Interpass rolling of Ti-6Al-4V wire + arc additively manufactured features for microstructural refinement
Source abstract
Abstract
In-process deformation methods such as rolling can be used to refine the large columnar grains that form when wire + arc additively manufacturing (WAAM) titanium alloys. Due to the laterally restrained geometry, application to thick walls and intersecting features required the development of a new ‘inverted profile’ roller. A larger radii roller increased the extent of the recrystallised area, providing a more uniform grain size, and higher loads increased the amount of refinement. Electron backscatter diffraction showed that the majority of the strain is generated toward the edges of the rolled groove, up to 3 mm below the rolled surface. These results will help facilitate future optimisation of the rolling process and industrialisation of WAAM for large-scale titanium components.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Cranfield University, www.waammat.com, (2017).
2. Wire + arc additive manufacturing10.1179/1743284715Y.0000000073 ↗
3. Wire-feed additive manufacturing of metal components: technologies, developments and future interests10.1007/s00170-015-7077-3 ↗
4. Martina · 2014
5. System architectures for large scale wire + arc Additive Manufacture
6. Application of bulk deformation methods for microstructural and material property improvement and residual stress and distortion control in additively manufactured components10.1016/j.scriptamat.2016.10.031 ↗
7. Microstructure of interpass rolled wire + arc additive manufacturing Ti-6Al-4V components10.1007/s11661-015-3172-1 ↗
8. The effect of inter-layer cold working and post-deposition heat treatment on porosity in additively manufactured aluminum alloys10.1016/j.jmatprotec.2015.11.006 ↗
9. Microstructure and mechanical properties of wire and arc additive manufactured Ti-6Al-4V10.1007/s11661-012-1444-6 ↗
10. The effectiveness of combining rolling deformation with wire-arc additive manufacture on β-grain refinement and texture modification in Ti-6Al-4V10.1016/j.matchar.2016.02.001 ↗
11. Donoghue · 2016
12. Microstructure and residual stress improvement in wire and arc additively manufactured parts through high-pressure rolling10.1016/j.jmatprotec.2013.04.012 ↗
13. Hybrid direct manufacturing method of metallic parts using deposition and micro continuous rolling10.1108/RPJ-01-2012-0006 ↗
14. Simulation of microstructure evolution during hybrid deposition and micro-rolling process10.1007/s10853-016-9961-0 ↗
15. Improvement in geometrical accuracy and mechanical property for arc-based additive manufacturing using metamorphic rolling mechanism
16. Residual stress characterization and control in the additive manufacture of large scale metal structures
17. Rosales · 2016
18. Variant selection during cooling after beta annealing of Ti-6Al-4V ingot material10.1007/s11661-012-1245-y ↗
19. Validation of neutron texture data on GEM at ISIS using electron backscattered diffraction10.1088/0957-0233/19/3/034002 ↗
20. Development of microstructure and crystallographic texture during stationary shoulder friction stir welding of Ti-6Al-4V10.1007/s11661-011-0606-2 ↗
21. The calculation of a parent grain orientation from inherited variants for approximate (b.c.c. − h.c.p.) orientation relations research papers10.1107/S0021889802005824 ↗
22. Investigating the limits of polycrystal plasticity modeling10.1016/j.ijplas.2003.10.009 ↗
23. The effectiveness of combining rolling deformation with wire-arc additive manufacture on β-grain refinement and texture modification in Ti-6Al-4V10.1016/j.matchar.2016.02.001 ↗
24. Influence of microstructure on mechanical properties of laser metal wire-deposited Ti-6Al-4V10.1016/j.msea.2016.07.038 ↗
25. Investigation of post-weld rolling methods to reduce residual stress and distortion10.1016/j.jmatprotec.2017.04.018 ↗