journal article·2020-12

Microstructure and mechanical properties of (TiB+TiC)/Ti composites fabricated in situ via selective laser melting of Ti and B4C powders

Changjun Han, Rita Babicheva, Jasper Dong Qiu Chua, Upadrasta Ramamurty, Shu Beng Tor, Chen-Nan Sun, Kun Zhou

Publisher page

Abstract

Abstract Titanium matrix composites reinforced with titanium boride (TiB) and titanium carbide (TiC) were fabricated in situ via selective laser melting (SLM). Varying contents of boron carbide (B4C) from 0 to 5 wt% were added to pure Ti to prepare blended powders for SLM. The influence of the B4C content on the printability, microstructure and mechanical properties of SLM-printed (TiB + TiC)/Ti composites was studied. The relative densities of all the fabricated composites were greater than 97.8 %; an increase in the B4C content resulted in a decrease in their relative density. The microstructure of the composites varied from a lath-shaped structure (0 wt%) to a dendritic structure (1 wt%) and to a cellular + dendritic structure (2–5 wt%), which was determined by the change of thermal convection within melt pools. Both the dendritic and cellular structures were arranged by coalescent clusters composed of TiB whiskers and TiC particles, while the clusters were formed through a self-joining behavior of the TiB whiskers that were mechanically locked with the TiC particles. The composites with the addition of 1 wt% B4C exhibited the highest ultimate tensile strength of 946 MPa, yield strength of 762 MPa and elastic modulus of 128 GPa, which were 62.4 %, 49.2 % and 15.3 % higher than those of the Ti matrix, respectively. The remarkable enhancement in the mechanical strengths was attributed to the synergistic effect of dispersion strengthening and grain refinement strengthening. The (TiB + TiC)/Ti composites fabricated in situ by SLM with an optimized material formulation not only ensured comparable mechanical properties to those of their counterparts manufactured by conventional processes but also demonstrated the potential in manufacturing complex and/or customized parts with design freedom for industrial applications.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. Particle-reinforced metal matrix nanocomposites fabricated by selective laser melting: a state of the art review10.1016/j.pmatsci.2019.04.006 ↗
2. Recent developments and opportunities in additive manufacturing of titanium-based matrix composites: a review10.1016/j.ijmachtools.2018.06.003 ↗
3. Processing-structure-property aspects of particulate-and whisker-reinforced titanium matrix composites10.1016/j.compscitech.2007.07.016 ↗
4. Titanium metal matrix composites by powder metallurgy (PM) routes
5. Interfacial reaction in cast WC particulate reinforced titanium metal matrix composites coating produced by laser processing10.1016/j.optlastec.2015.01.003 ↗
6. In-situ preparation and formation of TiB/Ti-6Al-4V nanocomposite via laser additive manufacturing: microstructure evolution and tribological behavior10.1016/j.powtec.2018.09.088 ↗
7. Reactive-deposition-based additive manufacturing of Ti-Zr-BN composites
8. Effect of low-melting-point sintering aid on densification mechanisms of boron carbide during spark plasma sintering10.1016/j.scriptamat.2018.12.036 ↗
9. Densification and properties of B4C-based ceramics with CrMnFeCoNi high entropy alloy as a sintering aid by spark plasma sintering10.1016/j.powtec.2018.11.005 ↗
10. Effect of B4C particle size on microstructure of in situ titanium matrix composites prepared by reactive processing of Ti–B4C system10.1016/j.scriptamat.2006.05.024 ↗
11. Study of structure formation in TiC–TiB2–MexOy ceramics fabricated by SHS and densification10.1016/j.actamat.2007.11.022 ↗
12. Boron modified titanium alloys10.1016/j.pmatsci.2020.100653 ↗
13. Strengthening behavior of in situ-synthesized (TiC–TiB)/Ti composites by powder metallurgy and hot extrusion10.1016/j.matdes.2016.01.092 ↗
14. Fabrication and tensile properties of in situ TiBw and TiCp hybrid-reinforced titanium matrix composites based on Ti–B4C–C10.1016/j.msea.2007.06.004 ↗
15. Microstructural and mechanical characteristics of in situ metal matrix composites10.1016/S0927-796X(00)00024-3 ↗
16. TEM characterization of symbiosis structure of in situ TiC and TiB prepared by reactive processing of Ti–B4C10.1016/j.matlet.2007.06.033 ↗
17. Effect of volume fraction of reinforcement on room temperature tensile property of in situ (TiB+TiC)/Ti matrix composites10.1016/j.matdes.2004.11.030 ↗
18. Microstructure and mechanical properties of P/M titanium matrix composites reinforced by in-situ synthesized TiC–TiB10.1016/j.msea.2015.01.033 ↗
19. Recent advances on high‐entropy alloys for 3D printing10.1002/adma.201903855 ↗
20. Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: crack-inhibiting and multiple strengthening mechanisms10.1016/j.actamat.2020.03.060 ↗
21. Micro-and meso-structures and their influence on mechanical properties of selectively laser melted Ti-6Al-4V10.1016/j.actamat.2018.05.044 ↗
22. In situ synthesized TiB–TiN reinforced Ti6Al4V alloy composite coatings: microstructure, tribological and in-vitro biocompatibility10.1016/j.jmbbm.2013.09.006 ↗
23. Selective laser melting process optimization of Ti–Mo–TiC metal matrix composites10.1016/j.cirp.2019.04.120 ↗
24. Microstructure and properties of intermetallic composite coatings fabricated by selective laser melting of Ti–SiC powder mixtures10.1016/j.intermet.2013.11.012 ↗
25. Microstructure and property evolutions of titanium/nano-hydroxyapatite composites in-situ prepared by selective laser melting10.1016/j.jmbbm.2017.02.021 ↗
26. Titanium/hydroxyapatite (Ti/HA) gradient materials with quasi-continuous ratios fabricated by SLM: material interface and fracture toughness10.1016/j.matdes.2017.12.037 ↗
27. Selective laser melting of in situ titanium–titanium boride composites: processing, microstructure and mechanical properties10.1016/j.actamat.2014.05.022 ↗
28. Effect of powder particle shape on the properties of in situ Ti–TiB composite materials produced by selective laser melting10.1016/j.jmst.2015.08.007 ↗
29. Laser deposition-additive manufacturing of TiB-Ti composites with novel three-dimensional quasi-continuous network microstructure: effects on strengthening and toughening10.1016/j.compositesb.2017.09.019 ↗
30. Laser deposition-additive manufacturing of in situ TiB reinforced titanium matrix composites: TiB growth and part performance10.1007/s00170-017-0769-0 ↗
31. Graded layered titanium composite structures with TiB2 inclusions fabricated by selective laser melting10.1016/j.compstruct.2016.11.013 ↗
32. Additive layer manufacturing of titanium matrix composites using the direct metal deposition laser process10.1016/j.msea.2016.09.002 ↗
33. Characterization of (TiB+TiC)/TC4 in situ titanium matrix composites prepared by laser direct deposition10.1016/j.jmatprotec.2010.11.009 ↗
34. Microstructure growth behavior and its evolution mechanism during laser additive manufacture of in-situ reinforced (TiB+TiC)/Ti composite10.1016/j.jallcom.2017.09.033 ↗
35. Selective laser melting of hybrid ex-situ/in-situ reinforced titanium matrix composites: Laser/powder interaction, reinforcement formation mechanism, and non-equilibrium microstructural evolutions10.1016/j.matdes.2019.108185 ↗
36. Densification behavior, microstructure evolution and fretting wear performance of in-situ hybrid strengthened Ti-based composite by laser powder-bed fusion10.1016/j.vacuum.2018.11.023 ↗
37. Selective laser melting of stainless-steel/nano-hydroxyapatite composites for medical applications: microstructure, element distribution, crack and mechanical properties10.1016/j.jmatprotec.2015.02.010 ↗
38. Synthesis and structural characterization of Al–B4C nano-composite powders by mechanical alloying10.1016/j.jallcom.2008.12.076 ↗
39. A critical assessment and thermodynamic calculation of the boron-carbon-titanium (BC-Ti) ternary system10.1007/BF02646248 ↗
40. In situ reactions during direct laser deposition of Ti-B4C composites10.1016/j.scriptamat.2020.03.021 ↗
41. TiB whisker coating on titanium surfaces by solid-state diffusion: synthesis, microstructure, and mechanical properties10.1007/s11661-002-0336-6 ↗
42. Effect of boron concentration on martensitic transformation temperatures, stress for inducing martensite and slip stress of Ti-24 mol% Nb-3 mol% Al superelastic alloy10.2320/matertrans.48.407 ↗
43. Nanoindentation and wear properties of Ti and Ti-TiB composite materials produced by selective laser melting10.1016/j.msea.2017.01.096 ↗
44. The crystal structure of TiB10.1107/S0365110X5400014X ↗
45. Growth morphologies and mechanism of TiC in the laser surface alloyed coating on the substrate of TiAl intermetallics10.1016/S0925-8388(02)01077-0 ↗
46. Stacking faults formation mechanism of in situ synthesized TiB whiskers10.1016/j.scriptamat.2006.07.006 ↗
47. Mechanical properties and strengthening effects of in situ (TiB+TiC)/Ti-1100 composite at elevated temperatures10.1016/j.msea.2015.12.071 ↗
48. Multivortex convection of metal in molten pool with dispersed impurity induced by laser radiation10.1016/j.ijheatmasstransfer.2013.09.031 ↗
49. High temperature tensile properties of in situ TiBw/Ti6Al4V composites with a novel network reinforcement architecture10.1016/j.msea.2011.12.028 ↗
50. Pore elimination mechanisms during 3D printing of metals
51. In situ X-ray imaging of defect and molten pool dynamics in laser additive manufacturing10.1038/s41467-018-03734-7 ↗
52. Dynamics of pore formation during laser powder bed fusion additive manufacturing10.1038/s41467-019-10009-2 ↗
53. The influences of trace TiB and TiC on microstructure refinement and mechanical properties of in situ synthesized Ti matrix composite10.1016/j.compositesb.2012.01.075 ↗
54. Fundamentals of selective laser melting of alloyed steel powders10.1016/S0007-8506(07)60395-3 ↗
55. Thermal and solutal marangoni convection in In–Ga–Sb system10.1016/S0022-0248(98)01071-9 ↗
56. Nanocrystalline TiC reinforced Ti matrix bulk-form nanocomposites by Selective Laser Melting (SLM): densification, growth mechanism and wear behavior10.1016/j.compscitech.2011.07.010 ↗
57. Microstructure evolution and its effect on mechanical response of the multi-phase reinforced Ti-based composites by laser powder-bed fusion10.1016/j.jallcom.2018.12.182 ↗
58. Clyne · 1995
59. Argon · 2008
60. Fast parallel algorithms for short-range molecular dynamics10.1006/jcph.1995.1039 ↗
61. Modified embedded-atom method interatomic potentials for the Fe–Ti–C and Fe–Ti–N ternary systems10.1016/j.actamat.2009.03.019 ↗
62. Visualization and analysis of atomistic simulation data with OVITO–the open visualization tool
63. Quantum de-trapping and transport of heavy defects in tungsten10.1038/s41563-019-0584-0 ↗
64. On the strength of discontinuous silicon carbide reinforced aluminum composites10.1016/0036-9748(86)90210-3 ↗
65. Assessment of models used to predict the strength of discontinous silicon carbide reinforced aluminum alloys10.1016/0036-9748(87)90105-0 ↗
66. Hall-petch strengthening in nanocrystalline metals10.1016/0921-5093(93)90319-A ↗
67. Stability of strengthening effect of in situ formed TiCp and TiBw on the elevated temperature strength of (TiCp+TiBw)/Ti composites10.1016/j.jallcom.2014.06.094 ↗
68. Microstructure and mechanical properties of in situ synthesised (TiC+TiB)/Ti–6Al–4V composites prepared by powder metallurgy10.1179/174328409X421988 ↗
69. Effect of B4C size on tensile property of (TiB+ TiC) particulate reinforced titanium matrix composites by investment casting10.2320/matertrans.M2011079 ↗
70. Evaluation of the mechanical and wear properties of titanium produced by three different additive manufacturing methods for biomedical application10.1016/j.msea.2019.06.024 ↗
71. Microstructures and mechanical properties of Si and Zr modified Al–Zn–Mg–Cu alloy-A comparison between selective laser melting and spark plasma sintering10.1016/j.jallcom.2019.153520 ↗
72. Ductility of a Ti-6Al-4V alloy produced by selective laser melting of prealloyed powders10.1108/13552541011083371 ↗
73. Effect of molten pool boundaries on the mechanical properties of selective laser melting parts10.1016/j.jmatprotec.2014.06.002 ↗