3D laser shock peening – A new method for improving fatigue properties of selective laser melted parts
Source abstract
Abstract
Abstract Although Selective Laser Melting (SLM) currently revolutionizes the way parts are being manufactured, certain process inherent limitations such as accumulation of residual stresses and increased porosity content can lead to a decrease in fatigue life of produced parts. 3D Laser Shock Peening is a new hybrid additive manufacturing process whereby a periodic Laser Shock Peening (LSP) treatment is added to the standard SLM process. LSP can be applied selectively in the 3D volume of metallic parts, and is shown to influence the bulk internal stress state and hardness, as well as the distribution of porosities in the material. Here, a decoupled 3D LSP process was used, i.e. LSP treatments were applied during the SLM process, by removing the sample from the SLM chamber whenever needed. We report fatigue lives of 316 L stainless steel multiplied by more than 15 times compared to standard SLM parts, and more than 57 times compared to conventional manufacturing, with a significant improvement over other state-of-the art methods. The effect of the 3D LSP treatment on SLM parts and the consequence on crack initiation and propagation is investigated by measuring the near surface residual stresses, imaging the fractured surface, measuring the porosity content and analyzing the microstructure and microhardness.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Surface Treatment and Residual Stress · Additive Manufacturing Materials and Processes · Laser Material Processing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. 2018
2. 2018
3. Fatigue analysis in selective laser melting: review and investigation of thin-walled actuator housings
4. Part and material properties in selective laser melting of metals
5. The influence of the laser scan strategy on grain structure and cracking behaviour in SLM powder-bed fabricated nickel superalloy10.1016/j.jallcom.2014.06.172 ↗
6. Residual stresses in selective laser sintering and selective laser melting10.1108/13552540610707013 ↗
7. Selective Laser Melting of Crack-Free High Density M2 High Speed Steel Parts by Baseplate Preheating10.1115/1.4028513 ↗
8. Investigations on residual stresses and deformations in selective laser melting10.1007/s11740-009-0192-y ↗
9. Residual stress within metallic model made by selective laser melting process10.1016/S0007-8506(07)60677-5 ↗
10. Quality part production via multi-laser additive manufacturing10.1016/j.mfglet.2017.05.003 ↗
11. Correlation of the high power SLM process with resulting material properties for IN71810.1007/s00501-017-0589-4 ↗
12. Highly anisotropic steel processed by selective laser melting10.1007/s11663-013-9875-z ↗
13. In-situ residual stress reduction, martensitic decomposition and mechanical properties enhancement through high temperature powder bed pre-heating of Selective Laser Melted Ti6Al4V10.1016/j.msea.2017.04.033 ↗
14. A comparison of the tensile, fatigue, and fracture behavior of Ti–6Al–4V and 15-5 PH stainless steel parts made by selective laser melting10.1007/s00170-013-5106-7 ↗
15. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
16. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
17. Microstructure and mechanical properties of Hastelloy X produced by HP-SLM (high power selective laser melting)10.1016/j.matdes.2019.107598 ↗
18. Grain structure control of additively manufactured metallic materials10.3390/ma10111260 ↗
19. Tribological behavior of aluminum alloys in a vibratory finishing process10.1016/S0043-1648(03)00124-8 ↗
20. Improvement of fatigue life of Ti–6Al–4V alloy by laser shock peening10.1016/j.msea.2010.01.076 ↗
21. Effect of laser shock peening on residual stress and fatigue life of clad 2024 aluminium sheet containing scribe defects10.1016/j.msea.2012.04.002 ↗
22. Laser shock processing and its effects on microstructure and properties of metal alloys: a review10.1016/S0142-1123(02)00022-1 ↗
23. Enhancement of surface characteristics of direct metal laser sintered stainless steel 316L by shot peening10.1016/j.surfin.2018.04.010 ↗
24. Improving the surface quality and mechanical properties by shot-peening of 17-4 stainless steel fabricated by additive manufacturing10.1016/j.matdes.2016.08.037 ↗
25. Ultrasonic impact peening for the surface properties’ management10.1016/j.jsv.2007.03.054 ↗
26. Laser Peening Process and Its Impact on Materials Properties in Comparison with Shot Peening and Ultrasonic Impact Peening10.3390/ma7127925 ↗
27. Regain the fatigue strength of laser additive manufactured Ti alloy via laser shock peening10.1016/j.jallcom.2018.04.029 ↗
28. Laser peening: a tool for additive manufacturing post-processing
29. Method and device for implementing laser shock peening or warm laser shock peening during selective laser melting
30. Tailoring residual stress profile of selective laser melted parts by laser shock peening
31. Laser Shock Peening: a promising tool for tailoring metallic microstructures in Selective Laser Melting
32. 3D Laser Shock Peening – a new method for the 3D control of residual stresses in Selective Laser Melting10.1016/j.matdes.2017.05.083 ↗
33. 3D laser shock peening as a way to improve geometrical accuracy in selective laser melting
34. Healing cracks in selective laser melting by 3D laser shock peening
35. Effect of laser shock peening on aluminium alloy laser-welds10.1080/02670844.2016.1194513 ↗
36. Reducing porosity in AlSi10Mg parts processed by selective laser melting
37. Anisotropic high cycle fatigue behavior of Ti–6Al–4V obtained by powder bed laser fusion10.1016/j.ijfatigue.2016.04.032 ↗
38. Random-type scanning patterns in laser shock peening without absorbing coating in 2024-T351 Al alloy: A solution to reduce residual stress anisotropy10.1016/j.optlastec.2015.04.027 ↗
39. Fatigue striation spacing analysis10.1016/1044-5803(94)90046-9 ↗
40. Effect of surface roughness on fatigue performance of additive manufactured Ti–6Al–4V
41. Fatigue properties of type 316LN stainless steel in air and mercury
42. Fatigue performance of additive manufactured metallic parts
43. Effects of hot isostatic pressing on the elastic modulus and tensile properties of 316L parts made by powder bed laser fusion10.1016/j.msea.2017.03.100 ↗
44. On the fatigue properties of metals manufactured by selective laser melting – the role of ductility10.1557/jmr.2014.157 ↗
45. On the fatigue crack growth behavior in 316L stainless steel manufactured by selective laser melting10.1016/j.engfracmech.2014.03.008 ↗
46. Subsurface crack initiation during fatigue as a result of residual stresses10.1111/j.1460-2695.1979.tb00388.x ↗
47. Laser shock peening induced residual stresses and the effect on crack propagation behavior10.1016/j.ijfatigue.2017.04.002 ↗
48. Four-dimensional annihilation behaviors of micro pores during surface cold working10.2320/matertrans.M2010069 ↗
49. Enhanced fatigue behavior of powder metallurgy Ti–6Al–4V alloy by applying ultrasonic impact treatment10.1016/j.msea.2015.06.072 ↗
50. Influence of ultrasonic surface rolling on microstructure and wear behavior of selective laser melted Ti-6Al-4V alloy10.3390/ma10101203 ↗
51. Process dependent porosity and the influence of shot peening on porosity morphology regarding selective laser melted AlSi10Mg parts
52. Porosity induced fatigue damage of laser welded 7075-T6 joints investigated via synchrotron X-ray microtomography10.1179/1362171814Y.0000000249 ↗
53. Statistical assessment of fatigue crack initiation from sub-surface hydrogen micropores in high-quality die-cast aluminum10.1016/j.actamat.2011.04.049 ↗
54. Experimental study of porosity and its relation to fatigue mechanisms of model Al–Si7–Mg0.3 cast Al alloys10.1016/S0921-5093(01)01225-4 ↗
55. Influence of SLM process parameters on the surface finish, porosity rate and fatigue behavior of as-built Inconel 625 parts10.1016/j.jmatprotec.2017.12.043 ↗