journal article·2021-04Open access

Process-structure-property relations for as-deposited solid-state additively manufactured high-strength aluminum alloy

C.J.T. Mason, R.I. Rodriguez, D.Z. Avery, B.J. Phillips, B.P. Bernarding, M.B. Williams, S.D. Cobbs, J.B. Jordon, P.G. Allison

Abstract

Abstract Solid-state additive manufacturing methods provide innovative solutions to circumvent problems associated with materials susceptible to hot cracking by avoiding liquid solid phase transformations. In this work, the process parameter influence on microstructural evolution and mechanical response of a fully dense aluminum alloy 7050 (AA7050) component manufactured via a rapid, solid-state additive manufacturing process known as Additive Friction Stir Deposition (AFS-D) was quantified for the first time. Three sections (starting dwell, transient, crossover of roads) of the deposition that exhibit differing thermomechanical processing histories were evaluated for the resulting microstructure and mechanical response. The microstructural characterization was performed on the as-deposited AA7050 via Electron Backscatter Diffraction (EBSD), Transmission electron microscopy (TEM), optical microscopy, and Scanning Electron Microscopy (SEM). The microstructural characterization revealed refined constituent particles and grains throughout the as-deposited AA7050 microstructure. Furthermore, quasi-static tensile experiments were conducted in both the build and transverse directions, in order to quantify the orientation influence on tensile properties of the as-deposited AA7050 build. Spatially dependent tensile properties were observed in the material due to heat input variation coarsening of secondary phases towards the initial layers of the AFS-D build. Post-mortem analysis revealed that voids nucleated and coalesced from the overgrowth of the strengthening precipitates present in the material, resulting in fracture.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis · Additive Manufacturing Materials and Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (83)

Show source-provided references
1. Microstructures of the commercial 7075 Al alloy in the T651 and T7 tempers10.1007/BF02662363 ↗
2. Calorimetric studies of 7000 series aluminum alloys: II. Comparison of 7075, 7050 and RX720 alloys10.1007/BF02667404 ↗
3. Influence of microstructure on the mechanical10.1007/BF02661333 ↗
4. The effect of microstructure on the stress-corrosion susceptibility of a high purity AI-Zn-Mg alloy in a NaCI solution10.1007/BF03038387 ↗
5. Plasticity-damage modeling of strain rate and temperature dependence of aluminum alloy 7075-T651
6. Microstructure and mechanical properties of dissimilar friction stir welding of 6061-to-7050 aluminum alloys10.1016/j.matdes.2015.05.074 ↗
7. Design of the multi-stage quenching process for 7050 aluminum alloy10.1016/j.matdes.2013.09.029 ↗
8. Effect of retrogression and reaging treatment on the microstructure and fatigue crack growth behavior of 7050 aluminum alloy thick plate10.1016/j.matdes.2013.09.063 ↗
9. The room temperature mechanical properties of hot rolled 7075 aluminum alloy10.1016/j.matdes.2011.05.019 ↗
10. Constitutive base analysis of a 7075 aluminum alloy during hot compression testing10.1016/j.matdes.2011.05.040 ↗
11. The role of microstructure in hydrogen-assisted fracture of 7075 aluminum10.1007/BF02811712 ↗
12. Calibration, validation, and verification including uncertainty of a physically motivated internal state variable plasticity and damage model10.1016/j.ijsolstr.2009.09.025 ↗
13. Deformation behavior and microstructure evolution of 7050 aluminum alloy during high temperature deformation10.1016/j.msea.2007.10.051 ↗
14. Effect of heat exposure on the fatigue properties of AA7050 friction stir welds10.1007/s11665-018-3379-6 ↗
15. N. Kaufmann, M. Imran, T.M. Wischeropp, C. Emmelmann, S. Siddique, F. Walther, Influence of process parameters on the quality of aluminium alloy en AW 7075 using Selective Laser Melting (SLM), 2016, doi: 10.1016/j.phpro.2016.08.096.10.1016/j.phpro.2016.08.096 ↗
16. Changing the alloy composition of Al7075 for better processability by selective laser melting10.1016/j.jmatprotec.2016.08.003 ↗
17. W. Reschetnik, J.-P. Brüggemann, M.E. Aydinöz, O. Grydinc, K.-P. Hoyerc, Fatigue crack growth behavior and mechanical properties of EN AW-7075 aluminium alloy, in: 21st European Conference on Fracture, 2016, vol. 2, pp. 3040–3048, doi: 10.1016/j.prostr.2016.06.380.10.1016/j.prostr.2016.06.380 ↗
18. A. Singh, A. Ramakrishnan, G. Dinda, Direct Laser Metal Deposition of Al 7050 Alloy, SAE Technical Paper, 2017, 2017-01-0286.10.4271/2017-01-0286 ↗
19. Free surface modeling of contacting solid metal flows employing the ALE formulation10.4028/www.scientific.net/KEM.504-506.431 ↗
20. Cladding of advanced Al alloys employing friction stir welding10.4028/www.scientific.net/KEM.554-557.1014 ↗
21. Friction surface cladding: an exploratory study of a new solid state cladding process10.1016/j.jmatprotec.2015.10.029 ↗
22. Microstructures and mechanical behavior of Inconel 625 fabricated by solid-state additive manufacturing10.1016/j.msea.2017.03.105 ↗
23. Microstructure-deformation relationship of additive friction stir-deposition Al–Mg–Si10.1016/j.mtla.2019.100387 ↗
24. Dynamic testing at high strain rates of an ultrafine-grained magnesium alloy processed by ECAP10.1016/j.msea.2009.03.032 ↗
25. Microstructures and mechanical properties of ultrafine grained 7075 Al alloy processed by ECAP and their evolutions during annealing10.1016/j.actamat.2004.06.017 ↗
26. Microstructure evolutions and mechanical properties of tubular aluminum produced by friction stir back extrusion10.1016/j.matdes.2014.09.018 ↗
27. Dynamic evolution of oxide scale on the surfaces of feed stock particles from cracking and segmenting to peel-off while cold spraying copper powder having a high oxygen content10.1016/j.jmst.2020.06.019 ↗
28. Heat treatment of cold-sprayed C355 Al for repair: microstructure and mechanical properties10.1007/s11666-017-0665-z ↗
29. Solid-state additive manufacturing high performance aluminum alloy 6061 enabled by an in-situ micro-forging assisted cold spray10.1016/j.msea.2020.139024 ↗
30. Microstructural evolution of 7075 Al gas atomized powder and high-pressure cold sprayed deposition10.1016/j.surfcoat.2014.04.035 ↗
31. Microstructure evolution during FSW/FSP of high strength aluminum alloys10.1016/j.msea.2005.06.009 ↗
32. Microstructural investigation of friction stir welded 7050-T651 aluminium10.1016/S1359-6454(02)00449-4 ↗
33. R.S. Mishra, M.W. Mahoney, S.X. Mcfadden, N.A. Mara, A.K. Mukherjee, High strain rate superplasticity in a friction stir processed 7075 Al alloy.
34. Grain refinement of aluminum alloys by friction stir processing10.1080/14786430500267745 ↗
35. Friction stir processing of aluminium alloy AA7075: microstructure, surface chemistry and corrosion resistance10.1016/j.corsci.2016.02.006 ↗
36. M. Navaser, M. Atapour, Effect of friction stir processing on pitting corrosion and intergranular attack of 7075 aluminum alloy, 2017, doi: 10.1016/j.jmst.2016.07.008.10.1016/j.jmst.2016.07.008 ↗
37. Microstructure and cyclic deformation behavior of a friction-stir-welded 7075 Al alloy10.1007/s11661-009-0152-3 ↗
38. Properties of friction-stir-welded 7075 T651 aluminum10.1007/s11661-998-0021-5 ↗
39. Friction stir additive manufacturing for high structural performance through microstructural control in an Mg based WE43 alloy10.1016/j.matdes.2014.09.082 ↗
40. Formation characteristic, microstructure, and mechanical performances of aluminum-based components by friction stir additive manufacturing10.1007/s00170-015-7695-9 ↗
41. Surface characterization and influence of anodizing process on fatigue life of Al 7050 alloy10.1016/j.matdes.2011.02.027 ↗
42. Improvement of weld temperature distribution and mechanical properties of 7050 aluminum alloy butt joints by submerged friction stir welding10.1016/j.matdes.2011.06.021 ↗
43. Fatigue behavior of freestanding AA2024 and AA7075 cold spray deposits10.1016/j.ijfatigue.2018.03.007 ↗
44. Direct recycling of machine chips through a novel solid-state additive manufacturing process10.1016/j.matdes.2020.108850 ↗
45. Effect of thermomechanical processing on fatigue behavior in solid-state additive manufacturing of Al-Mg-Si alloy10.3390/met10070947 ↗
46. Friction stir welding of a commercial 7075-T6 aluminum alloy: grain refinement, thermal stability and tensile properties10.2320/matertrans.45.2503 ↗
47. Stir zone microstructure and strain rate during Al 7075-T6 friction stir spot welding10.1007/BF02586110 ↗
48. Evolution of microstructure and mechanical properties in naturally aged 7050 and 7075 Al friction stir welds10.1016/j.msea.2009.11.057 ↗
49. Friction stir processing of 7075 Al alloy and subsequent aging treatment10.1016/S1003-6326(15)63910-3 ↗
50. Friction-stir welding effects on microstructure and fatigue of aluminum alloy 7050-T7451
51. Influence of texture and grain refinement on the mechanical behavior of AA2219 fabricated by high shear solid state material deposition10.1016/j.msea.2018.03.088 ↗
52. Fatigue behavior of solid-state additive manufactured inconel 62510.1007/s11837-018-3114-7 ↗
53. Influence of grain refinement and microstructure on fatigue behavior for solid-state additively manufactured Al-Zn-Mg-Cu alloy10.1007/s11661-020-05746-9 ↗
54. Additive friction stir-enabled solid-state additive manufacturing for the repair of 7075 aluminum alloy10.3390/app9173486 ↗
55. R. Mishra, M.W. Mahoney, Y. Sato, Y. Hovanski, R. Verma, Friction stir welding and processing VII, 2016.10.1007/978-3-319-48108-1 ↗
56. ASTM, E384-17 Standard Test Method for Microindentation Hardness of Materials, ASTM International, pp. 1–40, 2017, doi: 10.1520/E0384-17.10.1520/E0384-17 ↗
57. ASTM, Standard Practice for Determining Average Grain Size Using Electron Backscatter Diffraction (EBSD) in Fully Recrystallized Polycrystalline Materials, ASTM International, pp. 1–5, 2014, doi: 10.1520/E2627.10.1520/E2627 ↗
58. Plasticity and fracture modeling/experimental study of a porous metal under various strain rates, temperatures, and stress states10.1115/1.4025292 ↗
59. Modeling and experimental study of fatigue of powder metal steel (FC-0205)10.1179/1743290113Y.0000000063 ↗
60. Strain rate effect on the tension and compression stress-state asymmetry for electron beam additive manufactured Ti6Al4V10.1016/j.msea.2017.12.062 ↗
61. Effect of strain-induced precipitation on the low angle grain boundary in AA7050 aluminum alloy10.1016/j.matdes.2011.04.025 ↗
62. Evolution of microstructure and mechanical properties in naturally aged 7050 and 7075 Al friction stir welds10.1016/j.msea.2009.11.057 ↗
63. Microstructural evolution in aluminium alloy 7050 during processing10.1016/j.msea.2004.05.006 ↗
64. Quantitative metallography of precipitating and secondary phases after strengthening treatment of net shaped casting of Al-Zn-Mg-Cu (7000) alloys10.1016/j.msea.2017.05.047 ↗
65. Nucleation mechanisms of dynamic recrystallization in Inconel 625 superalloy deformed with different strain rates10.1007/s12598-012-0494-7 ↗
66. Processing maps for hot deformation of the extruded 7075 aluminum alloy bar: anisotropy of hot workability10.1016/j.msea.2014.07.072 ↗
67. Dynamic softening behaviors of 7075 aluminum alloy10.1016/S1003-6326(10)60104-5 ↗
68. The microstructure evolution and nucleation mechanisms of dynamic recrystallization in hot-deformed Inconel 625 superalloy10.1016/j.matdes.2010.07.040 ↗
69. Relation between axial stresses and texture development during torsion testing: a simplified theory10.1016/0001-6160(85)90035-5 ↗
70. Effect of texture on earing in FCC metals: finite element simulations10.1016/S0749-6419(97)00044-2 ↗
71. EBSD study on microstructure and texture of friction stir welded AA5052-O and AA6061-T6 dissimilar joint10.1016/j.matdes.2015.08.060 ↗
72. On the microstructure and mechanical properties of similar and dissimilar AA7075 and AA2024 friction stir welding joints: effect of rotational speed10.1016/j.jmapro.2018.12.014 ↗
73. Heterogeneity of crystallographic texture in friction stir welds of aluminum10.1007/s11661-001-1037-2 ↗
74. Grain structure and texture evolution during friction stir welding of thin 6016 aluminum alloy sheets10.1016/j.msea.2009.11.029 ↗
75. Temperature evolution, microstructure and mechanical properties of friction stir welded thick 2219-O aluminum alloy joints10.1016/j.matdes.2008.09.021 ↗
76. Texture evolution and deformation mechanism in friction stir welding of 2219Al10.1016/j.msea.2014.06.014 ↗
77. Microtexture in the friction-stir weld of an aluminum alloy10.1007/s11661-001-0351-z ↗
78. Prediction of tricomponent plane stress yield surfaces and associated flow and failure behavior of strongly textured f.c.c. polycrystalline sheets10.1016/0025-5416(87)90494-0 ↗
79. Texture variations in an aluminum friction stir weld10.1016/j.scriptamat.2007.06.068 ↗
80. Axial stresses and texture development during the torsion testing of Al, Cu and α-Fe10.1016/0001-6160(84)90187-1 ↗
81. Three-dimensional particle cracking damage development in an Al-Mg-base wrought alloy10.1016/S0921-5093(03)00103-5 ↗
82. Quantification of damage evolution in a 7075 aluminum alloy using an acoustic emission technique10.1016/j.msea.2011.05.017 ↗
83. V. 2 ASM International Handbook, Heat treating, Metal Finishing, 101, p. 87, 2003, doi: 10.1016/S0026-0576(03)90166-8.10.1016/S0026-0576(03)90166-8 ↗