journal article·2022-09

Development of a high strength Zr/Sc/Hf-modified Al-Mn-Mg alloy using Laser Powder Bed Fusion: Design of a heterogeneous microstructure incorporating synergistic multiple strengthening mechanisms

Qiuge Li, Guichuan Li, Xin Lin, Daiman Zhu, Jinhang Jiang, Shuoqing Shi, Fenggang Liu, Weidong Huang, Kim Vanmeensel

Publisher page

Abstract

Laser Powder Bed Fusion (L-PBF) provides great advantages in creating supersaturated solid solutions due to its intrinsic ultrafast cooling and high solidification rate, which is particularly desired for enhanced solid solution strengthening and precipitation strengthening. In the present work, a novel high strength Zr/Sc/Hf-modified Al-Mn-Mg alloy with a good L-PBF processability is investigated. The as-built alloy exhibits a heterogeneous microstructure featuring a bi-modal grain structure with coarse columnar and fine equiaxed grains and heterogeneously distributed nanometer and submicrometer-sized cuboid-shaped primary Al3(Sc,Zr,Hf) particles. The Al3(Sc,Zr,Hf) phase, exhibiting a homogeneous elemental distribution of Zr, Sc, and Hf, adopts a cubic L12 structure with a lattice parameter of 0.4044 ± 0.009 nm, showing a good coherency with α-Al. Additionally, the rapid L-PBF solidification enables the formation of submicrometer-sized elongated and globular primary Al6Mn and a supersaturated Al matrix with a high dislocation density. This results in a good combination of strength (yield strength of 438 ± 3 MPa and ultimate tensile strength of 504 ± 2 MPa) and ductility (elongation at fracture of 10.9 ± 1.4 %), with a moderate work hardening strength of 113 ± 12 MPa. Direct-ageing at 325 °C for 10 h promotes the formation of a large amount of rod-shaped Al6Mn precipitates and a few spherical Al3(Sc,Zr,Hf) nanoprecipitates. The heat treatment increases the hardness from 166 ± 2 HV in as-built condition to 173 ± 4 HV and enhances the tensile strength (yield strength of 487 ± 2 MPa and ultimate tensile strength of 542 ± 3 MPa) but slightly reduces the ductility to 7.4 ± 0.7 %. The high strength was achieved by the synergistic effect of grain boundary strengthening, solid solution strengthening, and Orowan strengthening mechanisms.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (82)

Show source-provided references
1. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: processing, microstructure, and properties10.1016/j.pmatsci.2015.03.002 ↗
2. Progress in additive manufacturing on new materials: a review10.1016/j.jmst.2018.09.002 ↗
3. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
4. Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: crack-inhibiting and multiple strengthening mechanisms10.1016/j.actamat.2020.03.060 ↗
5. Additive manufacturing (3D printing): a review of materials, methods, applications and challenges10.1016/j.compositesb.2018.02.012 ↗
6. Exploiting the rapid solidification potential of laser powder bed fusion in high strength and crack-free Al-Cu-Mg-Mn-Zr alloys
7. Superior mechanical properties of a selective-laser-melted AlZnMgCuScZr alloy enabled by a tunable hierarchical microstructure and dual-nanoprecipitation10.1016/j.mattod.2021.11.019 ↗
8. Selective laser melting of a high strength Al Mn Sc alloy: alloy design and strengthening mechanisms10.1016/j.actamat.2019.04.014 ↗
9. Chemical heterogeneity enhances hydrogen resistance in high-strength steels10.1038/s41563-021-01050-y ↗
10. Microstructure evolution of 316L produced by HP-SLM (high power selective laser melting)
11. In situ design of advanced titanium alloy with concentration modulations by additive manufacturing10.1126/science.abj3770 ↗
12. Increasing the productivity of laser powder bed fusion: influence of the hull-bulk strategy on part quality, microstructure and mechanical performance of Ti-6Al-4V
13. Understanding the effect of scanning strategies on the microstructure and crystallographic texture of Ti-6Al-4V alloy manufactured by laser powder bed fusion10.1016/j.jmatprotec.2021.117366 ↗
14. Homogenization kinetics of a nickel-based superalloy produced by powder bed fusion laser sintering10.1016/j.scriptamat.2016.12.037 ↗
15. Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting10.1016/j.actamat.2018.04.053 ↗
16. Unravelling the multi-scale structure–property relationship of laser powder bed fusion processed and heat-treated AlSi10Mg10.1038/s41598-021-85047-2 ↗
17. Highly conductive and strong CuSn0.3 alloy processed via laser powder bed fusion starting from a tin-coated copper powder
18. The origin of high-density dislocations in additively manufactured metals10.1080/21663831.2020.1751739 ↗
19. Investigation of solidification and precipitation behavior of Si-modified 7075 aluminum alloy fabricated by laser-based powder bed fusion10.1007/s11661-020-06073-9 ↗
20. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
21. Formation and reduction of hydrogen porosity during selective laser melting of AlSi10Mg10.1016/j.jmatprotec.2015.02.013 ↗
22. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
23. Grain refinement mechanisms in additively manufactured nano-functionalized aluminum10.1016/j.actamat.2020.09.043 ↗
24. Effect of Zr content on formability, microstructure and mechanical properties of selective laser melted Zr modified Al-4.24Cu-1.97Mg-0.56Mn alloys10.1016/j.jallcom.2018.06.032 ↗
25. Microstructure and mechanical properties of Zr-modified aluminum alloy 5083 manufactured by laser powder bed fusion
26. Additive manufacturing and mechanical properties of the dense and crack free Zr-modified aluminum alloy 6061 fabricated by the laser-powder bed fusion
27. Processing and characterization of crack-free aluminum 6061 using high-temperature heating in laser powder bed fusion additive manufacturing
28. Study of the suitability of aluminum alloys for additive manufacturing by laser powder-bed fusion
29. Characterisation of structural properties for AlSi10Mg alloys fabricated by selective laser melting10.1080/02670836.2017.1398513 ↗
30. New aluminum alloys specifically designed for laser powder bed fusion: a review10.3390/ma12071007 ↗
31. Recent progress in laser additive manufacturing of aluminum matrix composites10.1016/j.coche.2020.01.005 ↗
32. Changing the alloy composition of Al7075 for better processability by selective laser melting10.1016/j.jmatprotec.2016.08.003 ↗
33. Niobium nanoparticle-enabled grain refinement of a crack-free high strength Al-Zn-Mg-Cu alloy manufactured by selective laser melting10.1016/j.jallcom.2021.163427 ↗
34. A novel method to 3D-print fine-grained AlSi10Mg alloy with isotropic properties via inoculation with LaB6 nanoparticles
35. Microstructure control and performance evolution of aluminum alloy 7075 by nano-treating10.1038/s41598-019-47182-9 ↗
36. Rapid fabrication of Al-based bulk-form nanocomposites with novel reinforcement and enhanced performance by selective laser melting10.1016/j.scriptamat.2014.10.011 ↗
37. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
38. On the microstructure and solidification behavior of new generation additively manufactured Al-Cu-Mg-Ag-Ti-B alloys
39. Selective laser melting additive manufacturing of 7xxx series Al-Zn-Mg-Cu alloy: cracking elimination by co-incorporation of Si and TiB2
40. Scandium in aluminium alloys10.1179/174328005X14311 ↗
41. B. Jetting, Shape casting: 5th international symposium 2014, in: Shape Cast. 5th Int. Symp. 2014, John Wiley & Sons, 2013, p. 311.
42. Control of thermally stable core-shell nano-precipitates in additively manufactured Al-Sc-Zr alloys
43. A “missing” family of classical orthogonal polynomials10.1088/1751-8113/44/8/085201 ↗
44. Influence of SLM scan-speed on microstructure, precipitation of Al3Sc particles and mechanical properties in Sc- and Zr-modified Al-Mg alloys10.1016/j.matdes.2017.11.053 ↗
45. SLM-processed Sc- and Zr- modified Al-Mg alloy: mechanical properties and microstructural effects of heat treatment10.1016/j.msea.2017.06.089 ↗
46. Laser powder bed fusion of high-strength Sc/Zr-modified Al–Mg alloy: phase selection, microstructural/mechanical heterogeneity, and tensile deformation behavior10.1016/j.jmst.2021.03.069 ↗
47. Fatigue and dynamic aging behavior of a high strength Al-5024 alloy fabricated by laser powder bed fusion additive manufacturing10.1016/j.actamat.2021.117312 ↗
48. Microstructure and tensile property of a novel AlZnMgScZr alloy additively manufactured by gas atomization and laser powder bed fusion10.1016/j.scriptamat.2018.08.025 ↗
49. Strength-ductility synergy of selective laser melted Al-Mg-Sc-Zr alloy with a heterogeneous grain structure
50. Origin of non-uniform plasticity in a high-strength Al-Mn-Sc based alloy produced by laser powder bed fusion10.1016/j.jmst.2021.06.042 ↗
51. Work hardening in aluminium alloys
52. Strength and strain hardening of a selective laser melted AlSi10Mg alloy10.1016/j.scriptamat.2017.07.025 ↗
53. A strategy to improve the work-hardening behavior of Ti–6Al–4V parts produced by additive manufacturing10.1080/21663831.2016.1245681 ↗
54. Metastable high-entropy dual-phase alloys overcome the strength-ductility trade-off10.1038/nature17981 ↗
55. Heterogeneous materials: a new class of materials with unprecedented mechanical properties10.1080/21663831.2017.1343208 ↗
56. The deformation of plastically non-homogeneous materials
57. Design approaches for printability-performance synergy in Al alloys for laser-powder bed additive manufacturing10.1016/j.matdes.2021.109640 ↗
58. Design of heterogeneous structured Al alloys with wide processing window for laser-powder bed fusion additive manufacturing
59. First-principles studies on lattice constants and local lattice distortions in solid solution aluminum alloys10.1016/j.commatsci.2012.08.037 ↗
60. Towards high-temperature applications of aluminium alloys enabled by additive manufacturing
61. Criteria for developing castable, creep-resistant aluminum-based alloys – a review10.1515/ijmr-2006-0042 ↗
62. N.A. Belov, D.G. Eskin, A.A. Aksenov, Chapter 9 – alloys with transition metals, in: N.A. Belov, D.G. Eskin, A.A. Aksenov (eds.), Multicomponent Phase Diagrams, Elsevier, Oxford, 2005, pp. 287–340. 〈https://doi.org/10.1016/B978-008044537-3/50009-3〉.10.1016/B978-008044537-3/50009-3 ↗
63. Ab initio calculations on elastic properties in L12 structure Al3X and X3Al-type (X = transition or main group metal) intermetallic compounds10.1016/j.ssc.2012.10.021 ↗
64. Precipitation evolution in Al–0.1Sc, Al–0.1Zr and Al–0.1Sc–0.1Zr (at%) alloys during isochronal aging10.1016/j.actamat.2010.05.054 ↗
65. Exploration of D022-type Al3TM (TM = Sc, Ti, V, Zr, Nb, Hf, Ta): elastic anisotropy, electronic structures, work function and experimental design10.3390/ma14092206 ↗
66. Metastable phases in the Al3X (X = Ti, Zr, and Hf) intermetallic system10.1016/0956-716X(91)90059-A ↗
67. Thermal stability of aluminum alloys10.3390/ma13153441 ↗
68. On the solubility of group IV elements (Ti, Zr, Hf) in liquid aluminum below 800 °C10.1007/s11669-013-0278-2 ↗
69. Precipitation kinetics, microstructure evolution and mechanical behavior of a developed Al–Mn–Sc alloy fabricated by selective laser melting10.1016/j.actamat.2020.04.015 ↗
70. Coarsening of Al3Sc precipitates in Al-Mg-Sc alloys10.1016/j.jallcom.2018.12.133 ↗
71. Grain refinement in laser manufactured Al-based composites with TiB2 ceramic10.1016/j.jmrt.2020.04.059 ↗
72. Hafnium in aluminum alloys: a review10.1007/s40195-016-0379-0 ↗
73. Effect of Zr and Sc on microstructure and properties of 7136 aluminum alloy10.1016/j.jmrt.2019.07.022 ↗
74. Grain refinement of commercially pure aluminum with addition of Ti and Zr elements based on crystallography orientation
75. Microstructure of Al3Sc with ternary transition-metal additions10.1016/S0921-5093(01)01608-2 ↗
76. Crack mitigation in Laser Powder Bed Fusion processed Hastelloy X using a combined numerical-experimental approach10.1016/j.jallcom.2021.158803 ↗
77. Simulation of primary particle development and their impact on microstructural evolution of Sc-modified aluminum alloys during additive manufacturing10.3390/met11071056 ↗
78. Prediction of phase selection in rapid solidification using time dependent nucleation theory10.1016/0956-7151(94)90391-3 ↗
79. Bevington · 2003
80. A simple relationship between Lüders elongation and work-hardening rate at lower yield stress10.1016/j.scriptamat.2005.09.011 ↗
81. Underlying material response for Lüders-like instabilities10.1016/j.ijplas.2012.12.002 ↗
82. Towards understanding the structure–property relationships of heterogeneous-structured materials10.1016/j.scriptamat.2020.05.013 ↗