Columnar to equiaxed transition during direct metal laser sintering of AlSi10Mg alloy: Effect of building direction
Source abstract
Abstract
Abstract In the current study, cylindrical samples of AlSi10Mg alloy were fabricated using direct metal laser sintering (DMLS) technique in vertical and horizontal directions. The microstructure of the samples was analyzed using scanning electron microscopy, electron backscatter diffraction and transmission electron microscopy. It was observed that, by changing the building direction from vertical to horizontal, columnar to equiaxed transition (CET) occurred in the alloy. While 75% of the grains in the vertical sample were columnar, by changing the direction to horizontal, 49% of the grains evolved with columnar shape and 51% of them were equiaxed. Moreover, the texture of DMLS-AlSi10Mg alloy changed due to CET. While {001} fiber texture evolved in the vertical sample, the direction tilted away from the building direction in the horizontal one. Using the fundamentals of solidification and constitutional undercooling, the solidification behavior of AlSi10Mg alloy during DMLS process was modeled. It was observed that, the determinant parameter in CET during DMLS of AlSi10Mg alloy is the angle between the nominal growth rate and h k l > direction of the growing dendrite, which is controlled by the geometry and building direction of the sample. Further TEM studies confirmed that, CET alters the shape and coherency of Si precipitates and dislocation density inside the α-Al dendrites in DMLS-AlSi10Mg alloy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (66)
Show source-provided references
1. Kou · 2003
2. Columnar to equiaxed transition in solidification processing10.1016/S1468-6996(01)00047-X ↗
3. Microstructure analysis of AZ31 magnesium alloy welds using phase-field models10.1016/j.actamat.2012.07.035 ↗
4. Steady state columnar and equiaxed growth of dendrites and eutectic10.1016/0025-5416(84)90201-5 ↗
5. Single-crystal laser deposition of superalloys: processing–microstructure maps10.1016/S1359-6454(00)00367-0 ↗
6. Simulation of the columnar-to-equiaxed transition in directionally solidified Al–Cu alloys10.1016/j.actamat.2004.10.019 ↗
7. Mechanical blocking mechanism for the columnar to equiaxed transition10.1007/s11661-008-9643-x ↗
8. Predicting the columnar-to-equiaxed transition for a distribution of nucleation undercoolings10.1016/j.actamat.2008.10.001 ↗
9. Laser additive manufacturing of metallic components: materials, processes and mechanisms10.1179/1743280411Y.0000000014 ↗
10. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
11. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
12. The metallurgy and processing science of metal additive manufacturing10.1080/09506608.2015.1116649 ↗
13. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
14. Solidification and solid-state transformation sciences in metals additive manufacturing10.1016/j.scriptamat.2017.01.005 ↗
15. Epitaxy and microstructure evolution in metal additive manufacturing10.1146/annurev-matsci-070115-031728 ↗
16. Strong morphological and crystallographic texture and resulting yield strength anisotropy in selective laser melted tantalum10.1016/j.actamat.2013.04.036 ↗
17. Role of anisotropic properties on topology optimization of additive manufactured load bearing structures10.1016/j.scriptamat.2016.10.021 ↗
18. Anisotropy and heterogeneity of microstructure and mechanical properties in metal additive manufacturing: a critical review10.1016/j.matdes.2017.11.021 ↗
19. Site specific control of crystallographic grain orientation through electron beam additive manufacturing10.1179/1743284714Y.0000000734 ↗
20. Crystallographic texture engineering through novel melt strategies via electron beam melting: inconel 71810.1179/1743284714Y.0000000697 ↗
21. Grain structure evolution in Inconel 718 during selective electron beam melting10.1016/j.msea.2016.05.046 ↗
22. Numerical modeling of heat-transfer and the influence of process parameters on tailoring the grain morphology of IN718 in electron beam additive manufacturing10.1016/j.actamat.2016.03.063 ↗
23. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
24. Textures formed in a CoCrMo alloy by selective laser melting10.1016/j.jallcom.2015.01.096 ↗
25. The influence of processing parameters on aluminium alloy A357 manufactured by Selective Laser Melting10.1016/j.matdes.2016.07.009 ↗
26. Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti-6Al-4V by selective electron beam melting10.1016/j.matchar.2013.07.012 ↗
27. Grain morphology evolution behavior of titanium alloy components during laser melting deposition additive manufacturing10.1016/j.jallcom.2015.01.256 ↗
28. Grain morphology control and texture characterization of laser solidformed Ti6Al2Sn2Zr3Mo1.5Cr2Nb titanium alloy10.1016/j.jmatprotec.2016.07.011 ↗
29. Controlling the microstructure and properties of wire arc additive manufactured Ti–6Al–4V with trace boron additions10.1016/j.actamat.2015.03.035 ↗
30. Selective laser melting of titanium alloy with 50 wt% tantalum: microstructure and mechanical properties10.1016/j.jallcom.2015.11.141 ↗
31. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
32. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
33. Microstructural features of Sc- and Zr-modified Al-Mg alloys processed by selective laser melting10.1016/j.matdes.2016.11.040 ↗
34. Columnar to equiaxed transition in Al-Mg(-Sc)-Zr alloys produced by selective laser melting10.1016/j.scriptamat.2017.10.021 ↗
35. The anisotropy of laser melting deposition additive manufacturing Ti–6.5Al–3.5Mo–1.5Zr–0.3Si titanium alloy10.1016/j.matdes.2014.11.001 ↗
36. Phase field simulation of powder bed-based additive manufacturing10.1016/j.actamat.2017.11.033 ↗
37. Gibson · 2010
38. Effects of build direction and heat treatment on creep properties of Ni-base superalloy built up by additive manufacturing10.1016/j.scriptamat.2016.10.035 ↗
39. Selective laser melting of AlSi10Mg alloy: process optimisation and mechanical properties development10.1016/j.matdes.2014.09.044 ↗
40. Effect of heat treatment on AlSi10Mg alloy fabricated by selective laser melting: microstructure evolution, mechanical properties and fracture mechanism10.1016/j.msea.2016.03.088 ↗
41. Effect of strut orientation on the microstructure heterogeneities in AlSi10Mg lattices processed by selective laser melting10.1016/j.scriptamat.2017.07.020 ↗
42. On dynamic mechanical behavior of additively manufactured AlSi10Mg_200C10.1016/j.matlet.2017.10.001 ↗
43. Achieving low surface roughness AlSi10Mg 200C parts using direct metal laser sintering
44. On microstructure and mechanical properties of additively manufactured AlSi10Mg_200C using recycled powder10.1016/j.msea.2017.09.041 ↗
45. Change in microstructure of selectively laser melted AlSi10Mg alloy with heat treatments10.1016/j.msea.2017.08.029 ↗
46. Strength and strain hardening of a selective laser melted AlSi10Mg alloy10.1016/j.scriptamat.2017.07.025 ↗
47. Microstructure and mechanical properties of Inconel 718 produced by selective laser melting: sample orientation dependence and effects of post heat treatments10.1016/j.msea.2017.12.043 ↗
48. Deformation mechanism during dynamic loading of an additively manufactured AlSi10Mg_200C10.1016/j.msea.2018.03.014 ↗
49. Microstructure and strength of selectively laser melted AlSi10Mg10.1016/j.actamat.2016.07.012 ↗
50. SLM-processed Sc- and Zr- modified Al-Mg alloy: mechanical properties and microstructural effects of heat treatment10.1016/j.msea.2017.06.089 ↗
51. Metallurgy of high-silicon steel parts produced using Selective Laser Melting10.1016/j.actamat.2016.03.037 ↗
52. Size dependence of microstructure of AlSi10Mg alloy fabricated by selective laser melting
53. Quantitative texture prediction of epitaxial columnar grains in additive manufacturing using selective laser melting
54. Gradient in microstructure and mechanical property of selective laser melted AlSi10Mg10.1016/j.jallcom.2017.11.020 ↗
55. Epitaxial laser metal forming: analysis of microstructure formation10.1016/S0921-5093(99)00202-6 ↗
56. Glicksman · 2011
57. A quantitative study of solute diffusion field effects on heterogeneous nucleation and the grain size of alloys10.1016/j.actamat.2010.12.014 ↗
58. Nanoparticle-inhibited growth of primary aluminum in Al–10Si alloys10.1016/j.actamat.2015.10.005 ↗
59. Flemings · 1974
60. Dendritic growth into undercooled alloy melts10.1016/0025-5416(84)90199-X ↗
61. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
62. FactSage™, Ver. 6.2. Thermfact (Montreal, Canada) and GTT-Technologies, Aachen, Germany, 1976-2010.
63. Parametric analysis of thermal behavior during selective laser melting additive manufacturing of aluminum alloy powder10.1016/j.matdes.2014.07.006 ↗
64. The evolution of dislocation density during heat treatment and creep of tempered martensite ferritic steels10.1016/S1359-6454(03)00324-0 ↗
65. Effect of processing parameters on the evolution of dislocation density and sub-grain size of a 12%Cr heat resistant steel during creep at 650°C10.1016/j.msea.2010.10.028 ↗
66. EELS log-ratio technique for specimen-thickness measurement in the TEM10.1002/jemt.1060080206 ↗