journal article·2021-02

A novel crack-free Ti-modified Al-Cu-Mg alloy designed for selective laser melting

Jinliang Zhang, Jianbao Gao, Bo Song, Lijun Zhang, Changjun Han, Chao Cai, Kun Zhou, Yusheng Shi

Publisher page

Abstract

Abstract A novel crack-free Ti-modified Al-Cu-Mg alloy for SLM was developed here, based on the thermodynamic calculations of the crack susceptibility index and growth-restriction factor. We found that the introduction of Ti into the Al-Cu-Mg alloy effectively promoted the grain refinement and columnar-to-equiaxed grain transition as a result of the heterogeneous nucleation provided by Al3Ti precipitates. The hot tearing cracks were eliminated after Ti modification due to the formation of the homogeneous and fine equiaxed microstructure. We created a new high-strength Al-Cu-Mg-Ti alloy with a tensile strength of 426.4 MPa, yield strength of 293.2 MPa and ductility of 9.1%. This novel Ti-modified Al alloy with fine equiaxed grains and highly-enhanced mechanical properties offers a new compositional space for the printable lightweight material categories specifically for the SLM technique.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Recent advances on high-entropy alloys for 3D printing10.1002/adma.201903855 ↗
2. A review of selective laser melting of aluminum alloys: processing, microstructure, property and developing trends10.1016/j.jmst.2018.09.004 ↗
3. An investigation into the effect of gradients on the manufacturing fidelity of triply periodic minimal surface structures with graded density fabricated by selective laser melting10.1016/j.jmatprotec.2019.116367 ↗
4. Recent development in aluminium alloys for aerospace applications10.1016/S0921-5093(99)00674-7 ↗
5. Progress in structural materials for aerospace systems10.1016/j.actamat.2003.08.023 ↗
6. Review of selective laser melting: Materials and applications10.1063/1.4935926 ↗
7. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: processing, microstructure and properties10.1016/j.pmatsci.2015.03.002 ↗
8. Comparative study of performance comparison of AlSi10Mg alloy prepared by selective laser melting and casting10.1016/j.jmst.2019.08.049 ↗
9. Simultaneous enhancements of strength and toughness in an Al-12Si alloy synthesized using selective laser melting10.1016/j.actamat.2016.06.009 ↗
10. Application of modern aluminium alloys to aircraft10.1016/0376-0421(95)00004-6 ↗
11. Numerical investigation and an effective modelling on the Selective Laser Melting (SLM) process with aluminium alloy 606110.1016/j.ijheatmasstransfer.2014.09.014 ↗
12. A novel processing approach for additive manufacturing of commercial aluminium alloys10.1016/j.phpro.2016.08.095 ↗
13. Changing the alloy composition of Al7075 for better processability by selective laser melting10.1016/j.jmatprotec.2016.08.003 ↗
14. Selective laser melting of Al-Zn-Mg-Cu: heat treatment, microstructure and mechanical properties10.1016/j.jallcom.2016.11.210 ↗
15. Selective laser melting of high strength Al-Cu-Mg alloys: processing, microstructure and mechanical properties10.1016/j.msea.2015.12.101 ↗
16. Laser and electron-beam powder-bed additive manufacturing of metallic implants: a review on processes, materials and designs10.1002/jor.23075 ↗
17. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
18. Effect of Zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al-Cu-Mg alloy10.1016/j.scriptamat.2017.02.036 ↗
19. Effect of Zr content on formability, microstructure and mechanical properties of selective laser melted Zr modified Al-4.24Cu-1.97Mg-0.56Mn alloys10.1016/j.jallcom.2018.06.032 ↗
20. Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting10.1016/j.actamat.2018.04.053 ↗
21. Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: crack-inhibiting and multiple strengthening mechanisms10.1016/j.actamat.2020.03.060 ↗
22. Selective laser melting of a high strength Al-Mn-Sc alloy: alloy design and strengthening mechanisms10.1016/j.actamat.2019.04.014 ↗
23. Recent developments in advanced aircraft aluminium alloys10.1016/j.matdes.2013.12.002 ↗
24. Susceptibility of ternary aluminum alloys to cracking during solidification10.1016/j.actamat.2016.12.028 ↗
25. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗
26. A simple test for assessing solidification cracking susceptibility and checking validity of susceptibility prediction10.1016/j.actamat.2017.09.065 ↗
27. A simple index for predicting the susceptibility to solidification cracking in welding
28. Gulliver · 1922
29. Thermo-Calc & DICTRA, computational tools for materials science10.1016/S0364-5916(02)00037-8 ↗
30. Ansara · 1998
31. Nucleation ahead of the advancing interface in directional solidification10.1016/S0921-5093(97)80081-0 ↗
32. Relation between grain size and coherency parameters in aluminium alloys10.1179/mst.1995.11.11.1099 ↗
33. Modelling of inoculation of metallic melts: application to grain refinement of aluminium by Al–Ti–B10.1016/S1359-6454(00)00094-X ↗
34. A model of grain refinement incorporating alloy constitution and potency of heterogeneous nucleant particles10.1016/S1359-6454(00)00368-2 ↗
35. Thermodynamic modelling of growth-restriction effects in aluminium alloys10.1016/j.actamat.2004.11.024 ↗
36. Grain refining mechanism in the Al/Al–Ti–B system10.1016/j.actamat.2014.10.055 ↗
37. Crystallographic study of grain refinement in aluminum alloys using the edge-to-edge matching model10.1016/j.actamat.2004.11.037 ↗
38. An analytical model for constitutional supercooling-driven grain formation and grain size prediction10.1016/j.actamat.2010.01.052 ↗
39. Effects of solutes on grain refinement of selected wrought aluminium alloys10.1179/mst.1997.13.8.650 ↗
40. Effects of solute content on grain refinement in an isothermal melt10.1016/j.actamat.2011.01.008 ↗
41. The quantitative effect of rapid cooling upon the constitution of binary alloys
42. Grain refinement of aluminum alloys: part I. the nucleant and solute paradigms-a review of the literature10.1007/s11661-999-0098-5 ↗
43. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
44. Formation of multiple intermetallic phases in a hypereutectic Al-Fe binary alloy additively manufactured by laser powder bed fusion10.1016/j.intermet.2020.106892 ↗
45. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
46. Influence of Nb concentration on the structure, stability, and electronic and mechanical properties of D022 Al3Ti by first-principles calculations and experiments10.1016/j.jpcs.2019.01.035 ↗
47. Lattice parameter variation of Al3 (Ti, V, Zr, Hf) in Al-2 at% (Ti, V, Zr, Hf) alloys10.1016/0036-9748(83)90293-4 ↗
48. Insight into the mechanisms of columnar to equiaxed grain transition during metallic additive manufacturing
49. Phase-field simulations and microstructural analysis of epitaxial growth during rapid solidification of additively manufactured AlSi10Mg alloy10.1016/j.matdes.2020.108985 ↗
50. Quantitative texture prediction of epitaxial columnar grains in additive manufacturing using selective laser melting
51. Grain refining mechanism in the Al/Al–Ti–B system10.1016/j.actamat.2014.10.055 ↗
52. Crystallographic study of grain refinement in aluminum alloys using the edge-to-edge matching model10.1016/j.actamat.2004.11.037 ↗
53. Enhanced strength-plasticity combination in an Al–Cu–Mg alloy-atomic scale microstructure regulation and strengthening mechanisms10.1016/j.msea.2020.139447 ↗
54. Crystal growth and its morphology in the mushy zone10.1016/j.actamat.2003.11.033 ↗
55. Initiation and growth mechanisms for weld solidification cracking10.1179/1743280413Y.0000000020 ↗
56. A solution to the hot cracking problem for aluminium alloys manufactured by laser beam melting10.1016/j.actamat.2020.07.015 ↗
57. Exploring dendrite coherency with the discrete element method10.1016/j.actamat.2011.11.042 ↗
58. Formability improvement, cracking behavior and control of Y-modified Ti-43Al-4Nb-1Mo-0.1B alloys produced by selective laser melting10.1016/j.jallcom.2020.157172 ↗
59. Cracking behavior and control of β-solidifying Ti-40Al-9V-0.5Y alloy produced by selective laser melting10.1016/j.jmst.2019.08.026 ↗