Tailoring residual stress profile of Selective Laser Melted parts by Laser Shock Peening

Nikola Kalentics, Eric Boillat, Patrice Peyre, Snežana Ćirić-Kostić, Nebojša Bogojević, Roland E. Logé

Abstract

The paper describes a new approach in controlling and tailoring residual stress profile of parts made by Selective Laser Melting (SLM). SLM parts are well known for the high tensile stresses in the as – built state in the surface or subsurface region. These stresses have a detrimental effect on the mechanical properties and especially on the fatigue life. Laser Shock Peening (LSP) as a surface treatment method was applied on SLM parts and residual stress measurements with the hole – drilling method were performed. Two different grades of stainless steel were used: a martensitic 15-5 precipitation hardenable PH1 and an austenitic 316L. Different LSP parameters were used, varying laser energy, shot overlap, laser spot size and treatments with and without an ablative medium. For both materials the as-built (AB) residual stress state was changed to a more beneficial compressive state. The value and the depth of the compressive stress was analyzed and showed a clear dependence on the LSP processing parameters. Application of LSP on SLM parts showed promising results, and a novel method that would combine these two processes is proposed. The use of LSP during the building phase of SLM as a “3D LSP” method would possibly give the advantage of further increasing the depth and volume of compressive residual stresses, and selectively treating key areas of the part, thereby further increasing fatigue life.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Surface Treatment and Residual Stress · Laser Material Processing Techniques · Erosion and Abrasive Machining

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Rapid manufacturing and rapid tooling with layer manufacturing (LM) technologies, state of the art and future perspectives
2. Wohlers Report 2012. [Online]. Available: http://www.wohlersassociates.com/2012report.htm. (Accessed: 11 September 2015).
3. Microstructure and mechanical properties of maraging steel 300 after Selective Laser Melting
4. Investigation on the inclusions in maraging steel produced by Selective Laser Melting
5. Highly Anisotropic Steel Processed by Selective Laser Melting10.1007/s11663-013-9875-z ↗
6. Mechanical properties of AlSi10Mg produced by selective laser melting10.1016/j.phpro.2012.10.059 ↗
7. Fatigue analysis in selective laser melting: review and investigation of thin-walled actuator housings
8. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
9. Graded microstructure and mechanical properties of additive manufactured Ti–6Al–4V via electron beam melting10.1016/j.actamat.2015.06.036 ↗
10. Microstructure and mechanical properties of direct metal laser sintered TI-6AL-4V
11. Microstructure and mechanical properties of a novel β titanium metallic composite by selective laser melting10.1016/j.actamat.2014.01.018 ↗
12. Microstructure and mechanical behavior of porous Ti?6Al?4 V parts obtained by selective laser melting10.1016/j.jmbbm.2013.05.011 ↗
13. Microstructure and mechanical behavior of 17-4 precipitation hardenable steel processed by selective laser melting10.1007/s11665-014-1226-y ↗
14. Part and material properties in selective laser melting of metals
15. Assessing and comparing influencing factors of residual stresses in selective laser melting using a novel analysis method10.1177/0954405412437085 ↗
16. Experimental analysis of residual stresses in the selective laser melting process
17. Texture, anisotropy in microstructure and mechanical properties of IN738LC alloy processed by selective laser melting (SLM)10.1016/j.msea.2014.10.003 ↗
18. Selective laser melting of crack-free high density M2 high speed steel parts by baseplate preheating10.1115/1.4028513 ↗
19. Strong morphological and crystallographic texture and resulting yield strength anisotropy in Selective Laser Melted tantalum10.1016/j.actamat.2013.04.036 ↗
20. High temperature material properties of IN738LC processed by selective laser melting (SLM) technology10.1108/13552541311323281 ↗
21. Further Understanding of TAl4V Selective Laser Melting Using Texture Analysis
22. Investigation on reducing distortion by preheating during manufacture of aluminum components using selective laser melting10.2351/1.4828755 ↗
23. An experimental investigation into additive manufacturing-Induced residual stresses in 316L stainless steel10.1007/s11661-014-2549-x ↗
24. Residual stress within metallic model made by selective laser melting process10.1016/S0007-8506(07)60677-5 ↗
25. Laser shock processing of aluminium alloys. Application to high cycle fatigue behaviour10.1016/0921-5093(95)10084-9 ↗
26. Laser shock peening effect on the dislocation transitions and grain refinement of Al?Mg?Si alloy10.1016/j.matchar.2014.08.020 ↗
27. Laser shock processing and its effects on microstructure and properties of metal alloys: a review10.1016/S0142-1123(02)00022-1 ↗
28. On the influence of mechanical surface treatments—deep rolling and laser shock peening—on the fatigue behavior of Ti–6Al–V at ambient and elevated temperatures10.1016/S0921-5093(03)00069-8 ↗
29. High temperature fatigue behavior and residual stress stability of laser-shock peened and deep rolled austenitic steel AISI 30410.1016/j.scriptamat.2004.02.012 ↗
30. Improvement of fatigue property in 7050–T7451 aluminum alloy by laser peening and shot peening10.1016/j.msea.2011.01.077 ↗
31. Effect of laser shock peening on residual stress and fatigue life of clad 2024 aluminium sheet containing scribe defects10.1016/j.msea.2012.04.002 ↗
32. Fatigue crack nucleation and growth rate behavior of laser shock peened titanium10.1016/S0142-1123(99)00072-9 ↗
33. Investigation on the surface and near-surface characteristics of Ti–2. 5Cu after various mechanical surface treatments10.1016/j.surfcoat.2011.01.001 ↗
34. Characteristics of surface layers formed on inconel 718 by laser shock peening with and without a protective coating10.1016/j.jmatprotec.2015.06.026 ↗
35. Laser shock peening enhanced corrosion properties in a nickel based Inconel 600 superalloy10.1016/j.jallcom.2016.10.093 ↗
36. The strengthening mechanism of a nickel-based alloy after laser shock processing at high temperatures10.1088/1468-6996/14/5/055010 ↗
37. An evaluation of shot peening, residual stress and stress relaxation on the fatigue life of AISI 4340 steel10.1016/S0142-1123(01)00205-5 ↗
38. Effects of laser induced shock waves on metals
39. Effects of fatigue and fretting on residual stresses introduced by laser shock peening10.1016/j.msea.2006.07.020 ↗
40. A comprehensive investigation on the effects of laser and shot peening on fatigue crack growth in friction stir welded AA 2195 joints10.1016/j.ijfatigue.2008.03.029 ↗
41. Effect of controlled shot peening and laser shock peening on the fatigue performance of 2024-T351 aluminum alloy10.1361/105994903770342944 ↗
42. Laser peening process and its impact on materials properties in comparison with shot peening and ultrasonic impact peening10.3390/ma7127925 ↗
43. EOS. Metal Materials for Additive Manufacturing. [Online]. Available: http://www.eos.info/material-m. (Accessed 12 October 2016).
44. Fatigue performance of additive manufactured metallic partsnull10.1108/13552541311302932 ↗
45. Laser adhesion test for thermal sprayed coatings on textured surface by laser10.2351/1.4944451 ↗
46. Laser-delayed double shock-wave generation in water-confinement regime10.2351/1.4906382 ↗
47. Random-type scanning patterns in laser shock peening without absorbing coating in 2024-T351 Al alloy: a solution to reduce residual stress anisotropy10.1016/j.optlastec.2015.04.027 ↗
48. Use of the hole-drilling method for measuring residual stresses in highly stressed shot-peened surfaces10.1007/BF02327502 ↗
49. Effect of laser shock processing on fatigue crack growth and fracture toughness of 6061-T6 aluminum alloy10.1016/j.msea.2004.07.025 ↗
50. Laser shock peening without absorbent coating (LSPwC) effect on 3D surface topography and mechanical properties of 6082-T651 Al alloy10.1016/j.surfcoat.2012.08.048 ↗
51. Methods of measuring residual stresses in components10.1016/j.matdes.2011.08.022 ↗
52. Relaxation methods for measuring residual stresses: techniques and opportunities10.1007/s11340-010-9386-7 ↗
53. V.M. Measurements, Measurement of residual stresses by the hole drilling strain gage method, Tech Note TN-503-6, 2007.
54. Residual stresses in welded structures10.1016/j.ijpvp.2007.10.004 ↗
55. Residual stress and microstructure in welds of 13%Cr–4%Ni martensitic stainless steel10.1016/j.jmatprotec.2008.05.005 ↗
56. A novel approach to characterising the mechanical properties of supermartensitic 13 Cr stainless steel welds10.1016/S0921-5093(04)00819-6 ↗
57. Laser shock processing with small impacts
58. Laser-shock processing of aluminium-coated 55C1 steel in water-confinement regime, characterization and application to high-cycle fatigue behaviour10.1023/A:1004331205389 ↗