoring and in-situ metrology for metal additive manufacturing10.1016/j.matdes.2016.01.099 ↗
6. Process mapping for qualification across multiple direct metal additive manufacturing processes
7. Overview of materials qualification needs for metal additive manufacturing10.1007/s11837-015-1810-0 ↗
8. Cunningham · 2018
9. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
10. Metal additive manufacturing: a review of mechanical properties10.1146/annurev-matsci-070115-032024 ↗
11. Porosity formation and gas bubble retention in laser metal deposition10.1007/s00339-009-5266-3 ↗
12. Kou · 2003
13. Mechanical behavior of additive manufactured, powder-bed laser-fused materials10.1016/j.msea.2015.10.068 ↗
14. Fatigue performance of additive manufactured metallic parts10.1108/13552541311302932 ↗
15. Fatigue performance evaluation of selective laser melted Ti-6Al-4V10.1016/j.msea.2014.01.041 ↗
16. Influence of defects, surface roughness and HIP on the fatigue strength of Ti-6Al-4V manufactured by additive manufacturing10.1016/j.ijfatigue.2018.07.020 ↗
17. 3D imaging and quantification of porosity in electron beam welded dissimilar steel to Fe-Al alloy joints by X-ray tomography10.1016/j.matdes.2016.02.010 ↗
18. The effect of Ar and N 2 shielding gas on laser weld porosity in steel, stainless steels, and nickel
19. Process optimization of dual-laser beam welding of advanced Al-Li alloys through hot cracking susceptibility modeling10.1007/s11661-016-3509-4 ↗
20. Prediction of lack-of-fusion porosity for powder bed fusion
21. Transient dynamics of powder spattering in laser powder bed fusion additive manufacturing process revealed by in-situ high-speed high-energy x-ray imaging10.1016/j.actamat.2018.03.036 ↗
22. Keyhole threshold and morphology in laser melting revealed by ultrahigh- speed X-ray imaging10.1126/science.aav4687 ↗
23. Balling phenomena during direct laser sintering of multi-component Cu-based metal powder10.1016/j.jallcom.2006.06.011 ↗
24. Instability of scan tracks of selective laser sintering of high speed steel powder10.1016/S1359-6462(99)00276-6 ↗
25. Synchrotron-based X-ray microtomography characterization of the effect of processing variables on porosity formation in laser power-bed additive manufacturing of Ti-6Al-4V10.1007/s11837-016-2234-1 ↗
26. 3D shape analysis of powder for laser beam melting by synchrotron X-ray CT10.3390/qubs3010003 ↗
27. ImageJ2: ImageJ for the next generation of scientific image data10.1186/s12859-017-1934-z ↗
28. Ilastik: Interactive learning and segmentation toolkit
29. Effects of defects in laser additive manufactured Ti-6Al-4V on fatigue properties10.1016/j.phpro.2014.08.120 ↗
30. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
31. The effectiveness of hot isostatic pressing for closing porosity in titanium parts manufactured by selective Electron beam melting10.1007/s11661-016-3429-3 ↗
32. Melt pool characterization for selective laser melting of Ti-6Al-4V pre-alloyed powder
33. Francis
34. Inclusions, porosity, and fatigue of AlSi10Mg parts produced by selective laser melting10.1016/j.ijfatigue.2016.06.002 ↗
35. Build rate optimization for powder bed fusion
36. Mathematical theory of heat distribution during welding and cutting
37. Cooling rates and peak temperatures in fusion welding
38. Heat transfer and fluid flow during keyhole mode laser welding of tantalum, Ti-6Al-4V, 304L stainless steel and vanadium10.1088/0022-3727/40/18/037 ↗
39. Observation of keyhole-mode laser melting in laser powder-bed fusion additive manufacturing10.1016/j.jmatprotec.2014.06.005 ↗
40. Eagar
41. Elmer · 1990 · 167
42. Physical processes in fusion welding10.1103/RevModPhys.67.85 ↗
43. In situ absorptivity measurements of metallic powders during laser powder-bed fusion additive manufacturing10.1016/j.apmt.2017.08.006 ↗
44. Keyhole modeling during laser welding10.1063/1.373033 ↗
45. High-speed simultaneous observation of plasma and keyhole behavior during high power CO2 laser welding: effect of shielding gas on porosity formation10.2351/1.1324717 ↗
46. Characterization of entrapped gases in rapidly solidified powders10.1016/0921-5093(90)90328-Z ↗
47. Feedstock powder processing research needs for additive manufacturing development10.1016/j.cossms.2018.01.002 ↗
48. Review of the methods for production of spherical Ti and Ti alloy powder10.1007/s11837-017-2513-5 ↗
49. A comparative study of Ti-6Al-4V powders for additive manufacturing by gas atomization, plasma rotating electrode process and plasma atomization10.1016/j.powtec.2018.04.013 ↗
50. Microstructural characterization and properties of Ti-28Ta at.% powders produced by plasma rotating electrode process10.1016/j.jallcom.2017.04.195 ↗
51. Laser powder-bed fusion additive manufacturing: physics of complex melt flow and formation mechanisms of pores, spatter, and denudation zones Saad10.1016/j.actamat.2016.02.014 ↗
52. Fundamental aspects of hot isostatic pressing: an overview10.1007/s11661-000-0078-2 ↗