journal article·2021-05

Additive manufacturing and mechanical properties of the dense and crack free Zr-modified aluminum alloy 6061 fabricated by the laser-powder bed fusion

Abhishek Mehta, Le Zhou, Thinh Huynh, Sharon Park, Holden Hyer, Shutao Song, Yuanli Bai, D. Devin Imholte, Nicolas E. Woolstenhulme, Daniel M. Wachs, Yongho Sohn

Publisher page

Abstract

Abstract For additive manufacturing such as laser powder bed fusion (LPBF), commercial aluminum alloy (AA) 6061 is typically considered unsuitable due to formation of solidification cracking and/or excessive porosity. In this study, to improve buildability/printability of AA6061, 1 wt% of Zr was alloyed to produce Zr-modified AA6061 by LPBF. Powders of unmodified and Zr-modified AA6061 were produced by gas atomization, and utilized as a feed-stock for the LPBF to fabricate specimens for microstructural examination and mechanical testing. The as-built unmodified AA6061 exhibited poor printability due to formation of cracks and porosity in the microstructure regardless of LPBF parameters. However, the Zr-modified AA6061 exhibited near full density, with substantial reduction in porosities without any solidification crack for a certain LPBF processing window. The improved printability of Zr-modified AA6061 was attributed to a significant grain refinement, which would reduce the solidification cracking susceptibility by hampering the epitaxial growth of long columnar cracks, as observed in unmodified AA6061. Yield strength, tensile strength and strain-at-failure for the as-built Zr-modified AA6061 were determined to be 210 MPa, 268 MPa, and 26.5%, respectively. These are superior to the tensile properties of AA6061 in O-annealed condition or in as-cast condition. After T6 heat treatment, yield strength, tensile strength and strain-at-failure of Zr-modified AA6061 were determined to be 300 MPa, 327 MPa, and 14%, which were again superior to the tensile properties of wrought AA6061 in T6 heat treated condition. Effects of Zr addition on the buildability/printability improvement and mechanical properties of AA6061 were corroborated by a variety of electron microscopic characterization.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (67)

Show source-provided references
1. Effect of welding processes on tensile properties of AA6061 aluminium alloy joints10.1007/s00170-007-1325-0 ↗
2. Phase transformations and microstructural development in the U-10 wt Pct Mo alloy with varying Zr Contents after heat treatments relevant to the monolithic fuel plate fabrication process10.1007/s11661-018-4987-3 ↗
3. Microstructural characterization of AA6061 versus AA6061 HIP bonded cladding–cladding interface10.1007/s11669-018-0629-0 ↗
4. Microstructural characteristics of plasma sprayed, electroplated, and co-rolled Zr diffusion barriers in hot isostatic pressed low enriched U-10 wt% Mo monolithic fuel plates10.1016/j.jnucmat.2019.05.056 ↗
5. Interdiffusion, reactions, and phase transformations observed during fabrication of low enriched uranium monolithic fuel system for research and test reactors10.4028/www.scientific.net/DDF.383.10 ↗
6. Relating diffusion couple experiment results to observed as-fabricated microstructures in low-enriched U-10wt% Mo monolithic fuel plates10.4028/www.scientific.net/DDF.375.18 ↗
7. Interdiffusion and reaction between Al and Zr in the temperature range of 425 to 475 °C10.1007/s11669-019-00729-9 ↗
8. Anomalous growth of Al8Mo3 phase during interdiffusion and reaction between Al and Mo10.1016/j.jnucmat.2020.152337 ↗
9. Interdiffusion and reaction between U and Zr10.1016/j.jnucmat.2018.01.063 ↗
10. A simple index for predicting the susceptibility to solidification cracking
11. 3D printing of aluminium alloys: additive manufacturing of aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
12. Selective laser melting of aluminium components10.1016/j.jmatprotec.2010.09.019 ↗
13. Microstructure, precipitates and hardness of selectively laser melted AlSi10Mg alloy before and after heat treatment10.1016/j.matchar.2018.04.022 ↗
14. Use of power factor and specific point energy as design parameters in laser powder-bed-fusion (L-PBF) of AlSi10Mg alloy10.1016/j.matdes.2019.108018 ↗
15. Defining the tensile properties of Al-12Si parts produced by selective laser melting10.1016/j.actamat.2016.12.044 ↗
16. A selective laser melting and solution heat treatment refined Al–12Si alloy with a controllable ultrafine eutectic microstructure and 25% tensile ductility10.1016/j.actamat.2015.05.017 ↗
17. Effects of alloy composition and solid-state diffusion kinetics on powder bed fusion cracking susceptibility
18. Pulsed laser powder bed fusion additive manufacturing of A35610.1016/j.matchar.2018.02.004 ↗
19. Laser powder bed fusion of Al–10 wt% Ce alloys: microstructure and tensile property10.1007/s10853-020-05037-z ↗
20. Microstructure and mechanical properties of Zr-modified aluminum alloy 5083 manufactured by laser powder bed fusion
21. B.A. Fulcher, D.K. Leigh, T.J. Watt, Comparison of AlSi10Mg and Al 6061 processed through DMLS, in: Proceedings of the Solid Freeform Fabrication (SFF) Symposium, Austin, TX, USA, (2014).
22. Influence of process parameters on the quality of aluminium alloy EN AW 7075 using Selective Laser Melting (SLM)10.1016/j.phpro.2016.08.096 ↗
23. Fabrication and characterization of high strength Al-Cu alloys processed using laser beam melting in metal powder bed10.1016/j.phpro.2014.08.156 ↗
24. Cracking mechanism and its sensitivity to processing conditions during laser powder bed fusion of a structural aluminum alloy10.1016/j.mtla.2020.100976 ↗
25. Selective Laser Melting of aluminium alloy using a uniform beam profile10.1080/17452759.2013.869608 ↗
26. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
27. A solution to the hot cracking problem for aluminium alloys manufactured by laser beam melting10.1016/j.actamat.2020.07.015 ↗
28. The crack healing effect of scandium in aluminum alloys during laser additive manufacturing10.1016/j.jmapro.2019.12.050 ↗
29. Processing and characterization of crack-free aluminum 6061 using high-temperature heating in laser powder bed fusion additive manufacturing
30. The effect of selective laser melting process parameters on the microstructure and mechanical properties of Al6061 and AlSi10Mg alloys10.3390/ma12010012 ↗
31. S.Z. Uddin, D. Espalin, J. Mireles, P. Morton, C. Terrazas, S. Collins, L.E. Murr, R. Wicker, Laser powder bed fusion fabrication and characterization of crack-free aluminum alloy 6061 using in-process powder bed induction heating, in: Proceedings of the SFF symposium, (2017) 214–227.
32. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
33. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
34. Microstructure, precipitates and mechanical properties of powder bed fused inconel 718 before and after heat treatment10.1016/j.jmst.2018.12.006 ↗
35. Selective laser melting of Al7050 powder: melting mode transition and comparison of the characteristics between the keyhole and conduction mode10.1016/j.matdes.2017.09.014 ↗
36. Vapour pressure equations for the metallic elements: 298–2500 K10.1179/cmq.1984.23.3.309 ↗
37. Additive manufacturing of dense WE43 Mg alloy by laser powder bed fusion
38. Observation of keyhole-mode laser melting in laser powder-bed fusion additive manufacturing10.1016/j.jmatprotec.2014.06.005 ↗
39. Effect of energy density and scanning strategy on densification, microstructure and mechanical properties of 316L stainless steel processed via selective laser melting10.1016/j.msea.2019.138455 ↗
40. On the weldability, composition, and hardness of pulsed and continuous Nd:YAG laser welds in aluminum alloys 6061, 5456, and 508610.1007/BF02654217 ↗
41. Equilibrium pseudobinary Al–Mg2Si phase diagram10.1179/026708301101510311 ↗
42. Nucleation and precipitation strengthening in dilute Al-Ti and Al-Zr alloys10.1007/s11661-007-9283-6 ↗
43. Investigation of performance and residual stress generation of AlSi10Mg processed by selective laser melting
44. Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
45. Effects of grain size on tensile property and fracture morphology of 316L stainless steel10.1016/j.matlet.2019.07.058 ↗
46. Composition-dependent solidification cracking of aluminum-silicon alloys during laser powder bed fusion10.1016/j.actamat.2021.116698 ↗
47. Novikov · 1966
48. Flemings · 1974
49. Kurz · 1989
50. Dilatant shear bands in solidifying metals10.1038/nature05426 ↗
51. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗
52. Crack susceptibility of binary aluminum alloys during solidification10.1016/j.actamat.2016.03.030 ↗
53. Effect of diffusion on susceptibility to cracking during solidification10.1016/j.actamat.2015.08.064 ↗
54. The Gulliver–Scheil method for the calculation of solidification paths
55. Effect of Zr content on formability, microstructure and mechanical properties of selective laser melted Zr modified Al-4.24 Cu-1.97 Mg-0.56 Mn alloys10.1016/j.jallcom.2018.06.032 ↗
56. The role of wettability in metal–ceramic joining10.1016/j.scriptamat.2010.03.007 ↗
57. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
58. Al-Zr (aluminum-zirconium)10.1361/105497102770331497 ↗
59. Synthesis of precipitation-strengthened Al-Sc, Al-Zr and Al-Sc-Zr alloys via selective laser melting of elemental powder blends
60. Effect of laser rescanning on the grain microstructure of a selective laser melted Al-Mg-Zr alloy10.1016/j.matchar.2018.03.033 ↗
61. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
62. Strengthening mechanisms in a high-strength bulk nanostructured Cu–Zn–Al alloy processed via cryomilling and spark plasma sintering10.1016/j.actamat.2012.09.036 ↗
63. Modelling of the age hardening behaviour of Al–Mg–Si alloys10.1016/S1359-6454(00)00301-3 ↗
64. Precipitation evolution in Al–0.1Sc, Al–0.1Zr and Al–0.1Sc–0.1Zr (at%) alloys during isochronal aging10.1016/j.actamat.2010.05.054 ↗
65. Effects of Zr on the microstructure and mechanical properties of 6061 alloys10.4028/www.scientific.net/MSF.917.202 ↗
66. Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: crack-inhibiting and multiple strengthening mechanisms10.1016/j.actamat.2020.03.060 ↗
67. Comparison of dislocation densities of primary and secondary recrystallization grains of Si-Fe10.1016/0001-6160(57)90122-0 ↗