Microstructure evolution and mechanical properties of the wire + arc additive manufacturing Al-Cu alloy
Source abstract
Abstract
Abstract Understanding and clarifying the formation and evolution mechanism of the microstructure in wire + arc additive manufacturing (WAAM) Al-Cu alloy is primary and essential for achieving the higher and more isotropic mechanical properties. In this study, the evolution of grain structure, precipitated phases and corresponding mechanical properties of the as-deposited WAAM processed 2219 Al-Cu alloy are investigated. The microstructure exhibits the heterogeneous band characteristics between the fine equiaxed α-Al grains in inter-layer zone (ITZ) and the columnar α-Al grains in inner-layer zone (INZ). Based on the re-melting experiment and the time-dependent nucleation theory, the occurrence of equiaxed grains is attributed to the heterogeneous nucleation of α-Al caused by the prior precipitation of Al3Zr particles at the molten pool boundaries. The relationship between the solidification conditions and the number of the prior Al3Zr nucleation sites is established. A large amount of spherical θ″-Al2Cu phases precipitate in Cu-rich regions around the α-Al+θ-Al2Cu eutectics and they agglomerate and transform to flaky-like θ′ phases under the in-situ thermal effect during WAAM deposition. The hardness of the ITZ (81 ± 2.7HV) is approximately 12% higher than that of the INZ (74 ± 3.6HV) which is mainly due to the finer grains and the more dispersive precipitates in ITZ.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (65)
Show source-provided references
1. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
2. Dislocation network in additive manufactured steel breaks strength–ductility trade-off10.1016/j.mattod.2017.11.004 ↗
3. Effects of heat accumulation on microstructure and mechanical properties of Ti6Al4V alloy deposited by wire arc additive manufacturing
4. Fabricating superior NiAl bronze components through wire arc additive manufacturing10.3390/ma9080652 ↗
5. In-depth study of the mechanical properties for Fe3Al based iron aluminide fabricated using the wire-arc additive manufacturing process10.1016/j.msea.2016.05.047 ↗
6. Oxide accumulation effects on wire + arc layer-by-layer additive manufacture process10.1016/j.jmatprotec.2017.10.030 ↗
7. A review of wire arc additive manufacturing and advances in wire arc additive manufacturing of aluminium10.1080/02670836.2018.1455012 ↗
8. Arc-based additive manufacturing of steel components—comparison of wire- and powder-based variants10.1007/s40194-017-0527-9 ↗
9. Study on arc welding processes for high deposition rate additive manufacturing10.1016/j.procir.2017.12.095 ↗
10. Wire and arc additive manufacturing of aluminum components10.3390/met9050608 ↗
11. Wire arc additive manufacturing of Al-Zn-Mg-Cu alloy: microstructures and mechanical properties
12. Microstructure, residual stress and tensile properties control of wire-arc additive manufactured 2319 aluminum alloy with laser shock peening10.1016/j.jallcom.2018.02.353 ↗
13. Effect of arc mode in cold metal transfer process on porosity of additively manufactured Al-6.3%Cu alloy
14. The effect of inter-layer cold working and post-deposition heat treatment on porosity in additively manufactured aluminum alloys10.1016/j.jmatprotec.2015.11.006 ↗
15. Effect of characteristic substrate parameters on the deposition geometry of CMT additive manufactured Al-6.3%Cu alloy10.1016/j.applthermaleng.2019.114302 ↗
16. The influence of build parameters and wire batch on porosity of wire and arc additive manufactured aluminium alloy 231910.1016/j.jmatprotec.2018.07.030 ↗
17. The strengthening effect of inter-layer cold working and post-deposition heat treatment on the additively manufactured Al–6.3Cu alloy10.1016/j.msea.2015.10.101 ↗
18. A comparative study of additively manufactured thin wall and block structure with Al-6.3%Cu alloy using cold metal transfer process10.3390/app7030275 ↗
19. Mechanical properties and fracture behaviors of GTA-additive manufactured 2219-Al after an especial heat treatment10.1007/s11665-017-2627-5 ↗
20. Mechanical properties of 2219-Al components produced by additive manufacturing with TIG
21. Microstructure and mechanical properties of double-wire + arc additively manufactured Al-Cu-Mg alloys10.1016/j.jmatprotec.2017.12.019 ↗
22. Microstructure evolution and mechanical behavior of 2219 aluminum alloys additively fabricated by the cold metal transfer process10.3390/ma11050812 ↗
23. Hot deformation induced microstructural evolution in local-heterogeneous wire + arc additive manufactured 2219 Al alloy10.1016/j.jallcom.2021.158949 ↗
24. Mechanical properties and precipitation behavior of the heat-treated wire + arc additively manufactured 2219 aluminum alloy10.1016/j.matchar.2020.110735 ↗
25. Laser-based directed energy deposition of novel Sc/Zr-modified Al-Mg alloys: columnar-to-equiaxed transition and aging hardening behavior10.1016/j.jmst.2020.08.003 ↗
26. Effect of laser rescanning on the grain microstructure of a selective laser melted Al-Mg-Zr alloy10.1016/j.matchar.2018.03.033 ↗
27. A solution to the hot cracking problem for aluminium alloys manufactured by laser beam melting10.1016/j.actamat.2020.07.015 ↗
28. Columnar to equiaxed transition in Al-Mg(-Sc)-Zr alloys produced by selective laser melting10.1016/j.scriptamat.2017.10.021 ↗
29. Influence of travel speed on microstructure and mechanical properties of wire + arc additively manufactured 2219 aluminum alloy10.1016/j.jmst.2019.06.016 ↗
30. The CMT short-circuiting metal transfer process and its use in thin aluminium sheets welding10.1016/j.matdes.2008.07.015 ↗
31. Characterisation of the composition and volume fraction of η′ and η precipitates in an Al–Zn–Mg alloy by a combination of atom probe, small-angle X-ray scattering and transmission electron microscopy10.1016/j.actamat.2005.03.004 ↗
32. Finite-element modeling of heat flow in deep-penetration laser welds in aluminum alloys10.1080/10407788908944721 ↗
33. Analysis of temperature and stress field in Al alloy’s twin wire welding10.1016/j.tafmec.2005.06.006 ↗
34. Numerical analysis of thermal fluid transport behavior during electron beam welding of 2219 aluminum alloy plate10.1016/S1003-6326(17)60153-5 ↗
35. Microstructure and mechanical properties of wire + arc additively manufactured 2024 aluminum alloy components: As-deposited and post heat-treated10.1016/j.jmapro.2019.03.003 ↗
36. Pore formation and evolution in wire + arc additively manufactured 2319 Al alloy
37. P D Hydrogen porosity in directionally solidified aluminium–copper alloys a mathematical model10.1016/S1359-6454(01)00043-X ↗
38. On the role of Zr content into Portevin-Le Chatelier (PLC) effect of selective laser melted high strength Al-Cu-Mg-Mn alloy10.1016/j.matlet.2019.03.112 ↗
39. Laser powder bed fusion of high-strength Sc/Zr-modified Al–Mg alloy: phase selection, microstructural/mechanical heterogeneity, and tensile deformation behavior10.1016/j.jmst.2021.03.069 ↗
40. Strength and strain hardening of a selective laser melted AlSi10Mg alloy10.1016/j.scriptamat.2017.07.025 ↗
41. External filler wire based GMA-AM process of 2219 aluminum alloy10.1080/10426914.2020.1779936 ↗
42. Effects of process conditions on the mechanical behavior of aluminium wrought alloy EN AW-2219 (AlCu6Mn) additively manufactured by laser beam melting in powder bed10.3390/mi8010023 ↗
43. Microstructures and tensile fracture behavior of 2219 wrought Al–Cu alloys with different impurity of Fe10.3390/met11010174 ↗
44. Single-crystal laser deposition of superalloys: processing–microstructure maps10.1016/S1359-6454(00)00367-0 ↗
45. R.T.M. Gäumann, W. Kurz, Nucleation ahead of the advancing interface in directional solidification, Materials Science and Engineering: A 226–228, 763–769. An experimental investigation of the columnar-to-equiaxed grain transition in aluminum, 1997.10.1016/S0921-5093(97)80081-0 ↗
46. An experimental investigation of the columnar-to-equiaxed grain transition in aluminum–copper hypoeutectic and eutectic alloys10.1016/j.jcrysgro.2010.04.040 ↗
47. Huang · 2007
48. Simulation of the columnar-to-equiaxed transition in directionally solidified Al–Cu alloys10.1016/j.actamat.2004.10.019 ↗
49. Dendrite growth at the limit of stability: tip radius and spacing10.1016/0001-6160(81)90082-1 ↗
50. The measurement of self-diffusion coefficients in liquid metals with quasielastic neutron scattering
51. The use of computational thermodynamics for the determination of surface tension and Gibbs–Thomson coefficient of multicomponent alloys10.1007/s00161-018-0670-6 ↗
52. Correlation between unsteady-state solidification conditions, dendrite spacings, and mechanical properties of Al-Cu alloys
53. Electron beam welding of AlSi10Mg workpieces produced by selected laser melting additive manufacturing technology
54. A mechanism for the formation of equiaxed grains in welds of aluminum–lithium alloy 209010.1016/S0921-5093(02)00858-4 ↗
55. Proposed mechanism for equiaxed grain formation along the fusion boundary in aluminum-copper-lithium alloys
56. Weldability of commercial AL-CU-LI Alloys10.4028/www.scientific.net/MSF.217-222.1685 ↗
57. Solution of the non-steady state problem in nucleation kinetics
58. Formation of crystal nuclei in liquid metals10.1063/1.1699435 ↗
59. Preferential nucleation in undercooled liquid aluminium alloys10.1179/mst.1988.4.2.157 ↗
60. Prediction of phase selection in rapid solidification using time dependent nucleation theory10.1016/0956-7151(94)90391-3 ↗
61. Homogeneous crystal nucleation in binary metallic melts10.1016/0001-6160(83)90019-6 ↗
62. Criteria for developing castable, creep-resistant aluminum-based alloys − a review10.3139/146.101249 ↗
63. Effect of ZrB2 particles on the microstructure and mechanical properties of hybrid (ZrB2 + Al3Zr)/AA5052 insitu composites10.1016/j.jallcom.2015.07.096 ↗
64. processes on the solid metal-molten metal interface, 6(20) (1984) 501-50710.1007/BF00723542 ↗
65. Strength-ductility synergy of selective laser melted Al-Mg-Sc-Zr alloy with a heterogeneous grain structure