journal article·2020-03Open access

Effects of inter layer time and build height on resulting properties of 316L stainless steel processed by laser powder bed fusion

Gunther Mohr, Simon J. Altenburg, Kai Hilgenberg

Abstract

Laser powder bed fusion (L-PBF) is the most prominent additive manufacturing (AM) technology for metal part production. Among the high number of factors influencing part quality and mechanical properties, the inter layer time (ILT) between iterative melting of volume elements in subsequent layers is almost completely unappreciated in the relevant literature on L-PBF. This study investigates the effect of ILT with respect to build height and under distinct levels of volumetric energy density (VED) using the example of 316L stainless steel. In-situ thermography is used to gather information on cooling conditions during the process, which is followed by an extensive metallographic analysis. Significant effects of ILT and build height on heat accumulation, sub-grain sizes, melt pool geometries and hardness are presented. Furthermore, the rise of defect densities can be attributed to a mutual interplay of build height and ILT. Hence, ILT has been identified as a crucial factor for L-PBF of real part components especially for those with small cross sections.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
2. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
3. Wohlers · 2017
4. Materials for additive manufacturing10.1016/j.cirp.2017.05.009 ↗
5. Microstructure and mechanical properties of as-processed scandium-modified aluminium using selective laser melting10.1016/j.cirp.2016.04.057 ↗
6. Processability of high strength aluminium-copper alloys AW-2022 and 2024 by laser beam melting in powder bed
7. Processing of a high-strength Al-Fe-Ni alloy using laser beam melting and its potential for in-situ graded mechanical properties
8. Damage development and damage tolerance of structure maanufactuired by selective laser melting - a review10.1016/j.prostr.2017.11.071 ↗
9. Schulze · 2010
10. Lowering thermal gradients in Selective Laser melting by pre-heating the baseplate
11. Residual stress within metallic model made by selective laser melting process10.1016/S0007-8506(07)60677-5 ↗
12. Rapid tooling by laser powder deposition: process simulation using finite element analysis10.1016/j.actamat.2005.05.003 ↗
13. Effects of process time interval and heat treatment on the mechanical and microstructural properties of direct laser deposited 316L stainless steel10.1016/j.msea.2015.07.056 ↗
14. Investigation of temperature and stress fields in laser cladded coatings10.1016/j.apsusc.2007.08.014 ↗
15. Effect of inter-layer dwell time on distortion and residual stress in additive manufacturing of titanium and nickel alloys10.1016/j.jmatprotec.2014.07.030 ↗
16. On the influence of inter-layer time and energy density on selected critical-to-quality properties of PA12 parts produced via laser sintering10.1016/j.polymertesting.2017.05.027 ↗
17. Möhrle · 2018
18. Hartogh · 2018 · 69
19. A decision support system for the validation of metal powder bed-based additive manufacturing applications10.1007/s00170-018-1676-8 ↗
20. Cost-driven build orientation and bin packing of parts in Selective Laser Melting (SLM)10.1016/j.ejor.2018.07.053 ↗
21. Production scheduling and nesting in additive manufacturing10.1016/j.cie.2018.09.048 ↗
22. Influence of build layout and orientation on microstructural characteristics of electron beam melted Alloy 71810.1007/s00170-018-2621-6 ↗
23. On the energy efficiency of pre-heating methods in SLM/SLS processes10.1007/s00170-017-1287-9 ↗
24. In situ tailoring microstructure in additively manufactured Ti-6Al-4V for superior mechanical performance10.1016/j.actamat.2016.12.027 ↗
25. New development in selective laser melting of Ti–6Al–4V: a wider processing window for the achievement of fully lamellar α + β microstructures10.1007/s11837-017-2599-9 ↗
26. Torries · 2016 · 1272
27. Build-up strategies for additive manufacturing of three dimensional Ti-6Al-4V-parts produced by laser metal deposition10.2351/1.4997852 ↗
28. Krauss · 2017
29. Consolidation phenomena in laser and powder-bed based layered manufacturing10.1016/j.cirp.2007.10.004 ↗
30. DIN · 2013
31. Microstructure, solidification texture, and thermal stability of 316 L stainless steel manufactured by laser powder bed fusion10.3390/met8080643 ↗
32. Intrinsic strain aging, Σ3 boundaries, and origins of cellular substructure in additively manufactured 316L
33. Saeidi · 2016
34. In situ heat treatment in selective laser melted martensitic AISI 420 stainless steels10.1016/j.matdes.2015.08.045 ↗
35. DIN · 2006
36. Laser powder bed fusion of stainless steel grades: a review10.3390/met9070731 ↗
37. An investigation into the effect of process parameters on melt pool geometry, cell spacing, and grain refinement during laser powder bed fusion10.1016/j.optlastec.2019.03.012 ↗
38. Effect of build geometry on the microstructural development of 316L parts produced by additive manufacturing10.1016/j.matchar.2018.04.040 ↗
39. Melt pool sensing and size analysis in laser powder-bed metal additive manufacturing10.1016/j.jmapro.2018.04.002 ↗