Abstract Additive manufacturing can produce parts with complex geometries in fewer steps than conventional processing, which leads to cost reduction and a higher quality of goods. One potential application is the production of molds and dies with conformal cooling for injection molding, die casting, and forging. AISI H13 tool steel is typically used in these applications because of its high hardness at elevated temperatures, high wear resistance, and good toughness. However, available data on the processing of H13 steel by additive manufacturing are still scarce. Thus, this study focused on the processability of H13 tool steel by powder bed fusion and its microstructural characterization. Laser power (97−216 W) and scan speed (300−700 mm/s) were varied, and the consolidation of parts, common defects, solidification structure, microstructure, and hardness were evaluated. Over the range of processing parameters, microstructural features were mostly identical, consisting of a predominantly cellular solidification structure of martensite and 19.8 %–25.9 % of retained austenite. Cellular/dendritic solidification structure displayed C, Cr, and V segregation toward cell walls. The thermal cycle resulted in alternating layers of heat-affected zones, which varied somewhat in hardness and microstructure. Retained austenite was correlated to the solidification structure and displayed a preferential orientation with {001}//build direction. Density and porosity maps were obtained by helium gas pycnometry and light optical microscopy, respectively, and, along with linear crack density, were used to determine appropriate processing parameters for H13 tool steel. Thermal diffusivity, thermal conductivity, and thermal capacity were measured to determine dimensionless processing parameters, which were then compared to others reported in the literature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Digital manufacturing- applications past, current, and future trends10.1016/j.proeng.2017.01.250 ↗
2. Direct digital manufacturing: definition, evolution, and sustainability implications10.1016/j.jclepro.2015.05.009 ↗
3. Direct rapid tooling: a review of current research10.1108/13552549810210248 ↗
4. Rapid tooling: the state of the art10.1016/S0924-0136(00)00613-0 ↗
5. Rapid prototyping and tooling techniques: a review of applications for rapid investment casting10.1007/s00170-003-1840-6 ↗
6. Rapid tooling route selection and evaluation for sand and investment casting10.1080/17452750701747088 ↗
7. Rapid prototyping – a technology transfer approach for development of rapid tooling10.1108/13552540910979794 ↗
8. A cost-effective approach for rapid fabricating cooling channels with smooth surface10.1007/s00170-017-1328-4 ↗
9. A framework for optimizing the design of injection molds with conformal cooling for additive manufacturing10.1016/j.promfg.2015.09.049 ↗
10. Hot extrusion dies with conformal cooling channels produced by additive manufacturing10.1016/j.matpr.2015.10.028 ↗
11. A methodological framework for the inclusion of modern additive manufacturing into the production portfolio of a focused factory10.1016/j.jmsy.2014.07.014 ↗
12. Predicting the future of additive manufacturing: a Delphi study on economic and societal implications of 3D printing for 203010.1016/j.techfore.2017.01.006 ↗
13. Numerical and experimental evaluation of a conformally cooled H13 steel injection mould manufactured with selective laser melting10.1007/s00170-017-0426-7 ↗
14. dies and die materials for Hot forging
15. ASM International · 1990
16. Ultrahigh-strength steels
17. Direct selective laser sintering of tool steel powders to high density. Part B: the effect on microstructural evolution
18. Direct selective laser sintering of tool steel powders to high density. Part a: effects of laser beam width and scan strategy
19. SLM additive manufacture of H13 tool steel with conformal cooling and structural lattices10.1108/RPJ-06-2014-0075 ↗
20. Preparation and mechanical properties of selective laser melted H13 steel
21. Optimization and simulation of SLM process for high density H13 tool steel parts10.1016/j.phpro.2016.08.004 ↗
22. Heat treatment and properties of a hot work tool steel fabricated by additive manufacturing10.1016/j.msea.2019.03.027 ↗
23. Selective laser melting of TiC/H13 steel bulk-form nanocomposites with variations in processing parameters10.1557/mrc.2017.9 ↗
24. General investigations on processing tool steel X40CrMoV5-1 with selective laser melting10.1016/j.jmatprotec.2018.01.012 ↗
25. Application of base plate preheating during selective laser melting10.1016/j.procir.2018.08.002 ↗
26. Microstructure and mechanical behavior of hot-work tool steels processed by Selective Laser Melting10.1016/j.matchar.2018.01.015 ↗
27. Influence of post treatment on microstructure, porosity and mechanical properties of additive manufactured H13 tool steel10.1016/j.msea.2018.08.046 ↗
28. Selective laser melting of TiB2/H13 steel nanocomposites: influence of hot isostatic pressing post-treatment10.1016/j.jmatprotec.2017.01.019 ↗
29. Density of additively-manufactured, 316L SS parts using laser powder-bed fusion at powers up to 400 W10.1007/s00170-014-5954-9 ↗
30. NIH Image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
31. Cullity · 1978
32. Wrought tool steels
33. An overview of powder granulometry on feedstock and part performance in the selective laser melting process
34. Effects of heat treatment on mechanical properties of h13 steel10.1007/s11041-010-9288-4 ↗
35. Influence of scan strategy and process parameters on microstructure and its optimization in additively manufactured nickel alloy 625 via laser powder bed fusion10.1007/s00170-016-9429-z ↗
36. Modeling and simulation of thermal field and solidification in laser powder bed fusion of nickel alloy IN62510.1016/j.optlastec.2018.08.016 ↗
37. The influence of the laser scan strategy on grain structure and cracking behaviour in SLM powder-bed fabricated nickel superalloy10.1016/j.jallcom.2014.06.172 ↗
38. A comprehensive study on microstructure and tensile behaviour of a selectively laser melted stainless steel10.1038/s41598-018-26136-7 ↗
39. Microstructure evolution and EBSD analysis of a graded steel fabricated by laser additive manufacturing10.1016/j.vacuum.2017.03.021 ↗
40. Microstructural characterization and mechanical performance of hot work tool steel processed by selective laser melting10.1007/s11663-014-0267-9 ↗
41. Diffusion and agglomeration of helium in stainless steel in the temperature range from RT to 600°C10.1016/S0168-583X(00)00018-5 ↗
42. Influence of powder bed preheating on microstructure and mechanical properties of H13 tool steel SLM parts10.1016/j.phpro.2016.08.092 ↗
43. Normalised model-based processing diagrams for additive layer manufacture of engineering alloys10.1016/j.actamat.2016.02.025 ↗
44. Diagrams for laser materials processing10.1016/0956-7151(92)90097-X ↗
45. Laser surface hardening of H13 steel in the melt case10.1016/j.matlet.2005.02.026 ↗
46. Residual stresses and cracking in Metal/Ceramic systems for microelectronics packaging10.1111/j.1151-2916.1985.tb09648.x ↗
47. An investigation on the usefulness and performance of new hot working tool steel by nitrocarburizing process10.1380/ejssnt.2012.1 ↗