Hot isostatic pressing in metal additive manufacturing: X-ray tomography reveals details of pore closure
Source abstract
Abstract
Hot isostatic pressing (HIP) of additively manufactured metals is a widely adopted and effective method to improve the density and microstructure homogeneity within geometrically-complex metal structures fabricated with laser powder bed fusion (LPBF). The role of pores in the fatigue performance of additively manufactured metal parts is increasingly being recognized as a critical factor and HIP post-processing is now heralded as a method to eliminate pores, especially for high-criticality applications such as in the aerospace industry. Despite the widely reported positive influence on fatigue performance and high efficiency of pore closure, examples have been reported in which pores have not been entirely closed or have subsequently re-opened upon heat treatment. A variety of porosity distributions and types of pores may be present in parts produced by LBPF and the effectiveness of pore closure may differ depending on these pore characteristics. In this work, X-ray tomography was employed to provide insights into pore closure efficiency by HIP for an intentional and artificially-induced cavity as well as for a range of typical process-induced pores (lack of fusion, keyhole, contour pores, etc.) in coupon samples of Ti6Al4V. The same samples were imaged non-destructively before and after HIP and aligned carefully for side-by-side viewing. High pore closure efficiency is demonstrated for all types of cavities and pores investigated, but near-surface pores of all types are shown to be problematic to varying degrees, in some cases perforating the superficial surface and creating new external notches. Subsequent heat treatments (annealing after HIP) in some cases resulted in internal pore reopening for previously closed internal pores as well as a new “blistering” effect observed for some near-surface pores, which the authors believe is reported for the first time. Implications of these results for quality control and HIP processing of LPBF parts are discussed. Finally, the utility of using HIP to consolidate intentionally-unmelted powder in order to improve production rates of powder bed fusion has great potential and is preliminarily demonstrated.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
2. Laser additive manufacturing of metallic components: materials, processes and mechanisms10.1179/1743280411Y.0000000014 ↗
3. Wohlers · 2018
4. Beautiful and functional: a. review of biomimetic design in additive manufacturing
5. Topology optimization for additive manufacturing as an enabler for light weight flight hardware10.3390/designs2040051 ↗
6. Designing for additive manufacturing: lightweighting through topology optimization enables lunar spacecraft10.1115/1.4037304 ↗
7. Additive manufacturing of titanium alloy for aircraft components10.1016/j.procir.2015.08.061 ↗
8. Scientific, technological and economic issues in metal printing and their solutions
9. Challenges in additive manufacturing of space parts: powder feedstock cross-contamination and its impact on end products10.3390/ma10050522 ↗
10. Additive manufacturing of fatigue resistant materials: challenges and opportunities10.1016/j.ijfatigue.2017.01.001 ↗
11. Overview of materials qualification needs for metal additive manufacturing10.1007/s11837-015-1810-0 ↗
12. Analysis of defect generation in Ti-6Al-4V parts made using powder bed fusion additive manufacturing processes
13. X-ray microcomputed tomography in additive manufacturing: a review of the current technology and applications
14. Standardized X-ray tomography testing of additively manufactured parts: a round robin test
15. Effects of defects on mechanical properties in metal additive manufacturing: a review focusing on X-ray tomography insights10.1016/j.matdes.2019.108385 ↗
16. Metal additive manufacturing: a review of mechanical properties10.1146/annurev-matsci-070115-032024 ↗
17. Fundamental aspects of hot isostatic pressing: an overview10.1007/s11661-000-0078-2 ↗
18. Investigation of porosity changes in cast Ti6Al4V rods after hot isostatic pressing10.1007/s11665-015-1580-4 ↗
19. A novel near α-Ti alloy prepared by hot isostatic pressing: microstructure evolution mechanism and high temperature tensile properties10.1016/j.matdes.2016.05.092 ↗
20. Effect of hot isostatic pressing procedure on performance of Ti6Al4V: surface qualities, microstructure and mechanical properties10.1016/j.jallcom.2016.05.280 ↗
21. A novel hybrid selective laser melting/hot isostatic pressing of near-net shaped Ti-6Al-4V alloy using an in-situ tooling: interfacial microstructure evolution and enhanced mechanical properties10.1016/j.msea.2018.01.079 ↗
22. Influence of defects, surface roughness and HIP on the fatigue strength of Ti-6Al-4V manufactured by additive manufacturing10.1016/j.ijfatigue.2018.07.020 ↗
23. Progress towards metal additive manufacturing standardization to support qualification and certification10.1007/s11837-017-2265-2 ↗
24. Standard specification for additive manufacturing Titanium-6 Aluminum-4 vanadium with powder bed fusion
25. HIP for AM - optimized material properties by HIP10.21741/9781644900031-1 ↗
26. Effects of HIP on microstructural heterogeneity, defect distribution and mechanical properties of additively manufactured EBM Ti-48Al-2Cr-2Nb10.1016/j.jallcom.2017.09.163 ↗
27. Application of microCT to the non-destructive testing of an additive manufactured titanium component, Case Stud
28. The effectiveness of hot isostatic pressing for closing porosity in titanium parts manufactured by selective electron beam melting10.1007/s11661-016-3429-3 ↗
29. Hot isostatic pressing of IN718 components manufactured by selective laser melting
30. Analyzing the effects of powder and post-processing on porosity and properties of electron beam melted Ti-6Al-4V10.1080/21663831.2017.1340911 ↗
31. Porosity regrowth during heat treatment of hot isostatically pressed additively manufactured titanium components10.1016/j.scriptamat.2016.05.002 ↗
32. Solubility of argon in laser additive manufactured α-titanium under hot isostatic pressing condition10.1016/j.commatsci.2017.01.040 ↗
33. Effects of process parameters on porosity in laser powder bed fusion revealed by X-ray tomography
34. The CT scanner facility at Stellenbosch University: an open access X-ray computed tomography laboratory10.1016/j.nimb.2016.08.005 ↗
35. MethodsX Standard method for microCT-based additive manufacturing quality control 1 : porosity analysis10.1016/j.mex.2018.09.005 ↗
36. Pore closure effect of laser shock peening of additively manufactured AlSi10Mg